SiC晶须增强硬Al合金复合材料的界面析出及其对性能的影响 |
毕敬;马宗义;吕毓雄;宁小光;高荫轩 |
中国科学院金属研究所;副研究员;沈阳(110015);中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
EFFECT OF INTERFACIAL PRECIPITATION ON PROPERTIES OF SiC WHISKER REINFORCED Al ALLOY COMPOSITES |
BI Jing;MA Zongyi;LU Yuxiong;NING Xiaoguang;GAO Yinxuan Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
毕敬;马宗义;吕毓雄;宁小光;高荫轩. SiC晶须增强硬Al合金复合材料的界面析出及其对性能的影响[J]. 金属学报, 1993, 29(2): 92-96.
,
,
,
,
.
EFFECT OF INTERFACIAL PRECIPITATION ON PROPERTIES OF SiC WHISKER REINFORCED Al ALLOY COMPOSITES[J]. Acta Metall Sin, 1993, 29(2): 92-96.
1 Nutt S R, Duva J M. Scr Metall. 1986; 20: 1055 2 Ma Z Y, Liu J, Yao C K. J Mater Sci. 1991; 26: 1971 3 Nutt S R, Carpenter R W. Mater Sci Eng. 1985; 75: 169 4 Mahon G J, Howe J M, Vasudevan A K. Acta Metall Mater. 1990; 38: 1503v |
|