| 柱状晶对Fe-3%Si电工钢再结晶织构演变规律的影响 |
| 张宁, 杨平, 毛卫民 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| INFLUENCE OF COLUMNAR GRAINS ON THE RECRYSTALLIZATION TEXTURE EVOLUTION IN Fe-3%Si ELECTRICAL STEEL |
| ZHANG Ning, YANG Ping, MAO Weimin |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
张宁 杨平 毛卫民. 柱状晶对Fe-3%Si电工钢再结晶织构演变规律的影响[J]. 金属学报, 2012, 48(3): 307-314.
,
,
.
INFLUENCE OF COLUMNAR GRAINS ON THE RECRYSTALLIZATION TEXTURE EVOLUTION IN Fe-3%Si ELECTRICAL STEEL[J]. Acta Metall Sin, 2012, 48(3): 307-314.
| [1] Tomida T, Tanaka T. ISIJ Int, 1995; 35: 548[2] Kovac F, Dzubinsky M, Sidor Y. J Magn Magn Mater, 2004; 269: 333[3] Gutierrez–Castaneda E J, Salinas–Rodriguez A. J Magn Magn Mater, 2011; 323: 2524[4] Kurz W, Fisher D J. Acta Metall, 1981; 29: 11[5] Kovac F, Stoyka V, Petryshynets I. J Magn Magn Mater, 2008; 320: 627[6] Takashima M, Komatsubara M, Morito N. ISIJ Int, 1997; 37: 1263[7] Walter J L, Koch E F. Acta Metall, 1962; 10: 1059[8] Abe H, Matsuo M, Ito K. Trans JIM, 1962; 26: 684[9] Koh P K, Dunn C G. Trans AIME, 1955; 203: 401[10] Dunn C G. Acta Metall, 1954; 2: 173[11] Walter J L, Hibbard W R. Trans Metall Soc AIME, 1958; 212: 731[12] Dorner D, Zaefferer S, Lahn L, Raabe D. J Magn Magn Mater, 2006; 304: 183[13] Inagaki H, Suda T. Texture, 1972; 1: 129[14] Tsuji N, Tsuzaki K, Maki T. ISIJ Int, 1993; 33: 783[15] Tsuji N, Tsuzaki K, Maki T. ISIJ Int, 1994; 34: 1008[16] Park J T, Szpunar J A. Acta Mater, 2003; 51: 3037[17] Samajdar I, Cicale S, Verlinden B, Van Houtte P, Abbruzzesse G. Scr Mater, 1998; 39: 1083[18] Ushioda K, Hutchinson W B. ISIJ Int, 1989; 29: 862[19] Haratani T, Hutchinson W B, Dillamore I L, Bate P. Metall Sci, 1984; 18: 57[20] Stojakovic D, Doherty R D, Kalidindi S R, Landgraf F J G. Metall Mater Trans, 2008; 39A: 1738[21] Verbeken K, Gomes E, Schneider J, Houbaert Y. J Solid State Phenom, 2010; 160: 189[22] Wenk H R, Van Houtte P. Rep Prog Phys, 2004; 67: 1367[23] Dillamore I L, Morris P L, Smith C J E, Hutchinson W B. Proc Roy Soc Lond, 1972; 329A: 405[24] Dunn C G, Walter J L. Trans Metall Soc AIME, 1962; 224: 518[25] Walker E V, Howard J. Trans Metall Soc AIME, 1962; 224: 876 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|