| Bi在Fe液中的溶解平衡及Ni,Mn的影响 |
| 徐建伦;宋波;陈继开;韩其勇;蒋国昌 |
| 上海工业大学;北京科技大学;上海工业大学;北京科技大学理化系;教授;北京(100083);上海工业大学 |
|
| DISSOLUTION EQUILIBRIUM OF Bi VAPOUR IN LIQUID Fe AND INFLUENCE OF Ni AND Mn |
| XU Jianlun;CHEN Jikai;JIANG Guochang;SONG Bo;HAN Qiyong Shanghai University of Science and Technology; University of Science and Technology Beijing |
引用本文:
徐建伦;宋波;陈继开;韩其勇;蒋国昌. Bi在Fe液中的溶解平衡及Ni,Mn的影响[J]. 金属学报, 1993, 29(1): 65-68.
,
,
,
,
.
DISSOLUTION EQUILIBRIUM OF Bi VAPOUR IN LIQUID Fe AND INFLUENCE OF Ni AND Mn[J]. Acta Metall Sin, 1993, 29(1): 65-68.
1 Xu Jianlun, Sen Caipin, Yang Senglun, Jiang Guochang, Zhu Yuru, Wang Liguo, Chen Jikai, Chang Li. Bull Bismuth Inst, 1991; 62: 2 2 Jiang Guochang, Huang Keli, Zhuang Yunqian, Yang Senglong, Xu Kuangdi, Bull Bismuth Inst, 1989; 56: 2 3 木村笃良,中村贞行,柴田范嘉.日本金属学会会报,1987;26:425 4 Han Qiyong, Zhang Xiaodong, Chen Dong, Wang Pengfei. Metall Trans, 1988; 19B: 617 5 Zhang Xiaodong, Han Qiyong, Chen Dong. Proe of the 5th China-Japan Symposium on Science and Technology of Iron and Steel, Bejing: International Academic Publishers, 1989: 301 6 Hultgren R. Selected Values of the Thermodynamic Properties of the Elements, Metals Park, Ohio: ASM, 1973: 77 7 Lupis C H P. Chemiclal Thermodynamics of Materials. New York: North-Holland, 1983: 530 8 Fuwa T, Chipman J. Trans AIME, 1959; 215: 708 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|