| 表面喷丸处理对NiCrAlYSi涂层恒温氧化行为的影响 |
刘冠熙, 黄光宏, 罗学昆, 申造宇, 何利民( ), 李建平, 牟仁德 |
| 中国航发北京航空材料研究院 航空材料先进腐蚀与防护重点实验室 北京 100095 |
|
| The Influence of Surface Shot Peening on the Isothermal Oxidation Behavior of NiCrAlYSi Coating |
LIU Guanxi, HUANG Guanghong, LUO Xuekun, SHEN Zaoyu, HE Limin( ), LI Jianping, MU Rende |
| Aviation Key Laboratory of Science and Technology on Advanced Corrosion and Protection for Aviation Material, AECC Beijing Institute of Aeronautical Materials, Beijing 100095, China |
引用本文:
刘冠熙, 黄光宏, 罗学昆, 申造宇, 何利民, 李建平, 牟仁德. 表面喷丸处理对NiCrAlYSi涂层恒温氧化行为的影响[J]. 金属学报, 2021, 57(5): 684-692.
Guanxi LIU,
Guanghong HUANG,
Xuekun LUO,
Zaoyu SHEN,
Limin HE,
Jianping LI,
Rende MU.
The Influence of Surface Shot Peening on the Isothermal Oxidation Behavior of NiCrAlYSi Coating[J]. Acta Metall Sin, 2021, 57(5): 684-692.
| 1 |
Padture N P, Gell M, Jordan E H. Thermal barrier coatings for gas-turbine engine applications [J]. Science, 2002, 296: 280
|
| 2 |
Clarke D R, Oechsner M, Padture N P. Thermal-barrier coatings for more efficient gas-turbine engines [J]. MRS Bull., 2012, 37: 891
|
| 3 |
Cao X Q. New Materials and Structures of Thermal Barrier Coatings [M]. Beijing: Science Press, 2016: 20
|
| 3 |
曹学强. 热障涂层新材料和新结构 [M]. 北京: 科学出版社, 2016: 20
|
| 4 |
Xu H B, Gong S K, Liu F S. Recent development in materials design of thermal barrier coatings for gas turbine [J]. Acta Aeronaut. Astronaut. Sin., 2000, 21: 7
|
| 4 |
徐惠彬, 宫声凯, 刘福顺. 航空发动机热障涂层材料体系的研究 [J]. 航空学报, 2000, 21: 7
|
| 5 |
Vaßen R, Jarligo M O, Steinke T, et al. Overview on advanced thermal barrier coatings [J]. Surf. Coat. Technol., 2010, 205: 938
|
| 6 |
Brandl W, Grabke H J, Toma D, et al. The oxidation behavior of sprayed MCrAlY coatings [J]. Surf. Coat. Technol., 1996, 86: 41
|
| 7 |
Yu D Q, Lu X Y, Ma J, et al. Study of oxidation behavior of the gradient NiCrAlY coating at 1000 and 1100oC [J]. Acta Metall. Sin., 2012, 48: 759
|
| 7 |
于大千, 卢旭阳, 马 军等. 梯度NiCrAlY涂层的1000和1100℃氧化行为研究 [J]. 金属学报, 2012, 48: 759
|
| 8 |
Feng Y, Dong T S, Li G L, et al. High temperature oxidation resistance and TGO growth mechanism of laser remelted thermal barrier coatings [J]. J. Alloys Compd., 2020, 828: 154266
|
| 9 |
Guan H R, Li M H, Sun X F, et al. Investigation on oxidation and failure of the thermal barrier coating deposited on superalloy [J]. Acta Metall. Sin., 2002, 38: 1133
|
| 9 |
管恒荣, 李美姮, 孙晓峰等. 高温合金热障涂层的氧化和失效研究 [J]. 金属学报, 2002, 38: 1133
|
| 10 |
Li M H, Zhang Z Y, Sun X F, et al. High temperature oxidation behavior of a EBPVD thermal barrier coating [J]. Acta Metall. Sin., 2002, 38: 989
|
| 10 |
李美姮, 张重远, 孙晓峰等. 电子束物理气相沉积热障涂层的高温氧化行为 [J]. 金属学报, 2002, 38: 989
|
| 11 |
Torkashvand K, Poursaeidi E, Mohammadi M. Effect of TGO thickness on the thermal barrier coatings life under thermal shock and thermal cycle loading [J]. Ceram. Int., 2018, 44: 9283
|
| 12 |
Tolpygo V K, Clarke D R, Murphy K S. Oxidation-induced failure of EB-PVD thermal barrier coatings [J]. Surf. Coat. Technol., 2001, 146-147: 124
|
| 13 |
Tolpygo V K, Clarke D R. Surface rumpling of a (Ni, Pt)Al bond coat induced by cyclic oxidation [J]. Acta Mater., 2000, 48: 3283
|
| 14 |
Balint D S, Kim S S, Liu Y F, et al. Anisotropic TGO rumpling in EB-PVD thermal barrier coatings under in-phase thermomechanical loading [J]. Acta Mater., 2011, 59: 2544
|
| 15 |
Davis A W, Evans A G. Effects of bond coat misfit strains on the rumpling of thermally grown oxides [J]. Metall. Mater. Trans., 2006, 37A: 2085
|
| 16 |
Shen Z Y, Huang G H, He L M, et al. Effect of surface treatments on lifetime and failure mechanism of thermal barrier coatings [J]. Rare Met. Mater. Eng., 2016, 45: 776
|
| 16 |
申造宇, 黄光宏, 何利民等. 表面处理对热障涂层寿命及失效机理的影响 [J]. 稀有金属材料与工程, 2016, 45: 776
|
| 17 |
Zhang D B, Gong S K, Xu H B, et al. Effect of bond coat surface roughness on the thermal cyclic behavior of thermal barrier coatings [J]. Surf. Coat. Technol., 2006, 201: 649
|
| 18 |
Tolpygo V K, Clarke D R, Murphy K S. The effect of grit blasting on the oxidation behavior of a platinum-modified nickel-aluminide coating [J]. Metall. Mater. Trans., 2001, 32A: 1467
|
| 19 |
Zhang H W, Zhang Y D, Wu Q. Numerical simulations of shot-peening process and impact effect [J]. Acta Metall. Sin., 2010, 46: 111
|
| 19 |
张洪伟, 张以都, 吴 琼. 喷丸强化过程及冲击效应的数值模拟 [J]. 金属学报, 2010, 46: 111
|
| 20 |
Zhang J W, Lu L T, Zhang W H. Analysis on fatigue property of microshot peened medium carbon steel [J]. Acta Metall. Sin., 2009, 45: 1378
|
| 20 |
张继旺, 鲁连涛, 张卫华. 微粒子喷丸中碳钢疲劳性能分析 [J]. 金属学报, 2009, 45: 1378
|
| 21 |
Karaoglanli A C, Doleker K M, Demirel B, et al. Effect of shot peening on the oxidation behavior of thermal barrier coatings [J]. Appl. Surf. Sci., 2015, 354: 314
|
| 22 |
Guinard C, Montay G, Guipont V, et al. Residual stress analysis of laser-drilled thermal barrier coatings involving various bond coats [J]. J. Therm. Spray Technol., 2015, 24: 252
|
| 23 |
Ma K K, Schoenung J M. Isothermal oxidation behavior of cryomilled NiCrAlY bond coat: Homogeneity and growth rate of TGO [J]. Surf. Coat. Technol., 2011, 205: 5178
|
| 24 |
Tomimatsu T, Zhu S, Kagawa Y. Effect of thermal exposure on stress distribution in TGO layer of EB-PVD TBC [J]. Acta Mater., 2003, 51: 2397
|
| 25 |
Naumenko D, Shemet V, Singheiser L, et al. Failure mechanisms of thermal barrier coatings on MCrAlY-type bondcoats associated with the formation of the thermally grown oxide [J]. J. Mater. Sci., 2009, 44: 1687
|
| 26 |
Shen Z Y, Zhong B T, He L M, et al. LaZrCeO/YSZ TBCs by EB-PVD: Microstructural evolution, residual stress and degradation behavior [J]. Mater. Chem. Front., 2019, 3: 892
|
| 27 |
Shen Z Y, He L M, Xu Z H, et al. Morphological evolution and failure of LZC/YSZ DCL TBCs by electron beam-physical vapor deposition [J]. Materialia, 2018, 4: 340
|
| 28 |
Shen Z Y, He L M, Mu R D, et al. Effects of gradient transitional layer on thermal cycling life and failure of LaZrCeO/YSZ thermal barrier coatings [J]. Corros. Sci., 2020, 163: 108224
|
| 29 |
Sauer T, translated by Pei Y R, Ma G Y. Numerical Analysis [M]. Beijing: China Machine Press, 2014: 124
|
| 29 |
Sauer T著, 裴玉茹, 马赓宇译. 数值分析 [M]. 北京: 机械工业出版社, 2014: 124
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|