| Cu/a—C:H双层膜的网络分形及Cu膜退炎缩聚 |
| 张人佶;王望弟;何大韧 |
| 清华大学机械系;北京100084;西北大学;西北大学 |
|
| NETWORK FRACTAL AND ANNEALING-INDUCED AGGREGATION OF Cu/a-C:H BILAYER FILMS |
| ZHANG Renji;WANG Wangdi;HE Daren Tsinghua University Northwest University; Xi'an Department of Mechanical Engineering;Tsinghua University;Beijing 100084 |
引用本文:
张人佶;王望弟;何大韧. Cu/a—C:H双层膜的网络分形及Cu膜退炎缩聚[J]. 金属学报, 1990, 26(4): 139-143.
,
,
.
NETWORK FRACTAL AND ANNEALING-INDUCED AGGREGATION OF Cu/a-C:H BILAYER FILMS[J]. Acta Metall Sin, 1990, 26(4): 139-143.
1 吴鹏,于明湘,刘买利,何大韧.应用激光,1988;8:200 2 Witten T A Jr., Sander L M. Phys Rev Lett, 1981; 47: 1400 3 Messier R. J Vac Sci Technol, 1986; A4: 490 4 Morchan B A, Demchishin A V. Phys Met Metallogr (USSR), 1969; 28: 83 5 Messier R, Yehoda J E. J Appl Phys, 1985; 58: 3739 6 张人佶,褚圣麟,吴自勤.物理学报,1986;35:365D |
|