| 18Mn TRIP钢温变形过程中马氏体逆相变行为 |
| 鲁法云,杨平,孟利,毛卫民 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| BEHAVIOR OF MARTENSITE REVERSE TRANSFORMATION IN A HIGH MANGANESE TRIP STEEL DURING WARM DEFORMATION |
| LU Fayun, YANG Ping, MENG Li, MAO Weimin |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
鲁法云 杨平 孟利 毛卫民. 18Mn TRIP钢温变形过程中马氏体逆相变行为[J]. 金属学报, 2010, 46(10): 1153-1160.
,
,
,
.
BEHAVIOR OF MARTENSITE REVERSE TRANSFORMATION IN A HIGH MANGANESE TRIP STEEL DURING WARM DEFORMATION[J]. Acta Metall Sin, 2010, 46(10): 1153-1160.
| [1] Zhang F C, Lei T Q. Wear, 1997;212: 195
[2] Gr?ssel O, Krüger L, Frommeyer G, Meyer L W. Int J Plast, 2000; 16: 1391
[3] Frommeryer G, Brüx U, Neumann P. ISIJ Int, 2003; 43: 438
[4] Curtze S, Kuokkala V-T, Hokka M, Peura P. Mater Sci Eng, 2009; A507: 124
[5] Byun T S, Hashimoto N, Farrell K. Acta Mater, 2004; 52: 3889
[6] Sawaguchi T, Bujoreanu L-G, Kikuchi T, Ogawa K, Koyamaa M, Murakamic M. Scr Mater, 2008; 59: 826
[7] Bergeon N, Guenin G, Esnouf C. Mater Sci Eng, 1998; A242: 87
[8] Stalder M, Vogel S, Bourke M A M, Maldonado J G, Thoma D J, Yuan V W. Mater Sci Eng, 2000; A280: 270
[9]Gauzzi F, Montanari R, Principi G, Tata M E. Mater Sci Eng, 2006; A438-440: 202
[10] Tavares S S M, Fruchart D, Miraglia S. J Alloys Compd, 2000; 307: 311
[11] Kundu S, Bhadeshia H K D H. Scr Mater, 2007; 57: 869
[12] Kitahara H, Ueji R, Tsuji N, Minamino Y. Acta Mater, 2006; 54: 1279
[13] Zhang M-X, Kelly P M, Gates J D. Mater Sci Eng,1999; A273-275: 251
[14] Gauzzi F, Montanari R. Mater Sci Eng, 1999; A273-275: 524
[15] Lee Se-J, Park Y-M, Lee Y-K. Mater Sci Eng, 2009; A515: 32
[16] Leem D-S, Lee Y-D, Jun J-H, Choi C-S. Scr Mater, 2001; 45: 767
[17] Gey N, Petit B, Humbert M. Metall Mater Trans, 2005; A36: 3291
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|