| 镍基合金表面Pt改性铝化物涂层的初期Al2O3微观结构分析 |
宋鹏( ), 陈榕, 冯晶, 吕建国, 陆建生 |
| 昆明理工大学材料科学与工程学院 昆明 650093 |
|
| Microstructure Analysis of Initial Alumina of Pt-Modified Aluminide Coatings on Ni-Based Alloy |
Peng SONG( ), Rong CHEN, Jing FENG, Jianguo Lü, Jiansheng LU |
| Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China |
引用本文:
宋鹏, 陈榕, 冯晶, 吕建国, 陆建生. 镍基合金表面Pt改性铝化物涂层的初期Al2O3微观结构分析[J]. 金属学报, 2017, 53(11): 1504-1510.
Peng SONG,
Rong CHEN,
Jing FENG,
Jianguo Lü,
Jiansheng LU.
Microstructure Analysis of Initial Alumina of Pt-Modified Aluminide Coatings on Ni-Based Alloy[J]. Acta Metall Sin, 2017, 53(11): 1504-1510.
| [1] | Goward G W. Progress in coatings for gas turbine airfoils [J]. Surf. Coat. Technol., 1998, 108-109: 73 | | [2] | Padture N P, Gell M, Jordan E H.Thermal barrier coatings for gas-turbine engine applications[J]. Science, 2002, 296: 280 | | [3] | Vassen R, Stuke A, St?ver D.Recent developments in the field of thermal barrier coatings[J]. J. Thermal Spray Technol., 2009, 18: 181 | | [4] | Schulz U, Leyens C, Fritscher K, et al.Some recent trends in research and technology of advanced thermal barrier coatings[J]. Aerosp. Sci. Technol., 2003, 7: 73 | | [5] | Gleeson B, Mu N, Hayashi S.Compositional factors affecting the establishment and maintenance of Al2O3 scales on Ni-Al-Pt systems[J]. J. Mater. Sci., 2009, 44: 1704 | | [6] | Tawancy H M, UI-Hamid A, Abbas N M, et al.Effect of platinum on the oxide-to-metal adhesion in thermal barrier coating systems[J]. J. Mater. Sci., 2008, 43: 2978 | | [7] | Vialas N, Monceau D.Effect of Pt and Al content on the long-term, high temperature oxidation behavior and interdiffusion of a Pt-modified aluminide coating deposited on Ni-base superalloys[J]. Surf. Coat. Technol., 2006, 201: 3846 | | [8] | Haynes J A, Pint B A, More K L, et al.Influence of sulfur, platinum, and hafnium on the oxidation behavior of CVD NiAl bond coatings[J]. Oxid. Met., 2002, 58: 513 | | [9] | Hou P Y, Tolpygo V K.Examination of the platinum effect on the oxidation behavior of nickel-aluminide coatings[J]. Surf. Coat. Technol., 2007, 202: 623 | | [10] | Svensson H, Christensen M, Knutsson P, et al.Influence of Pt on the metal-oxide interface during high temperature oxidation of NiAl bulk materials[J]. Corros. Sci., 2009, 51: 539 | | [11] | Qin F, Anderegg J W, Jenks C J, et al.The effect of Pt on Ni3Al surface oxidation at low-pressures[J]. Surf. Sci., 2007, 601: 146 | | [12] | Chieux M C, Molins R, Rémy L, et al. Effect of material and environmental parameters on the microstructure evolution and oxidation behavior of a Ni-based superalloy coated with a Pt-modified Ni-aluminide [J]. Mater. Sci. Forum, 2008, 595-598: 33 | | [13] | Tawancy H M, Abbas N M, Rhys-Jones T N. Role of platinum in aluminide coatings[J]. Surf. Coat. Technol., 1991, 49: 1 | | [14] | Tolpygo V K, Clarke D R.Microstructural study of the theta-alpha transformation in alumina scales formed on nickel-aluminides[J]. Mater. High Temp., 2000, 17: 59 | | [15] | Song P, Lu J S, Lü J G, et al.Influence factors of high temperature oxidation for Pt-modified-aluminide bond coatings[J]. Rare Met. Mater. Eng., 2010, 39: 304(宋鹏, 陆建生, 吕建国等. 铂铝涂层高温氧化的影响因素研究[J]. 稀有金属材料与工程, 2010, 39: 304) | | [16] | Song P, Lu J S, Zhang D F.High temperature oxidation of surface polished treatment Pt-modified-aluminide bond coats[J]. Chin. J. Nonferrous Met., 2009, 19: 1417(宋鹏, 陆建生, 张德丰. 抛光处理铂铝粘结层的高温氧化[J]. 中国有色金属学报, 2009, 19: 1417) | | [17] | Xing L L, Zheng Y J, Cui L S, et al.Progress of water vapour effect on growth of alumina forming alloys[J]. J. Chin. Soc. Corros. Prot., 2011, 31: 409(邢琳琳, 郑雁军, 崔立山等. 水蒸汽影响氧化铝膜生长的研究新进展[J]. 中国腐蚀与防护学报, 2011, 31: 409) | | [18] | Hayashi S, Narita T, Gleeson B. Early-stage oxidation behavior of γ′-Ni3Al-based alloys with and without Pt addition [J]. Mater. Sci. Forum, 2006, 522-523: 229 | | [19] | Hayashi S, Gleeson B.Early-stage oxidation behavior of Pt-modified γ′-Ni3Al-based alloys with and without Hf addition[J]. Oxid. Met., 2009, 71: 5 | | [20] | Pint B A, Haynes J A, Zhang Y, et al.The effect of water vapor on the oxidation behavior of Ni-Pt-Al coatings and alloys[J]. Surf. Coat. Technol., 2006, 201: 3852 | | [21] | Li M S, Zhou Y C.Transient oxidation of Al2O3 forming alloys[J]. Corros. Sci. Prot. Technol., 2005, 17: 409(李美栓, 周延春. Al2O3形成合金过渡态氧化行为[J]. 腐蚀科学与防护技术, 2005, 17: 409) | | [22] | Grabke H J.Oxidation of NiAl and FeAl[J]. Intermetallics, 1999, 7: 1153 | | [23] | Svensson H, Stiller K, Angenete J. Investigation of oxide formation during short-term oxidation of model NiAl alloys [J]. Mater. Sci. Forum, 2004, 461-464: 231 | | [24] | Svensson H, Knutsson P, Stiller K.Formation and healing of voids at the metal-oxide interface in NiAl alloys[J]. Oxid. Met., 2009, 71: 143 | | [25] | Hou P Y, Izumi T, Gleeson B.Sulfur segregation at Al2O3/γ-Νi + γ'-Ni3Al interfaces: Effects of Pt, Cr and Hf additions[J]. Oxid. Met., 2009, 72: 109 | | [26] | Hayashi S, Ford S I, Young D J, et al.α-NiPt(Al) and phase equilibria in the Ni-Al-Pt system at 1150 ℃[J]. Acta Mater., 2005, 53: 3319 |
|
|