| 黄铜矿表面生物氧化膜的形成过程 |
| 杨洪英, 潘颢丹, 佟琳琳, 刘媛媛 |
| 东北大学材料与冶金学院, 沈阳 110819 |
|
| FORMATION PROCESS OF BIOLOGICAL OXIDE FILM ON CHALCOPYRITE CRYSTAL SURFACE |
| YANG Hongying, PAN Haodan, TONG Linlin, LIU Yuanyuan |
| School of Materials and Metallurgy, Northeastern University, Shenyang 110819 |
引用本文:
杨洪英 潘颢丹 佟琳琳 刘媛媛. 黄铜矿表面生物氧化膜的形成过程[J]. 金属学报, 2012, 48(9): 1145-1152.
,
,
,
.
FORMATION PROCESS OF BIOLOGICAL OXIDE FILM ON CHALCOPYRITE CRYSTAL SURFACE[J]. Acta Metall Sin, 2012, 48(9): 1145-1152.
| [1] BrierleyJ A. FEMS Microbiol Lett, 1990; 75: 287[2] Rohwerder T, Gehrke T, Kinzler K, Sand W. Appl Microbiol Biotechnol, 2003; 63: 239[3] Dutrizac J E. Metall Trans, 1978; 9B: 431[4] Petersen J, David G D. Hydrometallurgy, 2006; 83: 40[5] Morin D, Lips A, Pinches T, Huisman J, Frias C, Norberg A, Forssberg E. Hydrometallurgy, 2006; 83: 69[6] Bestamin O, Erkan S, Pauliina N, Anna H K, Jaakko A P. Hydrometallurgy, 2007; 88: 67[7] Leahy MJ, DavidsonM R, SchwarzMP. Hydrometallurgy, 2007; 85: 24[8] Cecilia S D, Pedro A G P, Lorena V E G, V´?ctor J Z A, Danny C, Emilio O C. Hydrometallurgy, 2005; 80: 241[9] Rebecca B H, Peter D F, Jason J P. Hydrometallurgy, 2006; 83: 229[10] Parker A, Klauber C, Kougianos A, Watling H R, van Bronswijk W. Hydrometallurgy, 2003; 71: 265[11] Lopez–Juarez A, Gutierrez–Arenas N, Rivera–Santill´an R E. Hydrometallurgy, 2006; 83: 63[12] Brierley J A, Brierley C L. Hydrometallurgy, 2001; 59: 233[13] Watling H R. Hydrometallurgy, 2006; 84: 81[14] Mousavi S M, Yaghmaei S, Vossoughi M, Jafari A, Hoseini S A. Hydrometallurgy, 2005; 80: 139[15] Rodr?ques Y, Ballester A, Bl´azques M L, Gonzales F, Munoz J A. Hydrometallurgy, 2003; 71: 37[16] Hackl R P, Dreisinger D B, Peters E, King J A. Hydrometallurgy, 1995; 39: 25[17] Harmer S L, Thomas J E, Fornasiero D, Gerson A R. Geochim Cosmochim Acta, 2006; 70: 4392[18] Liang C L, Xia J L, Yang Y, Nie Z Y, Qiu G Z. Chin J Nonferrous Met, 2012; 22: 265(梁长利, 夏金兰, 杨益, 聂珍媛, 邱冠周. 中国有色金属学报, 2012; 22: 265)[19] Xia L X, Tang L, Xia J L, Yin C, Cai L Y, Zhao X J, Nie Z Y, Liu J S, Qiu G Z. Trans Nonferrous Met Soc China, 2012; 22: 192[20] Bevilaqua D, Diezperez I, Fugivara C S, Sanz F, Benedetti A V, Garcia Jr O. Bioelectrochemistry, 2004; 64: 79[21] Yao G C, Wen J K, Gao H Z, Wang D Z. J Cent South Univ (Sci Technol), 2010; 41: 1234(姚国成, 温建康, 高焕芝, 王淀佐. 中南大学学报(自然科学版), 2010; 41: 1234)[22] Ahmadi A, Schaffie M, Manafi Z, Ranjbar M. Hydrometallurgy, 2010; 104: 99[23] Third K A, Cordruwisch R, Watling H R. Hydrometallurgy, 2000; 57: 225[24] Silverman M, Lundgren D. J Bacteriol, 1959; 77: 642[25] Pan H D, Yang H Y, Chen S D, Li W T. In: Niu Y J ed., Memoir of the 8th Annual Conf Transactions of Nonferrous Metals Society of China, Changsha: Central South University Press, 2010: 146(潘颢丹, 杨洪英, 陈世栋, 李伟涛. 见: 钮因健 主编, 第八届中国有色金属年会会议论文集, 长沙: 中南大学出版社, 2010: 146)[26] Fu B, Li H C eds.. Manual of Nonferrous Metallurgical Analysis. Beijing: Metallurgical Industry Press, 2004: 1(符斌, 李华昌编. 有色冶金分析手册. 北京: 冶金工业出版社, 2004: 1)[27] Yang H Y, Yang L, Wei X J. Trans Nonferrous Met Soc China, 2001; 11: 323(杨洪英, 杨 立, 魏绪钧. 中国有色金属学报, 2001; 11: 323)[28] Gebhardt J E, McCarron J J, Richardson P E, Buckley A N. Hydrometallurgy, 1986; 17: 27[29] Harmer S L, Thomas J E, Fornasiero D, Gerson A R. Geochim Cosmochim Acta, 2006; 70: 4392[30] Dora N, Ignacio G. Electrochim Acta, 2006; 51: 5295[31] Weisener C G, Smart R St C, Gerson A R. Geochim Cosmochim Acta, 2003; 67: 823[32] Yuri L M, Yevgeny V T, Igor P A, Alexander V O, Vladimir A V, Denis V V. Appl Surf Sci, 2005; 225: 395[33] McIntyre N S, Zetaruk D G. Anal Chem, 1997; 49: 1521[34] Klauber C, Parker A, Bronswijk W V, Watling H. Int J Miner Process, 2001; 62: 65[35] Lazaro I, Nicol M J. In: Young C, Alfantazi A M, Anderson C G eds., Hydrometallurgy. Warrendale, PA: TMS, 2003: 405[36] Stott M B,Watling H R, Franzmann P D, Sutton D. Miner Eng, 2000; 13: 1117 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|