| 质粒DNA光化学反应制备Ag纳米颗粒 |
| 刘建华, 章锦丹, 张晓亮, 李松梅, 于美 |
| 北京航空航天大学材料科学与工程学院, 北京 100191 |
|
| PREPARATION OF Ag NANOPARTICLES BASED ON PHOTOIRRADIATION METHOD WITH PLASMID DNA-TEMPLATED |
| LIU Jianhua, ZHANG Jindan, ZHANG Xiaoliang, LI Songmei, YU Mei |
| School of Materials Science and Engineering, Beihang University, Beijing 100191 |
引用本文:
刘建华 章锦丹 张晓亮 李松梅 于美. 质粒DNA光化学反应制备Ag纳米颗粒[J]. 金属学报, 2012, 48(9): 1139-1144.
,
,
,
,
.
PREPARATION OF Ag NANOPARTICLES BASED ON PHOTOIRRADIATION METHOD WITH PLASMID DNA-TEMPLATED[J]. Acta Metall Sin, 2012, 48(9): 1139-1144.
| [1] Ozawa K, Nakao Y, Cheng Z X, Wang D F, Osada M, Okada R, Saeki K, Itoh H, Iso F. Mater Lett, 2009; 63: 366[2] Fan T X, Chow S K, Zhang D. Prog Mater Sci, 2009; 54: 542[3] Zhang L D, Mou J M. Nanomaterial and Nanostructure. Beijing: Science Press, 2001: 80(张立德, 牟季美.纳米材料和纳米结构. 北京: 科学出版社, 2001: 80)}[4] Zhao X Q, Liang Y, Hu Z L. Acta Metall Sin, 2001; 37: 633(赵新清, 梁 勇, 胡壮麟. 金属学报, 2001; 37: 633)[5] Salaita K, Wang Y, Fragala J, Vega R A, Liu C, Mirkin C A. Angew Chem Int Ed, 2006; 45: 7220[6] Hoinville J, Bewick A, Gleesson D, Jones R, Kasyutich O, Nartowski A, Warne B, Wiggins J, Wong K. J Appl Phys, 2003; 93: 7187[7] Pan B, Cui D, Ozkan C, Xu P, Huang T, Li Q, Chen H, Liu F, Gao F, He R. J Phys Chem, 2007; 111C: 12572[8] Gazit E. Chem Soc Rev, 2007; 36: 1263[9] Sotiropoulou S, Yajaira S S, Mark S S, Batt C A. Chem Mater, 2008; 20: 821[10] Deng Z X, Mao C D. Nano Lett, 2003; 3: 1545[11] Kundu S, Lee H, Liang H. Inorg Chem, 2009; 48: 121[12] Gu Q, Haynie D T. Mater Lett, 2008; 62: 3047[13] Wirtz D. Phys Rev Lett, 1995; 75: 2436[14] Kundu S, Wang K, Huitink D, Liang H. Langmuir, 2009; 25: 10146[15] Samson J, Varotto A, Nahirney P C, Toschi A, Piscopo I, Drain C M. ACS Nano, 2009; 3: 339[16] Berti L, Alessandrini A, Facci P. J Am Chem Soc, 2005; 127: 11216[17] Zhang X L, Yu M, Liu J H, Li S M. Langmuir, 2012; 28: 3690[18] Liu J H, Zhang X L, Li S M, Yu M. Appl Surf Sci, 2011; 257: 2383[19] Zhang X L, Liu J H, Li S M. Mater Lett, 2009; 63: 1907[20] Liang X, Liu J H, Li S M. Mater Lett, 2008; 62: 2999[21] Liu J H, Zhang X L, Yu M, Li S M, Zhang J D. Small, 2012; 8: 310[22] Zhang X L, Yu M, Liu J H, Li S M. Mater Lett, 2011; 65: 719[23] Zhang J, Liu Y, Ke Y, Yan H. Nano Lett, 2006; 6: 248[24] Mirkin C A, Letsinger R L, Mucic R C, Storhoff J J. Nature, 1996; 382: 607[25] Keren K, Krueger M, Gilad R, Ben–Yoseph G, Sivan U, Braun E. Science, 2002; 297: 72[26] Braun E, Eichen Y, Sivan U, Ben–Yoseph G. Nature, 1998; 391: 775 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|