| 高炉风口回旋区三维数学模型 |
| 陈义胜;贺友多 |
| 包头钢铁学院;包头钢铁学院 |
|
| MATHEMATICAL MODELLING OF RACEWAY IN BLAST FURNACE |
| CHEN Yisheng;HE Youduo Baotou University of Iron and Steel Technology |
引用本文:
陈义胜;贺友多. 高炉风口回旋区三维数学模型[J]. 金属学报, 1993, 29(10): 51-56.
,
.
MATHEMATICAL MODELLING OF RACEWAY IN BLAST FURNACE[J]. Acta Metall Sin, 1993, 29(10): 51-56.
1 Wagstaff J B, Holman W H. J Met, 1952; 4: 709 2 中村正和,杉山乔,鹈野健夫,原行明,近藤真一.铁钢,1977;63:28 3 稻谷稔宏,福武刚,滨田尚夫,近藤幹夫,冈部侠儿.铁钢,1976;62:25 4 羽田野道春,平冈文章,福田充一朗,增池保.铁钢,1976;62:505 5 成兰伯,曾祥明.钢铁,1982;17:54 6 Kase M, Sugata M, Yamaguchi K, Nakagome K. Trans Iron Steel Inst Jpn, 1982; 22. 811 7 Hillnhuter F W, Kister H, Kruger B. Ironmaking Proc, 1975; 34: 368 8 桑原守,谢裕生,鞭岩.铁钢,1980;66:1918 9 福武刚著,杜鹤桂译.高炉回旋区和炉缸工作文集,北京:冶金工业出版社,1986 10 Jamaluddin A S, Wall T F, Truelove J S. Ironmaking Steelmaking, 1986; 13: 91 11 桑原守,赫冀成,鞭岩.铁钢,1986;72:1847 12 王应时,范维澄,周力行,徐旭常.燃烧过程数值计算,北京:科学出版社,1986 13 谢裕生,车秀珍,李琪.钢铁,1985;20(10) :12 |
|