| 弥散固态颗粒对Al-Bi合金液-液相分离过程的影响 |
张林,满田囡,王恩刚( ) |
| 东北大学材料电磁过程研究教育部重点实验室 沈阳 110819 |
|
| Influence of Dispersed Solid Particles on the Liquid-Liquid Separation Process of Al-Bi Alloys |
Lin ZHANG,Tiannan MAN,Engang WANG( ) |
| Key Laboratory of Electromagnetic Processing of Materials Ministry of Education, Northeastern University, Shenyang 110819, China |
引用本文:
张林,满田囡,王恩刚. 弥散固态颗粒对Al-Bi合金液-液相分离过程的影响[J]. 金属学报, 2019, 55(3): 399-409.
Lin ZHANG,
Tiannan MAN,
Engang WANG.
Influence of Dispersed Solid Particles on the Liquid-Liquid Separation Process of Al-Bi Alloys[J]. Acta Metall Sin, 2019, 55(3): 399-409.
| [1] | Ratke L, Diefenbach S. Liquid immiscible alloys [J]. Mater. Sci. Eng., 1995, R15: 263 | | [2] | Manasijević D, Minić D, Balanović L, et al. Experimental investigation and thermodynamic prediction of the Al-Bi-In phase diagram [J]. J. Alloys Compd., 2016, 687: 969 | | [3] | Carlberg T, Fredriksson H. The influence of microgravity on the solidification of Zn-Bi immiscible alloys [J]. Metall. Trans., 1980, 11A: 1665 | | [4] | Huang Q, Luo X H, Li Y Y. An alloy solidification experiment conducted on Shenzhou spacecraft [J]. Adv. Space Res., 2005, 36: 86 | | [5] | Andrews J B, Briggs C J, Robinson M B. Containerless low gravity processing of immiscible gold-rhodium alloys [R]. Alabama: Marshall Space Flight Center, 1990 | | [6] | Wang N, Zhang L, Peng Y L, et al. Composition-dependence of core-shell microstructure formation in monotectic alloys under reduced gravity conditions [J]. J. Alloys Compd., 2016, 663: 379 | | [7] | Chen S, Zhao J Z. Solidification of monotectic alloy under laser surface treatment conditions [J]. Acta Metall. Sin., 2013, 49: 537 | | [7] | 陈 书, 赵九洲. 偏晶合金在激光表面处理条件下的凝固行为研究 [J]. 金属学报, 2013, 49: 537 | | [8] | Li Z Q, Wang W L, Zhai W, et al. Formation mechanism of layered microstructure and monotectic cell within rapidly solidified Fe62.1Sn27.9Si10 alloy [J]. Acta Phys. Sin., 2011, 60: 705 | | [8] | 李志强, 王伟丽, 翟 薇等. 快速凝固Fe62.1Sn27.9Si10合金的分层组织和偏晶胞形成机理 [J]. 物理学报, 2011, 60: 705 | | [9] | Wei B, Herlach D M, Sommer F, et al. Rapid solidification of undercooled eutectic and monotectic alloys [J]. Mater. Sci. Eng., 1993, A173: 355 | | [10] | Luo S B, Wang W L, Chang J, et al. A comparative study of dendritic growth within undercooled liquid pure Fe and Fe50Cu50 alloy [J]. Acta Mater., 2014, 69: 355 | | [11] | Zhao L, Jiang H X, Ahmad T, et al. Study of solidification for gas-atomized droplet of Cu-Co-Fe alloy [J]. Acta Metall. Sin., 2015, 51: 883 | | [11] | 赵 雷, 江鸿翔, Ahmad T等. Cu-Co-Fe合金雾化合金液滴凝固过程研究 [J]. 金属学报, 2015, 51: 883 | | [12] | Zhai W, Liu H M, Zuo P F, et al. Effect of power ultrasound on microstructural characteristics and mechanical properties of Al81.3Sn12.3Cu6.4 monotectic alloy [J]. Prog. Nat. Sci., 2015, 25: 471 | | [13] | Da D A, Jiang W S, Wang Y M. Process of binary monotectic alloy under simulated microgravity effect by electromagnetic force [J]. Chin. Space Sci. Technol., 1988, 8(6): 20 | | [13] | 达道安, 姜万顺, 王毓敏. 用电磁力模拟空间微重力效应制备二元偏晶合金 [J]. 中国空间科学技术, 1988, 8(6): 20) | | [14] | Jiang H X, He J, Zhao J Z. Influence of electric current pulses on the solidification of Cu-Bi-Sn immiscible alloys [J]. Sci. Rep., 2015, 5: 12680 | | [15] | Zhang L, Wang E G, Zuo X W, et al. Effect of high magnetic field on solidified structure of Cu-80%Pb hypermonotectic alloy [J]. Acta Metall. Sin., 2008, 44: 165 | | [15] | 张 林, 王恩刚, 左小伟等. 强磁场对Cu-80%Pb过偏晶合金凝固组织的影响 [J]. 金属学报, 2008, 44: 165 | | [16] | He J, Zhao J Z, Wang X F, et al. Investigation of rapid directional solidification of Al-based immiscible alloys Ⅱ. Effect of static magnetic field [J]. Acta Metall. Sin., 2007, 43: 567 | | [16] | 何 杰, 赵九洲, 王晓峰等. Al基难混溶合金快速定向凝固研究Ⅱ. 恒定磁场的影响 [J]. 金属学报, 2007, 43: 567 | | [17] | Yasuda H, Ohnaka I, Kawakami O, et al. Effect of magnetic field on solidification in Cu-Pb monotectic alloys [J]. ISIJ Int., 2003, 43: 942 | | [18] | Zhang L, Man T N, Huang M H, et al. Numerical simulation of droplets behavior of Cu-Pb immiscible alloys solidifying under magnetic field [J]. Materials, 2017, 10: 1005 | | [19] | Kaban I G, Hoyer W. Characteristics of liquid-liquid immiscibility in Al-Bi-Cu, Al-Bi-Si, and Al-Bi-Sn monotectic alloys: Differential scanning calorimetry, interfacial tension, and density difference measurements [J]. Phys. Rev., 2008, 77B: 125426 | | [20] | Zhang H W, Xian A P. Effect of the third element on the structure of casting Al-Bi immiscible alloys [J]. Acta Metall. Sin., 2000, 36: 347 | | [20] | 张宏闻, 冼爱平. 第三组元对Al-Bi偏晶合金凝固组织的影响 [J]. 金属学报, 2000, 36: 347 | | [21] | He J, Zhao J Z, Wang X F, et al. Investigation of rapid directional solidification of Al-based immiscible alloys Ⅲ. Effect of the third element [J]. Acta Metall. Sin., 2007, 43: 573 | | [21] | 何 杰, 赵九洲, 王晓峰等. Al基难混溶合金快速定向凝固研究Ⅲ.第三组元的影响 [J]. 金属学报, 2007, 43: 573 | | [22] | Kaban I, K?hler M, Ratke L, et al. Phase separation in monotectic alloys as a route for liquid state fabrication of composite materials [J]. J. Mater. Sci., 2012, 47: 8360 | | [23] | Sun Q, Jiang H X, Zhao J Z, et al. Effect of TiC particles on the liquid-liquid decomposition of Al-Pb alloys [J]. Mater. Des., 2016, 91: 361 | | [24] | Sun Q, Jiang H X, Zhao J Z, et al. Microstructure evolution during the liquid-liquid phase transformation of Al-Bi alloys under the effect of TiC particles [J]. Acta Mater., 2017, 129: 321 | | [25] | Zhang L, Wang E G, Zuo X W, et al. Effect of magnetic field on liquid-liquid separation of Cu-Pb-La hypermonotectic alloy [J]. Rare Met. Mater. Eng., 2015, 44: 344 | | [25] | 张 林, 王恩刚, 左小伟等. 磁场对Cu-Pb-La过偏晶合金液-液分离的作用 [J]. 稀有金属材料与工程, 2015, 44: 344 | | [26] | Nestler B, Wheeler A A, Ratke L, et al. Phase-field model for solidification of a monotectic alloy with convection [J]. Physica, 2000, 141D: 133 | | [27] | Farjami S, Koyama T, Kainuma R, et al. Phase-field simulation of dragging of liquid Bi particles during the thermally activated migration of grain boundaries in the Al-Bi system [J]. Scr. Mater., 2007, 56: 433 | | [28] | Ratke L. Coarsening of liquid Al-Pb dispersions under reduced gravity conditions [J]. Mater. Sci. Eng., 1995, A203: 399 | | [29] | Zhao J Z, Ratke L. A model describing the microstructure evolution during a cooling of immiscible alloys in the miscibility gap [J]. Scr. Mater., 2004, 50: 543 | | [30] | Li H L, Zhao J Z, Zhang Q X, et al. Microstructure formation in a directionally solidified immiscible alloy [J]. Metall. Mater. Trans., 2008, 39A: 3308 | | [31] | Patankar S V. Numerical Heat Transfer and Fluid Flow [M]. New York: Mcgraw-Hill, 1980: 13 | | [32] | Ratke L, Voorhees P W. Growth and Coarsening: Ostwald Ripening in Materials Processing [M]. Berlin, Heidelberg: Springer, 2002: 242 | | [33] | Kaptay G. On the temperature gradient induced interfacial gradient force, acting on precipitated liquid droplets in monotectic liquid alloys [J]. Mater. Sci. Forum, 2006, 508: 269 |
|
|