| 燃气轮机用大型定向结晶铸件制备及组织与性能研究 |
| 张健, 申健, 卢玉章, 楼琅洪 |
| 中国科学院金属研究所, 沈阳 110016 |
|
| PROCESSING, MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LARGE DIRECTIONALLY SOLIDIFIED CASTINGS FOR INDUSTRIAL GAS TURBINE APPLICATIONS |
| ZHANG Jian, SHEN Jian, LU Yuzhang, LOU Langhong |
| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
张健 申健 卢玉章 楼琅洪. 燃气轮机用大型定向结晶铸件制备及组织与性能研究[J]. 金属学报, 2010, 46(11): 1322-1326.
,
,
,
.
PROCESSING, MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LARGE DIRECTIONALLY SOLIDIFIED CASTINGS FOR INDUSTRIAL GAS TURBINE APPLICATIONS[J]. Acta Metall Sin, 2010, 46(11): 1322-1326.
| [1] Seth B B. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, Mclean M, Olson S, Schirra J J, eds., Superalloys 2000, Warrendale, PA: TMS, 2000: 3
[2] Konter M, Thumann M. J Mater Proc Technol, 2001; 117: 386
[3] Zhang J, Lou L H. J Mater Sci Technol, 2007; 23: 289
[4] Lohmueller A, EsserW, Grossmann J, Hoerdler M, Preuhs J, Singer R F. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, Mclean M, lson S, Schirra J J, eds., Superalloys 2000, Warrendale, PA: TMS, 2000: 181
[5] Tang W S, Shen J, Zhang J, Chen L J. J Shenyang Univ Technol, 2009; 31: 397
(唐文书, 申 健, 张 健, 陈立佳. 沈阳工业大学学报, 2009; 31: 397) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|