| 定向凝固过程中NH4Cl-H2O枝晶生长的数值模拟 |
| 石玉峰, 许庆彦, 龚铭, 柳百成 |
| 清华大学机械工程系先进成形制造教育部重点实验室, 北京 100084 |
|
| SIMULATION OF NH4Cl-H2O DENDRITIC GROWTH IN DIRECTIONAL SOLIDIFICATION |
| SHI Yufeng, XU Qingyan, GONG Ming, LIU Baicheng |
| Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, Department of Mechanical Engineering, Tsinghua University, Beijing 100084 |
引用本文:
石玉峰 许庆彦 龚铭 柳百成. 定向凝固过程中NH4Cl-H2O枝晶生长的数值模拟[J]. 金属学报, 2011, 47(5): 620-627.
,
,
,
.
SIMULATION OF NH4Cl-H2O DENDRITIC GROWTH IN DIRECTIONAL SOLIDIFICATION[J]. Acta Metall Sin, 2011, 47(5): 620-627.
| [1] Hunt J D, Lu S Z. Metall Mater Trans, 1996; 27A: 611[2] Kurz W, Fisher D J. Acta Metall, 1981; 29: 11[3] Somboonsuk K, Trivedi R. Acta Metall, 1985; 33: 1051[4] Huang W, Geng X, Zhou Y. J Cryst Growth, 1993; 134: 105[5] Rappaz M, Gandin C A. Acta Metall, 1993; 41: 345[6] Gandin C A, Rappaz M, Tintillier R. Metall Mater Trans, 1994; 25A: 629[7] Nastac L. Acta Mater, 1999; 47: 4253[8] Beltran–Sanchez L, Stefanescu D M. Metall Mater Trans, 2004; 35A: 2471[9] WangW, Lee P D, McLean M. Acta Mater, 2003; 51: 2971[10] Zhu M F, Hong C P. ISIJ Int, 2001; 41: 436[11] Liu Y, Xu Q Y, Liu B C. Tsinghua Sci Technol, 2006; 11: 495[12] Shan B W, Huang W D, Lin X, Wei L. Acta Metall Sin, 2008; 44: 1042(单博炜, 黄卫东, 林鑫, 魏雷. 金属学报, 2008; 44: 1042)[13] Esaka H. PhD thesis, Ecole Polytechnique Federale de Lausanne, Switzerland, 1986[14] Hansen G, Liu S, Lu S Z, Hellawell A. J Cryst Growth, 2002; 234: 731[15] Bennon W D, Incropera F P. Metall Mater Trans, 1987; 18B: 611[16] Feng Y H, Nie H, Zhang X X. J Eng Thermoph, 2008; 29: 301(冯妍会, 聂红, 张欣欣. 工程热物理学报, 2008; 29: 301)[17] Yu J, Xu Q Y, Cui K, Liu B C. Acta Metall Sin, 2007; 43: 731 (于 靖, 许庆彦, 崔锴, 柳百成. 金属学报, 2007; 43: 731)[18] Li B, Xu Q Y, Pan D, Liu B C, Xiong Y C, Zhou Y J, Hong R Z. Acta Metall Sin, 2008; 44: 243(李 斌, 许庆彦, 潘冬, 柳百成, 熊艳才, 周永江, 洪润洲. 金属学报, 2008; 44: 243)[19] Chen J, Zhu M F, Sun G X. Acta Metall Sin, 2005; 41: 799(陈晋, 朱鸣芳, 孙国雄. 金属学报, 2005; 41: 799)[20] Kurz W, Giovanola B, Trivedi R. Acta Metall, 1986; 34: 823[21] Walton D, Chalmers B. Trans Metall Soc AIME, 1959; 215: 447[22] Langer J S, M¨uller–Krumbhaar H. Acta Metall, 1978; 26: 1681 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|