| 冷轧高强钢板淬火过程板形瓢曲缺陷演变规律研究 |
张清东,林潇( ),曹强,卢兴福,张勃洋,胡树山 |
| 北京科技大学机械工程学院 北京 100083 |
|
| Flatness Defect Evolution of Cold-Rolled High Strength Steel Strip During Quenching Process |
Qingdong ZHANG,Xiao LIN( ),Qiang CAO,Xingfu LU,Boyang ZHANG,Shushan HU |
| School of Mechanical and Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
张清东,林潇,曹强,卢兴福,张勃洋,胡树山. 冷轧高强钢板淬火过程板形瓢曲缺陷演变规律研究[J]. 金属学报, 2017, 53(4): 385-396.
Qingdong ZHANG,
Xiao LIN,
Qiang CAO,
Xingfu LU,
Boyang ZHANG,
Shushan HU.
Flatness Defect Evolution of Cold-Rolled High Strength Steel Strip During Quenching Process[J]. Acta Metall Sin, 2017, 53(4): 385-396.
| [1] | Kang Y L.Lightweight vehicle, advanced high strength steel and energy-saving and emission reduction[J]. Iron Steel, 2008, 43(6): 1 | | [1] | (康永林. 汽车轻量化先进高强钢与节能减排[J]. 钢铁, 2008, 43(6): 1) | | [2] | Rong Y H.Advanced Q-P-T steels with ultrahigh strength-high ductility[J]. Acta Metall. Sin., 2011, 47: 1483 | | [2] | (戎咏华. 先进超高强度-高塑性Q-P-T钢 [J]. 金属学报, 2011, 47: 1483) | | [3] | Wang L J, Cai Q W, Yu W, et al.Microstructure and mechanical properties of 1500 MPa grade ultra-high strength low alloy steel[J]. Acta Metall. Sin., 2010, 46: 687 | | [3] | (王立军, 蔡庆伍, 余伟等. 1500 MPa级低合金超高强钢的微观组织与力学性能[J]. 金属学报, 2010, 46: 687) | | [4] | Wang Y, Zhang K, Guo Z H, et al.A new effect of retained austenite on ductility enhancement of low carbon Q-P-T steel[J]. Acta Metall. Sin., 2012, 48: 641 | | [4] | (王颖, 张柯, 郭正洪等. 残余奥氏体增强低碳Q-P-T钢塑性的新效应[J]. 金属学报, 2012, 48: 641) | | [5] | Jia X S, Zuo X W, Chen N L, et al.Microstructure and properties of Q235 steel treated by novel Q-P-T process[J]. Acta Metall. Sin., 2013, 49: 35 | | [5] | (贾晓帅, 左训伟, 陈乃录等. 经新型Q-P-T工艺处理后Q235钢的组织与性能[J]. 金属学报, 2013, 49: 35) | | [6] | Ju B, Wu H B, Tang D, et al.Effect of microstructure evolution on mechanical properties of ultra-high strength wear resistance steel[J]. Acta Metall. Sin., 2014, 50: 1055 | | [6] | (巨彪, 武会宾, 唐荻等. 微观组织演变对超高强耐磨钢板力学性能的影响[J]. 金属学报, 2014, 50: 1055) | | [7] | Zhu D M, Liu G Y, Li L H, et al.Research of martensite transformation on technical parameters of non-restraint quenching[J]. Iron Steel, 2008, 43(1): 50 | | [7] | (朱冬梅, 刘国勇, 李龙海等. 相变对无约束淬火控冷工艺参数的影响[J]. 钢铁, 2008, 43(1): 50) | | [8] | Qiao X, Yu F, Liu Y.Flatness control of thin plate in the process of quenching[J]. J. Iron Steel Res., 2011, 23(suppl.1): 159 | | [8] | (乔馨, 于峰, 刘源. 薄规格钢板淬火过程中的板形控制[J]. 钢铁研究学报, 2011, 23(增刊1): 159) | | [9] | Wu Y L, Wang D C, Kong L.Analysis of transverse flatness distribution of steel plate during the quenching process[J]. Adv. Mater. Res., 2015, 1095: 689 | | [10] | Liu G Y, Li M W, Zhang S J.Thermal numerical simulation and experiment in quenching process of medium and heavy plate[J]. J. Iron Steel Res., 2007, 19(8): 51 | | [10] | (刘国勇, 李谋渭, 张少军. 中厚板淬火过程的热力学数值模拟及实验[J]. 钢铁研究学报, 2007, 19(8): 51) | | [11] | Kaseda Y, Masui T.Control of buckling and crossbow in strip processing lines[J]. Iron Steel Eng., 1994, 71: 14 | | [12] | Zhang Q D, Chang T Z, Dai J B, et al.Finite element simulation of the transverse distribution of tensile stress in the strip during continuous annealing process[J]. J. Univ. Sci. Technol. Beijing, 2006, 28: 1162 | | [12] | (张清东, 常铁柱, 戴江波等. 连退线上带钢张应力横向分布的有限元仿真[J]. 北京科技大学学报, 2006, 28: 1162 | | [13] | Zhang Q D, Chang T Z, Dai J B.Theory and experiment of the strip transverse buckling under high temperature[J]. Chin. J. Mech. Eng., 2008, 44(8): 219 | | [13] | (张清东, 常铁柱, 戴江波. 带钢高温态横向瓢曲的理论与试验[J]. 机械工程学报, 2008, 44(8): 219) | | [14] | Zhang Q D, Liu Z Z, Zhou X M, et al.Research on strip profile buckling deformation during continuous annealing process[J]. Shanghai Met., 2005, 27(4): 27 | | [14] | (张清东, 刘赞赞, 周晓敏等. 带钢在连续退火过程中的板形屈曲变形原因分析[J]. 上海金属, 2005, 27(4): 27) | | [15] | Lu X F.Study on buckling and warping deformation of steel strip [D]. Beijing: University of Science and Technology Beijing, 2015 | | [15] | (卢兴福. 钢板带板形瓢曲与翘曲变形行为研究 [D]. 北京: 北京科技大学, 2015) | | [16] | Dai J B, Zhang Q D, Chen X L, et al.Large thermo-deflection of steel strip being processed in continuous anneal furnace[J]. Chin. J. Mech. Eng., 2003, 39(12): 71 | | [16] | (戴江波, 张清东, 陈先霖等. 连续退火炉内带钢的热态大挠度变形分析[J]. 机械工程学报, 2003, 39(12): 71) | | [17] | Dai J T, Zhang Q D.Analysis and experiment on central buckling and post buckling of thin cold-rolled sheet[J]. Chin. J. Mech. Eng., 2011, 47(2): 44 | | [17] | (戴杰涛, 张清东. 冷轧薄板中浪板形缺陷的屈曲及后屈曲理论与轧制试验研究[J]. 机械工程学报, 2011, 47(2): 44) | | [18] | Dai J T, Zhang Q D, Qin J.Analysis of local buckling for thin cold-rolled strip[J]. Eng. Mech., 2011, 28(10): 236 | | [18] | (戴杰涛, 张清东, 秦剑. 薄宽冷轧带钢局部板形屈曲行为解析研究[J]. 工程力学, 2011, 28(10): 236) | | [19] | Lequesne C, Pensis O, Renard M, et al.Roller pressure quench process of steel plate modelling [A]. Proceedings of the 14th International Conference on Material Forming, ESAFORM 2011[C]. Melville: American Institute of Physics, 2011: 115 | | [20] | Liu Z, Wu Z J, Wu J Z.Numerical Simulation of Heat Treatment Processing [M]. Beijing: Science Press, 1996: 1 | | [20] | (刘庄, 吴肇基, 吴景之. 热处理过程的数值模拟. 北京: 科学出版社, 1996: 1) | | [21] | De Oliveira W P, Savi M A, Pacheco P M C L. Finite element method applied to the quenching of steel cylinders using a multi-phase constitutive model[J]. Arch. Appl. Mech., 2013, 83: 1013 | | [22] | Zhou Z F, Wang X Y, Gu J F.Numerical simulation of eccentric cylinder quenching process[J]. J. Mech. Eng., 2011, 47(12): 62 | | [22] | (周志方, 王晓燕, 顾剑锋. 偏心圆环淬火过程的数值模拟[J]. 机械工程学报, 2011, 47(12): 62) | | [23] | Song G S, Liu X H, Wang G D, et al.Numeric simulation on the effect of phase transformation on quenching stress of 22CrMo steel[J]. J. Plast. Eng., 2006, 13(2): 75 | | [23] | (宋广胜, 刘相华, 王国栋等. 相变对22CrMo钢淬火应力影响的数值模拟[J]. 塑性工程学报, 2006, 13(2): 75) | | [24] | He L F, Li H P, Zhao G Q.FEM simulation of temperature, phase-transformation and stress/strain in quenching process[J]. Trans. Mater. Heat Treat., 2011, 32(1): 128 | | [24] | (贺连芳, 李辉平, 赵国群. 淬火过程中温度、组织及应力/应变的有限元模拟[J]. 材料热处理学报, 2011, 32(1): 128) | | [25] | Zhang Q D, Cao Q, Zhang X F.A modified Johnson-Cook model for advanced high-strength steels over a wide range of temperatures[J]. J. Mater. Eng. Perform., 2014, 23: 4336 | | [26] | Sun C Y, Zeng P, Zhao S X, et al.Distortion prediction of larger-size plate for armour steel during quenching[J]. Heat Treat. Met., 2008, 33(8): 73 | | [26] | (孙朝阳, 曾攀, 赵书行等. 装甲防护厚板淬火过程形状畸变的预测[J]. 金属热处理, 2008, 33(8): 73) | | [27] | Wang C, Wang Z D, Yuan G, et al.Heat transfer during quenching by plate roller quenching machine[J]. J. Iron Steel Res. Int., 2013, 20(5): 1 | | [28] | Cheng H M, Wang H G, Chen T L.Solution of heat conduction inverse problem for steel 45 during quenching[J]. Acta Metall. Sin., 1997, 33: 467 | | [28] | (程赫明, 王洪纲, 陈铁力. 45钢淬火过程中热传导方程逆问题求解[J]. 金属学报, 1997, 33: 467) | | [29] | Cheng B S, Xiao N M, Li D Z, et al.Sensitivity analysis of the effect of interfacial heat transfer coefficient on distortion simulation during quenching[J]. Acta Metall. Sin., 2012, 48: 696 | | [29] | (程柏松, 肖纳敏, 李殿中等. 界面换热系数对淬火过程变形模拟影响的敏感性分析[J]. 金属学报, 2012, 48: 696) | | [30] | Wang X H, Li Y Y, Wang Y, et al.Control of asymmetric higher order flattness in cold rolling mill[J]. Steel Roll., 2008, 25(3): 25 | | [30] | (王训宏, 李有元, 王勇等. 冷轧机组不对称高次浪形的控制[J]. 轧钢, 2008, 25(3): 25) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|