| Mn1.2Fe0.8P0.76Ge0.24磁制冷材料相变过程与磁性能关系的研究 |
| 张孟1),刘丹敏1),刘翠秀1),黄清镇2),王少博1),张虎1),岳明3) |
| 1) 北京工业大学固体微结构与性能研究所, 北京 100124
2) NIST Center for Neutron Research, National Institute of Standards and Technology,Gaithersburg, Maryland 20899
3) 北京工业大学材料科学与工程学院, 北京 100124 |
|
| RESEARCH OF THE RELATIONSHIP BETWEEN PHASE TRANSITION PROCESS AND MAGNETIC PROPERTIES IN MAGNETIC REFRIGERATION MATERIAL Mn1.2Fe0.8P0.76Ge0.24 |
| ZHANG Meng1), LIU Danmin1), LIU Cuixiu1), HUANG Qingzhen2), WANG Shaobo1), ZHANG Hu1), YUE Ming3) |
| 1) Institute of Microstructure and Property of Advanced Materials, Beijing University of Technology, Beijing 100124
2) NIST Center for Neutron Research, National Institute of Standards and Technology, Gaithersburg, Maryland 20899
3) College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124 |
引用本文:
张孟,刘丹敏,刘翠秀,黄清镇,王少博,张虎,岳明. Mn1.2Fe0.8P0.76Ge0.24磁制冷材料相变过程与磁性能关系的研究[J]. 金属学报, 2013, 49(7): 783-788.
ZHANG Meng,
LIU Danmin,
LIU Cuixiu,
HUANG Qingzhen,
WANG Shaobo,
ZHANG Hu,
YUE Ming.
RESEARCH OF THE RELATIONSHIP BETWEEN PHASE TRANSITION PROCESS AND MAGNETIC PROPERTIES IN MAGNETIC REFRIGERATION MATERIAL Mn1.2Fe0.8P0.76Ge0.24[J]. Acta Metall Sin, 2013, 49(7): 783-788.
| [1] Dan'kov S Y, Tishin A M, Pecharsky V K, Gschneidner K A. Phys Rev, 1998; 57B: 3478
[2] Pecharsky V K, Gschneidner K A.Phys Rev Lett, 1997; 78: 4494
[3] Hu F X, Shen B G, Sun J R.Appl Phys Lett, 2001; 78: 3675
[4] Tegus O, Bruck E, Buschowet K H J, de Boer F R. Nature, 2002; 415: 150
[5] Wang G F, Song L, Li F A, Ha S C L, Li X W, Tegus O. Acta Metall Sin, 2008; 43: 889
(王高峰, 松林, 李福安, 哈斯朝鲁, 李新文, 特古斯. 金属学报, 2008; 43: 889)
[6] Hu F X, Qian X L, Wang G J, Sun J R, Shen B G, Cheng Z H, Gao J. Chin Phys, 2005; 14: 2329
[7] Li F A, Song L, Bao L H, Ha S C L, Tegus O, Huang J H.Acta Metall Sin, 2008; 44: 371
(李福安, 松林, 包黎红, 哈斯朝鲁, 特古斯, 黄焦宏. 金属学报, 2008; 44: 371)
[8] Tegus O, Bruck E, Li X W, Zhang L, Dagula W, de Boer F R, Buschow K H J.J Magn Magn Mater, 2004; 272: 2389
[9] Kim Y K, Cho Y W. J Alloys Compd, 2005; 394: 19
[10] Tegus O, Lin G X, Dagula W, Fuquan B, Zhang L, Bruck E, de Boer F R,Buschow K H J. J Magn Magn Mater, 2005; 290: 658
[11] Hermann R P, Tegus O, Bruck E, Buschow K H J, de Boer F R, Long G J,Grandjean F. Phys Rev, 2004; 70B: 214425
[12] Tegus O, Koyama K, Her J L, Watanabe K, Bruck E, Buschow K H J,de Boer F R.Physica, 2007; 392B: 151
[13] Bruck E, Kamarad J, Sechovsky V, Arnold Z, Tegus O, de Boer F R.J Magn Magn Mater,2007; 310: e1008
[14] Tegus O, Fuquan B, Dagula W, Zhang L, Bruck E, Si P Z, de Boer F R,Buschow K H J.J Alloys Compd, 2005; 396: 6
[15] Thanh D T Cam, Bruck E, Tegus O, Klaasse J C P, Buschow K H J. J Magn Magn Mater,2007; 310: e1012
[16] Thanh D T, Bruck E, Tegus O, Klaasse J C P, Gortenmulder T J,Buschow K H J. J Appl Phys, 2006; 99: 1
[17] Li X W, Tegus O, Zhang L, Dagula W, Bruck E, Buschow K H J, de Boer F R.IEEE Trans Magn, 2003; 39: 3148
[18] Yue M, Li Z Q, Xu H, Huang Q Z, Liu X B, Liu D M, Zhang J X. J Appl Phys, 2010; 107: 09A939
[19] Dagula W, Tegus O, Fuquan B, Zhang L, Si P Z, Zhang M, Zhang W S,Bruck E, de Boer F R, Buschow K H J. IEEE Trans Magn, 2005; 41: 2778
[20] Qu Z Q, Wang G F, Lin S, Tegus O, Bruck E, Buschow K H J. J Phys: Condes Matter,2006; 18: 11577
[21] Bao Y M, Zhang K D. Magnetic Refrigeration Technology. Beijing: Chemical Industry Press, 2004: 69
(鲍雨梅, 张康达. 磁制冷技术. 北京: 化学工业出版社, 2004: 69)
[22] Feng H B, Zhou Y, Jia D C. Mater Sci Thchnol, 2003; 11: 327
(冯海波, 周玉, 贾德昌. 材料科学与工艺, 2003; 11: 327)
[23] Zhang J X, Liu K G, Zhou M L. Powder Metall Technol, 2002; 20: 129
(张久兴, 刘科高, 周美玲. 粉末冶金技术, 2002; 20: 129)
[24] Gao L, Miyamoto H.J Inorg Mater, 1997; 12: 129
(高濂, 宫本大树. 无机材料学报, 1997; 12: 129)
[25] Yamada H, Goto T. { Phys Rev, 2003; 68B: 184417 |
|