Nb-Ti-Si-Cr基超高温合金表面ZrSi2-NbSi2复合渗层的组织及其抗高温氧化性能* |
李轩,郭喜平( ),乔彦强 |
西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
MICROSTRUCTURE AND OXIDATION BEHAVIOR OF ZrSi2-NbSi2 MULTILAYER COATINGS ON AN Nb-Ti-Si-Cr BASE ULTRAHIGH TEMPERATURE ALLOY |
Xuan LI,Xiping GUO( ),Yanqiang QIAO |
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
李轩, 郭喜平, 乔彦强. Nb-Ti-Si-Cr基超高温合金表面ZrSi2-NbSi2复合渗层的组织及其抗高温氧化性能*[J]. 金属学报, 2015, 51(6): 693-700.
Xuan LI,
Xiping GUO,
Yanqiang QIAO.
MICROSTRUCTURE AND OXIDATION BEHAVIOR OF ZrSi2-NbSi2 MULTILAYER COATINGS ON AN Nb-Ti-Si-Cr BASE ULTRAHIGH TEMPERATURE ALLOY[J]. Acta Metall Sin, 2015, 51(6): 693-700.
[1] | Bewlay B P, Jackson M R, Zhao J C, Subramaniam P R. Metall Mater Trans, 2003; 34A: 2043 | [2] | Guo X P, Gao L M, Guan P, Kusabiraki K, Fu H Z. Mater Sci Forum, 2007; 539-543: 3690 | [3] | Murayama Y, Hanada S. Sci Technol Adv Mater, 2002; 3: 145 | [4] | Zelenitsas K, Tsakiropoulos P. Mater Sci Eng, 2006; A416: 269 | [5] | Vilasi M, Steinmetz J, Allemand B G. J Adv Mater, 2000; 32: 53 | [6] | Suzuki R O, Ishikawa M, Ono K. J Alloys Compd, 2002; 336: 280 | [7] | Tian X D, Guo X P. Acta Metall Sin, 2008; 44: 585 (田晓东, 郭喜平. 金属学报, 2008; 44: 585) | [8] | Zhang P, Guo X P. Corros Sci, 2013; 71: 10 | [9] | Majumdar S, Sengupta T P, Kale G B, Sharma I G. Surf Coat Technol, 2006; 200: 3713 | [10] | Cockeram B V, Rapp R A. Mater Sci Eng, 1995; A192: 980 | [11] | Dzyadikevich Y V, Kitskai L I. Powder Metall Met Ceram, 1997; 36: 77 | [12] | Yoon J K, Kim G H, Han J H, Shon I J, Doh J M, Hong K T. Intermetallics, 2005; 13: 1146 | [13] | Christensen R J, Tolpygo V K, Clarke D R. Acta Mater, 1997; 45: 1761 | [14] | Qiao Y Q, Guo X P. Appl Surf Sci, 2010; 256: 7462 | [15] | Wang W, Yuan B F, Zhou C G. Corros Sci, 2014; 80: 164 | [16] | Tian X D, Guo X P. Surf Coat Technol, 2009; 204: 313 | [17] | Hong S J, Hwang G H, Han W K, Lee K S, Kang S G. Intermetallics, 2010; 18: 864 | [18] | Xiang Z D, Datta P K. Acta Mater, 2006; 54: 4453 | [19] | Li X, Guo X P. Acta Metall Sin, 2012; 48: 1394 (李 轩, 郭喜平. 金属学报, 2012; 48: 1394) | [20] | Kelly P J, Brien J O, Arnell R D. Vacuum, 2004; 74: 1 | [21] | Zhang P, Guo X P. Acta Metall Sin, 2010; 46: 821 (张 平, 郭喜平. 金属学报, 2010; 46: 821) | [22] | Salpadoru N H, Flower H M. Metall Mater Trans, 1995; 26A: 243 | [23] | Wang R C, Jin Z P, Liu C L. J Cent South Univ Technol, 2002; 33: 385 (王日初, 金展鹏, 柳春雷. 中南工业大学学报, 2002; 33: 385) | [24] | Zhao J C, Jackson M R, Peluso L A. Mater Sci Eng, 2004; A372: 21 | [25] | Sanjib M, Indrakumar S, Indradev S, Parag B. J Electrochem Soc, 2008; 155D: 743 | [26] | Cockeram B V, Rapp R A. Metall Mater Trans, 1995; 26A: 777 | [27] | Pan J S,Tong J M,Tian M B. Fundamentals of Materials Science. Beijing: Tsinghua University Press, 1998: 466 (潘金生,仝建民,田民波. 材料科学基础. 北京: 清华大学出版社, 1998: 466) | [28] | Patil R V, Kale G B, Garg S P. J Nucl Mater, 1995; 223: 169 | [29] | Milanese C, Buscaglia V, Maglia F, Tamburini U A. Acta Mater, 2003; 51: 4837 | [30] | Colinet C, Tedenac J C. Intermetallics, 2010; 18: 1444 | [31] | Fernandes P B, Coelho G C, Ferreira F, Nunes C A, Sundman B. Intermetallics, 2002; 10: 993 | [32] | Pelleg J, Shor Y. Microelectron Eng, 2003; 69: 65 | [33] | Kaiser A, Lobert M, Telle R. J Eur Ceram Soc, 2008; 28: 2199 | [34] | Ebener S, Winter W. J Eur Ceram Soc, 1996; 16: 1179 | [35] | Moon D P. Mater Sci Technol, 1989; 5: 754 | [36] | Thanneeru R, Patil S, Deshpande S, Seal S. Acta Mater, 2007; 55: 3457 |
|
|