| DP1180双相钢在高应变速率变形条件下应变硬化行为及机制 |
| 代启锋1,宋仁伯1,范午言1,郭志飞1,2,关小霞1 |
1. 北京科技大学材料科学与工程学院, 北京 100083
2. 首钢技术研究院, 北京 100043 |
|
| BEHAVIOUR AND MECHANISM OF STRAIN HARDENING FOR DUAL PHASE STEEL DP1180 UNDER HIGH STRAIN RATE DEFORMATION |
| DAI Qifeng 1, SONG Renbo 1, FAN Wuyan 1, GUO Zhifei 1,2, GUAN Xiaoxia 1 |
1. School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
2. Shougang Research Institute of Technology, Beijing 100043 |
引用本文:
代启锋 宋仁伯 范午言 郭志飞 关小霞. DP1180双相钢在高应变速率变形条件下应变硬化行为及机制[J]. 金属学报, 2012, 48(10): 1160-1165.
DAI Qifeng SONG Renbo FAN Wuyan GUO Zhifei GUAN Xiaoxia.
BEHAVIOUR AND MECHANISM OF STRAIN HARDENING FOR DUAL PHASE STEEL DP1180 UNDER HIGH STRAIN RATE DEFORMATION[J]. Acta Metall Sin, 2012, 48(10): 1160-1165.
| [1] Chongthairungruang B, Uthaisangsuk V, Suranuntchai S, Jirathearanat S. Mater Des, 2012; 39: 318[2] Giri S K, Bhattacharjee D. J Mater Eng Perform, 2012; 21: 988[3] Pouranvari M. Mater Sci Eng, 2012; A546: 129[4] Queiroz R R U, Cunha F G G, Gonzalez B M. Mater Sci Eng, 2012; A543: 84[5] Ahmad E, Manzoor T, Ziai M M A, Hussain N. J Mater Eng Perform, 2012; 21: 382[6] Nouri A, Saghafian H, Kheirandish S. Int J Mater Res, 2010; 101: 1286[7] Calcagnotto M, Adachi Y, Ponge D, Raabe D. Acta Mater, 2011; 59: 658[8] Sun X, Choi K S, Soulami A, Liu W N, Khaleel M A. Mater Sci Eng, 2009; A526: 140[9] Huh H, Kang W J, Han S S. Exp Mech, 2002; 42(1): 8[10] Deng Z J, Liu J, Wang H, Li P H. J Mater Therm Treat, 2011; 32: 111(邓照军, 刘静, 王辉, 李平和. 材料热处理学报, 2011; 32: 111)[11] Kamp A, Celotto S, Hanlon D N. Mater Sci Eng, 2012; A538: 35[12] Colla V, De Sanctis M, Dimatteo A, Lovicu G, Solina A, Valentini R. Metall Mater Trans, 2009; 40A: 2557[13] Sung J H, Kim J H, Wagoner R H. Int J Plast, 2010; 26: 1746[14] Beynon N D, Jones T B, Fourlaris G. Mater Sci Technol, 2005; 21: 103[15] Kuang S, Kang Y L, Yu H, Liu R D. J Mater Eng, 2009; (2): 11(邝霜, 康永林, 于浩, 刘仁东. 材料工程, 2009; (2): 11)[16] Ramos L F, Matlock D K, Krauss G. Metall Trans, 1979; 10A: 259[17] Samuel F H. Mater Sci Eng, 1987; 92: L1[18] Jha B K, Avtar R, Dwivedi V S, Ramaswamy V. J Mater Sci Lett, 1987; 6: 891[19] Swift H W. J Mech Phys Solids, 1952; (1): 1[20] Das D, Chattopadhyay P P. J Mater Sci, 2009; 44: 2957[21] Yu Y N. Fundamentals of Materials Science. Beijing: High Education Press, 2006: 566(余永宁. 材料科学基础. 北京: 高等教育出版社, 2006: 566)[22] Winther G, Jensen D J, Hansen N. Acta Mater, 1997; 45: 5059[23] Sha G Y, Sun X G, Liu T, Zhu Y H, Feng X G. Chin J Mater Res, 2010; 24: 567(沙桂英, 孙晓光, 刘腾, 朱宇宏, 冯晓刚. 材料研究学报, 2010; 24: 567)[24] Hughes D A, Hansen N, Bammann D J. Scr Mater, 2003; 48: 147[25] Wu Z Q, Tang Z Y, Li H Y, Zhang H D. Acta Metall Sin, 2012; 48: 593(吴志强, 唐正友, 李华英, 张海东. 金属学报, 2012; 48: 593)[26] Wu C C, Wang S H, Chen C Y, Yang J R, Chiu P K, Fang J. Scr Mater, 2007; 56: 717 |
|