| 电磁搅拌对灰铸铁宏观偏析的影响 |
| 曹志强;张丽萍;任忠鸣;金俊泽 |
| 大连理工大学;助教;大连(116023)大连理工大学铸造工程研究中心;大连理工大学;大连理工大学;大连理工大学 |
|
| INFLUENCE OF ELECTROMAGNETIC STIRRING ON MACRO-SEGREGATION OF GREY CAST IRON |
| CAO Zhiqiang;ZHANG Liping;REN Zhongming;JIN Junze Dalian University of Technology |
引用本文:
曹志强;张丽萍;任忠鸣;金俊泽. 电磁搅拌对灰铸铁宏观偏析的影响[J]. 金属学报, 1992, 28(2): 82-85.
,
,
,
.
INFLUENCE OF ELECTROMAGNETIC STIRRING ON MACRO-SEGREGATION OF GREY CAST IRON[J]. Acta Metall Sin, 1992, 28(2): 82-85.