Please wait a minute...
金属学报  2026, Vol. 62 Issue (8): 1427-1442    DOI: 10.11900/0412.1961.2025.00157
  研究论文 本期目录 | 过刊浏览 |
Ti551合金的热变形行为及热加工图构建
尹建年1, 马英杰2, 杨锐2, 雷家峰2, 齐敏2(), 周丽1()
1 烟台大学 机电汽车工程学院 烟台 264005
2 中国科学院金属研究所 沈阳材料科学国家研究中心 沈阳 110016
Hot Deformation Behavior and Hot Processing Map Construction of the Ti551 Alloy
YIN Jiannian1, MA Yingjie2, YANG Rui2, LEI Jiafeng2, QI Min2(), ZHOU Li1()
1 School of Electromechanical and Vehicle Engineering, Yantai University, Yantai 264005, China
2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
引用本文:

尹建年, 马英杰, 杨锐, 雷家峰, 齐敏, 周丽. Ti551合金的热变形行为及热加工图构建[J]. 金属学报, 2026, 62(8): 1427-1442.
Jiannian YIN, Yingjie MA, Rui YANG, Jiafeng LEI, Min QI, Li ZHOU. Hot Deformation Behavior and Hot Processing Map Construction of the Ti551 Alloy[J]. Acta Metall Sin, 2026, 62(8): 1427-1442.

全文: PDF(7165 KB)   HTML
摘要: 

Ti551合金的热变形行为及其微观组织演变高度复杂,为拓展该合金的工程应用,需确定其热加工工艺窗口。本工作利用Gleeble-3500热模拟试验机在变形温度(T)为800~1100 ℃、应变速率(ε˙)为0.001~10 s-1条件下对Ti551合金进行热压缩实验,研究其热变形行为,构建热加工图并确定热加工窗口。在摩擦修正和温度修正的基础上,采用应变补偿Arrhenius (SCA)模型和反向传播人工神经网络(BPANN)模型建立了Ti551合金的本构关系,并通过统计分析对模型精度进行评估,发现BPANN模型在预测数据上表现出良好的拟合能力。基于动态材料模型建立Ti551合金的热加工图,确定其最佳加工区域为:ε˙ = 0.001~0.1 s-1、T = 900~1050 ℃。失稳区主要集中在高温高应变速率区域(T ≥ 1000 ℃、ε˙ ≥ 1 s-1)。变形温度和应变速率对应力影响显著,随着温度下降或应变速率增加,流变应力明显增加,体现了典型的热激活变形特征。微观组织分析表明,Ti551合金在热压缩过程中的组织演化与应变、温度和应变速率密切相关,应变越大,晶粒变形越显著,随温度的降低或应变速率的增大,动态再结晶晶粒尺寸明显细化。此外,Ti551合金热变形过程中的主要动态再结晶机制为连续动态再结晶和不连续动态再结晶。

关键词 : Ti551合金,  热变形行为,  本构方程,  热加工图,  微观组织    
Abstract:

The Ti551 alloy exhibits exceptional thermal stability, retaining over 80% of its room-temperature strength within 300-400 oC, outperforming most α-type Ti alloys. Consequently, it has emerged as the primary structural material for applications in extreme operating environments, such as deep-sea oil drilling pipes. Despite this advantage, the Ti551 alloy exhibits considerably complex thermal deformation behavior and microstructural evolution. Establishing the alloy's precise hot processing window is critical to broaden its engineering applications. Therefore, this study investigated the thermal deformation behavior of the Ti551 alloy using a Gleeble-3500 thermal simulation tester. Specifically, isothermal compression tests were conducted over the temperatures (T) of 800-1100 oC and a strain rate (ε˙) of 0.001-10 s-1. Considering friction and temperature corrections, strain-compensated Arrhenius (SCA) and back-propagation artificial neural network (BPANN) models were selected to establish a constitutive model of the Ti551 alloy. The accuracies of both models were evaluated using the correlation coefficient, average absolute relative error, and relative error. The results demonstrate that the BPANN model outperformed the SCA model, yielding superior accuracy in predicting the flow stress. Thereafter, a hot processing map was constructed based on the dynamic materials model, and the corresponding microstructural evolution during thermal compression was systematically analyzed. Analysis of the hot processing map identified the optimal processing window with the following parameters: ε˙ = 0.001-0.1 s-1 and T = 900-1050 oC. Additionally, the instability zone was primarily concentrated in the high-T, high-ε˙ region (T ≥ 1000 °C, ε˙ ≥ 1 s-1). These findings demonstrate that the deformation T and ε˙ substantially influenced the flow stress. Specifically, the flow stress markedly increased with the decrease in T or increase in ε˙. During hot compression, the microstructural evolution of the Ti551 alloy exhibited a close relationship with T and ε˙, and the dynamic recrystallized grain size notably decreased as T decreased or ε˙ increased. Furthermore, the dominant dynamic recrystallization (DRX) mechanisms during hot deformation comprised continuous and discontinuous DRX processes.

Key words: Ti551 alloy    hot deformation behavior    constitutive equation    hot processing map    microstructure
收稿日期: 2025-06-06     
ZTFLH:  TG146.23  
基金资助:国家重点研发计划项目(2024YFB3714201);山东省自然科学基金项目(ZR2023ME097)
通讯作者: 齐 敏,mqi17s@imr.ac.cn,主要从事结构钛合金研究; 周 丽,lizhou@ytu.edu.cn,主要从事复合材料成形加工研究
Corresponding author: QI Min, Tel: 18742418386, E-mail: mqi17s@imr.ac.cn; ZHOU Li, professor, Tel: 13889124507, E-mail: lizhou@ytu.edu.cn
作者简介: 尹建年,男,2001年生,硕士生
图1  热压缩实验示意图
图2  Ti551合金初始微观组织的SEM像和EBSD结果
图3  Ti551合金在不同热压缩条件下真应力-应变曲线及经摩擦修正、温度修正后的真应力-应变曲线
图4  Ti551合金在不同热压缩条件下的温度变化
图5  lnε˙-lnσ、lnε˙-σ、lnε˙-ln[sinh(ασ)]、ln[sinh(ασ)]-T-1和lnZ-ln[sinh(ασ)]的拟合曲线
εQ / (J·mol-1)lnAnα / MPa-1
0.10155144.7412.06712.87800.01426
0.15151640.3711.81662.93790.01389
0.20145891.0411.41702.95330.01375
0.25143261.6311.04922.96860.01374
0.30140042.8510.73652.97040.01373
0.35138616.4310.66232.99570.01372
0.40135233.8810.32182.99920.01371
0.45132736.4510.09403.03690.01372
0.50129037.869.71583.07270.01375
0.55125617.229.38483.09670.01374
0.60121303.178.96103.12850.01372
0.65119952.938.85743.18010.01364
表1  不同真应变时的材料常数
图6  材料常数与真应变的关系曲线
图7  反向传播人工神经网络(BPANN)模型结构图
图8  隐藏层中的神经元数量对均方误差(MSE)的影响
图9  不同热压缩条件下流变应力预测值与实验值对比
图10  应变补偿Arrhenius (SCA)模型和BPANN模型中流变应力预测值与实验值的比较及相对误差分布
图11  Ti551合金的热压缩有限元模型和上模的载荷-行程曲线
图12  不同真应变下Ti551合金的功率耗散图
图13  Ti551合金在不同真应变下的失稳图
图14  Ti551合金在不同真应变下的热加工图
图15  Ti551合金在真应变为0.69时不同热压缩条件下微观组织的OM像(a) 900 oC, 0.01 s-1 (b)1000 oC, 0.01 s-1(c)1100 oC, 0.01 s-1 (d) 1100 oC, 1 s-1 (e) 1100 oC, 10 s-1
图16  Ti551合金在应变为0.69时不同热压缩条件下的反极图(a) 900 oC, 0.01 s-1 (b)1000 oC, 0.01 s-1(c)1100 oC, 0.01 s-1 (d) 1100 oC, 1 s-1 (e) 1100 oC, 10 s-1
图17  Ti551合金在应变为0.69时不同热压缩条件下的局部取向差(KAM)分布图(a) 900 oC, 0.01 s-1 (b)1000 oC, 0.01 s-1(c)1100 oC, 0.01 s-1 (d) 1100 oC, 1 s-1 (e) 1100 oC, 10 s-1
图18  Ti551合金在1000 ℃、1 s-1变形条件下的应变场分布和不同区域微观组织的OM像
[1] Zhang M C, Xu Q S, Liu Y, et al. Effect of hot-pressing temperature on the microstructure and properties of the diffusion-bonded region of TC4 alloy [J]. Acta Metall. Sin., 2025, 61: 1183
[1] 张洺川, 徐勤思, 刘 意 等. 热压温度对TC4合金扩散连接区组织与性能的影响 [J]. 金属学报, 2025, 61: 1183
[2] Yang L, Yu S M, Zhan C, et al. Dynamic recrystallization and texture evolution of a novel near-α Ti-6Al-1Mo-2Zr-0.55Fe-0.1B alloy during hot compression [J]. J. Mater. Res. Technol., 2025, 36: 4803
[3] Zhan J W, Ma C H, Liu J L, et al. Improved dynamic impact behavior of TC4 alloy coated with Ti-SiC [J]. Mater. Lett., 2025, 395: 138727
[4] Deng Y C, An Y X, Xiao Y Z H, et al. Deformation mechanism diagram and deformation instability of a Ti-5Al-5Mo-5V-1Cr-1Fe titanium alloy during the hot compression [J]. J. Alloys Compd., 2023, 966: 171446
[5] Zhang H B, Peng H A, Zhou H P, et al. Hot compression behavior and dynamic recrystallization mechanisms of Ti-5Mo-5V-8Cr-3Al alloy [J]. J. Alloys Compd., 2025, 1014: 178727
[6] Liu C C, Li Y H Z, Gu J, et al. Effect of high-strain-rate hot compression on the microstructural evolution and flow behaviors of Ti-55511 alloy [J]. Mater. Sci. Eng., 2025, A937: 148436
[7] Mao Y C, Liu X H, Wang Y, et al. Mechanical behaviour and microstructural evolution of Ti-6Al-1Mo-1V-2Zr-2Cr-1Fe alloy subjected to hot compression deformation [J]. J. Mater. Res. Technol., 2023, 27: 2548
[8] Sun T L, Cao J, Guo Z C, et al. Thermomechanical behaviour of Ti-42.5Al-4Nb-0.5Mo-0.1B-(C, W, Y) alloy during hot compression [J]. Mater. Today Commun., 2023, 34: 105186
[9] Wang Y Q, Shen Y F, Jia N, et al. Dynamic recrystallization and constitutive equation of 15Cr-10Mn-Ni-N steel under hot deformation [J]. Mater. Today Commun., 2023, 35: 105648
[10] Liu Q Q, Lu Y, Zhang Y F, et al. Thermal deformation behavior of Al19.3Co15Cr15Ni50.7 high entropy alloy [J]. Acta Metall. Sin., 2021, 57: 1299
[10] 刘庆琦, 卢 晔, 张翼飞 等. Al19.3Co15Cr15Ni50.7高熵合金的热变形行为 [J]. 金属学报, 2021, 57: 1299
[11] Zhao X J, Cao S G, Fan C L, et al. Hot deformation behavior of a 4Al alumina-forming austenitic heat-resistant steel: Constitutive equation, prediction model, processing map and dynamic recrystallization mechanism [J]. J. Mater. Res. Technol., 2025, 35: 7084
[12] Zhu P, Yang S, Gao Z J, et al. Optimization of hot deformation parameters for multi-directional forging of Ti65 alloy based on the integration of processing maps and finite element method [J]. J. Mater. Res. Technol., 2024, 29: 5271
[13] Wang T, Chen Y Z, Ouyang B, et al. Artificial neural network modified constitutive descriptions for hot deformation and kinetic models for dynamic recrystallization of novel AZE311 and AZX311 alloys [J]. Mater. Sci. Eng., 2021, A816: 141259
[14] Shi S X, Liu X S, Zhang X Y, et al. Comparison of flow behaviors of near beta Ti-55511 alloy during hot compression based on SCA and BPANN models [J]. Trans. Nonferrous Met. Soc. China, 2021, 31: 1665
[15] Peng W W, Zeng W D, Wang Q J, et al. Comparative study on constitutive relationship of as-cast Ti60 titanium alloy during hot deformation based on Arrhenius-type and artificial neural network models [J]. Mater. Des., 2013, 51: 95
[16] Zamani M R, Mirzadeh H, Malekan M. Artificial neural network applicability in studying hot deformation behaviour of high-entropy alloys [J]. Mater. Sci. Technol., 2023, 39: 3351
[17] Ebrahimi R, Najafizadeh A. A new method for evaluation of friction in bulk metal forming [J]. J. Mater. Process. Technol., 2004, 152: 136
[18] Han Y, Qiao G J, Sun J P, et al. A comparative study on constitutive relationship of as-cast 904L austenitic stainless steel during hot deformation based on Arrhenius-type and artificial neural network models [J]. Comput. Mater. Sci., 2013, 67: 93
[19] Han Y Z, Zhu H C, Qu J L, et al. Flow stress and dynamic recrystallization behavior and modeling of GH4738 superalloy during hot compression [J]. J. Mater. Res. Technol., 2023, 26: 4957
[20] Sellars C M, McTegart W J. On the mechanism of hot deformation [J]. Acta Metall., 1966, 14: 1136
[21] Ni K, Yang Y H, Cao J C, et al. Softening behavior of 18.7Cr-1.0Ni-5.8Mn-0.2N low nickel-type duplex stainless steel during hot compression deformation under large strain [J]. Acta Metall. Sin., 2021, 57: 224
[21] 倪 珂, 杨银辉, 曹建春 等. 18.7Cr-1.0Ni-5.8Mn-0.2N节Ni型双相不锈钢的大变形热压缩软化行为 [J]. 金属学报, 2021, 57: 224
[22] Dong X M, Xu J, Feng Z X, et al. Exploring hot deformation behavior of the solutionized Cu-15Ni-8Sn alloy through constitutive equations and processing maps [J]. J. Mater. Res. Technol., 2024, 29: 2142
[23] Kareem S A, Anaele J U, Aikulola E O, et al. Hot deformation behavior of aluminum alloys: A comprehensive review on deformation mechanism, processing maps analysis and constitutive model description [J]. Mater. Today Commun., 2025, 44: 112004
[24] Huang B, Yu Y, Ye W J, et al. Hot deformation behavior and constitutive equation of TA15N titanium alloy [J]. Materials, 2025, 18: 2067
[25] Li Q Q, Wen J, Wang G S, et al. Strain-compensated constitutive model and hot processing map for extruded Al-Mg-Mn-Ti alloy based on reheating deformation behavior [J]. Mater. Today Commun., 2025, 42: 111492
[26] Wei Z X, Gao Q, Su X X, et al. Flow characteristics, ANN-based prediction, 3D processing map, and interface microstructure of titanium/stainless steel bimetallic composite [J]. J. Mater. Res. Technol., 2024, 29: 2918
[27] Asghari E, Hayati R, Momeni A, et al. Predicting the flow stress of Inconel 617 superalloy using constitutive equation and artificial neural network approach [J]. Mater. Today Commun., 2025, 43: 111690
[28] Chai Y P, Zhu Y C, Qin L, et al. High-temperature hot deformation behavior and processing map of Ti-22Al-25Nb alloy [J]. Mater. Today Commun., 2024, 41: 110599
[29] Bao C L, LI H, Hu L, et al. Construction of hot processing map of solutionized Mg-10Gd-6Y-1.5Zn-0.5Zr alloy and microstructure evolution [J]. Acta Metall. Sin., 2025, 61: 632
[29] 包成利, 李 豪, 胡 励 等. 固溶态Mg-10Gd-6Y-1.5Zn-0.5Zr合金热加工图构建及微观组织演变 [J]. 金属学报, 2025, 61: 632
[30] Zarghani F, Ebrahimi G R, Taheri J, et al. Hot compressive deformation behavior of Ti-8Al-1Mo-1V titanium alloy at elevated temperatures: Focus on flow behavior, constitutive modeling, and processing maps [J]. Mater. Today Commun., 2023, 37: 107235
[1] 杨坤, 郭庆伟, 李超, 张高龙, 赵宇宏, 侯华. 冲击加载下60钢的动态力学响应及层裂行为[J]. 金属学报, 2026, 62(8): 1405-1416.
[2] 杨何, 侯自勇, 胡兴益, 程金骏, 王亚茹, 范国华, 黄晓旭. 超高强不锈钢微丝表征技术:进展与展望[J]. 金属学报, 2026, 62(7): 1189-1206.
[3] 王玮, 张宇博, 赵燕, 王同敏, 李廷举. 高熵合金颗粒对选区激光熔化Al12Si合金固溶组织和力学性能的影响[J]. 金属学报, 2026, 62(6): 1009-1020.
[4] 王彬, 赵鹏, 刘家伟, 张春波, 秦志伟, 董红刚, 李鹏. 热处理对FGH96高温合金惯性摩擦焊接头微观组织演变及力学性能的影响[J]. 金属学报, 2026, 62(6): 1043-1058.
[5] 郭恩宇, 杜泽龙, 李炳志, 王同敏. 基于同步辐射原位表征技术的镁合金研究进展[J]. 金属学报, 2026, 62(5): 890-904.
[6] 陆善平, 孙健. 高强钢焊缝金属组织设计与强韧化机理研究进展[J]. 金属学报, 2026, 62(1): 1-16.
[7] 阴嘉琳, 石磊, 武传松. 超声振动对镁/铝异质合金搅拌摩擦搭接焊接头界面组织演变的影响[J]. 金属学报, 2026, 62(1): 133-147.
[8] 李红, 姜玉清, 曹玉鹏, 王加友, 刘澍彬. 冷丝辅助旋转/摇动电弧窄间隙MAG焊缝成形特性及接头组织性能演变机制[J]. 金属学报, 2026, 62(1): 235-252.
[9] 王洪瑛, 姚志浩, 李大禹, 郭婧, 姚凯俊, 董建新. 高 γ' 相含量粉末及变形高温合金组织和力学性能的异同性[J]. 金属学报, 2025, 61(9): 1364-1374.
[10] 肖文龙, 臧晨阳, 郭锦涛, 冯佳文, 马朝利. 基于原位电阻法的7A65铝合金厚板双级时效工艺[J]. 金属学报, 2025, 61(8): 1153-1164.
[11] 吴泽威, 颜俊雄, 胡励, 韩修柱. 双峰分离非基面织构AZ31镁合金板材反常中温轧制变形行为及机理[J]. 金属学报, 2025, 61(8): 1165-1173.
[12] 谢旭, 万一博, 钟明, 邹晓东, 王聪. CaF2-TiO2 焊剂作用下EH36船板钢气电立焊焊缝金属组织优化及力学性能调控[J]. 金属学报, 2025, 61(7): 998-1010.
[13] 孙欢腾, 马运柱, 蔡青山, 王健宁, 段有腾, 张梦祥. fcc和bcc钢板在超高速撞击下的微观组织差异[J]. 金属学报, 2025, 61(7): 1011-1023.
[14] 郝旭邦, 程伟丽, 李戬, 王利飞, 崔泽琴, 闫国庆, 翟凯, 余晖. 低合金化Mg-Ag镁空气电池阳极材料的电化学行为和放电性能[J]. 金属学报, 2025, 61(6): 837-847.