| 国产核用不锈钢辐照损伤研究 |
邓平1,2, 彭群家1,3( ), 韩恩厚1, 柯伟1, 孙晨3, 夏海鸿3, 焦治杰4 |
1 中国科学院金属研究所中科院核用材料与安全性评价重点实验室 沈阳 110016 2 中国科学技术大学材料科学与工程学院 沈阳 110016 3 国家电投集团科学技术研究院有限公司 北京 102209 4 Department of Nuclear Engineering and Radiological Sciences, University of Michigan,Ann Arbor, MI 48109, U.S.A. |
|
| Study of Irradiation Damage in Domestically Fabricated Nuclear Grade Stainless Steel |
Ping DENG1,2, Qunjia PENG1,3( ), En-Hou HAN1, Wei KE1, Chen SUN3, Haihong XIA3, Zhijie JIAO4 |
1 CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China 3 State Power Investment Corporation Research Institute, Beijing 102209, China 4 Department of Nuclear Engineering and Radiological Sciences, University of Michigan, Ann Arbor, MI 48109, U.S.A. |
引用本文:
邓平, 彭群家, 韩恩厚, 柯伟, 孙晨, 夏海鸿, 焦治杰. 国产核用不锈钢辐照损伤研究[J]. 金属学报, 2017, 53(12): 1588-1602.
Ping DENG,
Qunjia PENG,
En-Hou HAN,
Wei KE,
Chen SUN,
Haihong XIA,
Zhijie JIAO.
Study of Irradiation Damage in Domestically Fabricated Nuclear Grade Stainless Steel[J]. Acta Metall Sin, 2017, 53(12): 1588-1602.
| [1] | Stephenson K J, Was G S.Crack initiation behavior of neutron irradiated model and commercial stainless steels in high temperature water[J]. J. Nucl. Mater., 2014, 444: 331 | | [2] | Ioka I, Ishijima Y, Usami K, et al.Radiation hardening and IASCC susceptibility of extra high purity austenitic stainless steel[J]. J. Nucl. Mater., 2011, 417: 887 | | [3] | Fukuya K, Nakano M, Fujii K, et al.IASCC susceptibility and slow tensile properties of highly-irradiated 316 stainless steels[J]. J. Nucl. Sci. Technol., 2004, 41: 673 | | [4] | Ge?rard R, Somville F. Situation of the baffle-former bolts in Belgian units [A]. Proceeding 17th International Conference on Nuclear Engineering[C]. Brussels, Belgium: American Society of Mechanical Engineers, 2009: 521 | | [5] | Andersen P L, Ford F P, Murphy S M, et al.State of knowledge of radiation effects on environmental cracking in light water reactor core materials [A]. Proceeding 4th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors[C]. Houston: National Association of Corrosion Engineers, 1989: 83 | | [6] | Nishioka H, Fukuya K, Fujii K, et al.IASCC initiation in highly irradiated stainless steels under uniaxial constant load conditions[J]. J. Nucl. Sci. Technol., 2008, 45: 1072 | | [7] | Zhou R S, West E A, Jiao Z J, et al.Irradiation-assisted stress corrosion cracking of austenitic alloys in supercritical water[J]. J. Nucl. Mater., 2009, 395: 11 | | [8] | Was G S, Bruemmer S M.Effects of irradiation on intergranular stress corrosion cracking[J]. J. Nucl. Mater., 1994, 216: 326 | | [9] | Stephenson K J, Was G S.Comparison of the microstructure, deformation and crack initiation behavior of austenitic stainless steel irradiated in-reactor or with protons[J]. J. Nucl. Mater., 2015, 456: 85 | | [10] | Jiao Z J, Was G S, Miura T, et al.Aspects of ion irradiations to study localized deformation in austenitic stainless steels[J]. J. Nucl. Mater., 2014, 452: 328 | | [11] | Jiao Z, Was G S.Impact of localized deformation on IASCC in austenitic stainless steels[J]. J. Nucl. Mater., 2011, 408: 246 | | [12] | Jiao Z J, Was G S.Oxidation of a proton-irradiated 316 stainless steel in simulated BWR NWC environment [A]. Proceeding 15th International Conference on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors[C]. Chichster: John Wiley & Sons, 2011: 1329 | | [13] | Gan J, Was G S.Microstructure evolution in austenitic Fe-Cr-Ni alloys irradiated with rotons: Comparison with neutron-irradiated microstructures[J]. J. Nucl. Mater., 2001, 297: 161 | | [14] | Was G S.Recent developments in understanding irradiation assisted stress corrosion cracking [A]. Proceeding 11th International Conference on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors[C]. La Grange Park, IL: American Nuclear Society, 2003: 965 | | [15] | Bruemmer S M, Simonen E P, Scott P M, et al.Radiation-induced material changes and susceptibility to intergranular failure of light-water-reactor core internals[J]. J. Nucl. Mater., 1999, 274: 299 | | [16] | Edwards D J, Simonen E P, Bruemmer S M.Evolution of fine-scale defects in stainless steels neutron-irradiated at 275 ℃[J]. J. Nucl. Mater., 2003, 317: 13 | | [17] | Singh B N, Foreman A J E, Trinkaus H. Radiation hardening revisited: Role of intracascade clustering[J]. J. Nucl. Mater., 1997, 249: 103 | | [18] | Huang H F, Li J J, Liu R D, et al.Temperature effect of Xe ion irradiation to 316 austenitic stainless steel[J]. Acta Metall. Sin., 2014, 50: 1189(黄鹤飞, 李健健, 刘仁多等. 316奥氏体不锈钢离子辐照损伤中的温度效应研究[J]. 金属学报, 2014, 50: 1189) | | [19] | Jiao Z, Was G S.The role of irradiated microstructure in the localized deformation of austenitic stainless steels[J]. J. Nucl. Mater., 2010, 407: 34 | | [20] | Gupta G, Jiao Z, Ham A N, et al.Microstructural evolution of proton irradiated T91[J]. J. Nucl. Mater., 2006, 351: 162 | | [21] | Gan J, Edwards D J, Simonen E P, et al.Microstructural evolution and hardening in 300-series stainless steels: Comparison between neutron and proton irradiations [A]. Proceeding 10th International Symposium on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors[C]. Houston: NACE International Publications, 2002 (in CD-ROM) | | [22] | Jiao Z, Was G S.Novel features of radiation-induced segregation and radiation-induced precipitation in austenitic stainless steels[J]. Acta Mater., 2011, 59: 1220 | | [23] | Miller M K.Atom Probe Tomography: Analysis at the Atomic Level[M]. New York: Springer, 2012: 173 | | [24] | Liu W Q, Liu Q D, Gu J F.Development and application of atom probe tomography[J]. Acta Metall. Sin., 2013, 49: 1025(刘文庆, 刘庆冬, 顾剑锋. 原子探针层析技术(APT)最新进展及应用[J]. 金属学报, 2013, 49: 1025) | | [25] | Sencer B H, Was G S, Sagisaka M, et al.Proton irradiation emulation of PWR neutron damage microstructures in solution annealed 304 and cold-worked 316 stainless steels[J]. J. Nucl. Mater., 2003, 323: 18 | | [26] | Wiedersich H, Okamoto P R, Lam N Q.A theory of radiation-induced segregation in concentrated alloys[J]. J. Nucl. Mater., 1979, 83: 98 | | [27] | Perks J M, Marwick A D, English C A.A Computer Code to Calculate Radiation-induced Segregation in Concentrated Ternary Alloys[M]. Harwell: AEA Technology, Atomic Energy Research Establishment, 1986: 48 | | [28] | Allen T R, Was G S.Modeling radiation-induced segregation in austenitic Fe-Cr-Ni alloys[J]. Acta Mater., 1998, 46: 3679 | | [29] | Rothman S J, Nowicki L J, Murch G E.Self-diffusion in austenitic Fe-Cr-Ni alloys[J]. J. Phys., 1980, 10F: 383 | | [30] | Allen T R, Was G S, Kenik E A.The effect of alloy composition on radiation-induced segregation in Fe-Cr-Ni alloys[J]. J. Nucl. Mater., 1997, 244: 278 | | [31] | Siegel R W. Vacancy concentrations in metals [J]. J. Nucl. Mater., 1978, 69-70: 117 | | [32] | Kiritani M, Takata H. Dynamic studies of defect mobility using high voltage electron microscopy [J]. J. Nucl. Mater., 1978, 69-70: 277 | | [33] | Allen T R, Busby J T, Was G S, et al.On the mechanism of radiation-induced segregation in austenitic Fe-Cr-Ni alloys[J]. J. Nucl. Mater., 1998, 255: 44 | | [34] | Lee E H, Maziasz P J, Rowcliffe A F, et al.Phase Stability during Irradiation[M]. Warrendale: TMS-AIME, 1981: 141 | | [35] | Was G S, Busby J T.Use of proton irradiation to determine IASCC mechanisms in light water reactors: Solute addition alloys [R]. Final Report, EPRI Project EP-P3038/C1434. Palo Alto, CA: Electric Power Research Institute, 2003 (in CD-ROM) | | [36] | Wan Q M, Shu G G, Wang R S, et al.Study on the microstructure evolution of A508-3 steel under proton irradiarion[J]. Acta Metall. Sin., 2012, 48: 929(万强茂, 束国刚, 王荣山等. A508-3钢质子辐照条件下微结构演变研究[J]. 金属学报, 2012, 48: 929) | | [37] | Li Z C, Chen L.Irradiation embrittlement mechanisms and relevant influence factors of nuclear reactor pressure vessel steels[J]. Acta Metall. Sin., 2014, 50: 1285(李正操, 陈良. 核能系统压力容器辐照脆化机制及其影响因素[J]. 金属学报, 2014, 50: 1285) | | [38] | Li Z C, Abe H, Sekimura N.Detection of point defects upon ion irradiation by means of precipitate coherency[J]. J. Nucl. Mater., 2007, 362: 87 | | [39] | Higgy H R, Hammad F H.Effect of fast-neutron irradiation on mechanical properties of stainless steels: AISI types 304, 316 and 347[J]. J. Nucl. Mater., 1975, 55: 177 |
|
|