| 陶瓷基复合材料辅助脉冲电流液相扩散连接的界面反应及接头强化机制 |
吴铭方1,刘飞2,王凤江1( ),乔岩欣1 |
| 2 镇江技师学院, 镇江 212000 |
|
| INTERFACIAL REACTION AND STRENGTHENING MECHANISM OF CERAMIC MATRIX COMPOSITE JOINTS USING LIQUID PHASE DIFFUSION BONDING WITH AUXILIARY PULSE CURRENT |
Mingfang WU1,Fei LIU2,Fengjiang WANG1( ),Yanxin QIAO1 |
1 Key Laboratory of Advanced Welding Technology of Jiangsu Province, Jiangsu University of Science and Technology, Zhenjiang 212003 2 Zhenjiang Institute of Technology, Zhenjiang 212000 |
引用本文:
吴铭方,刘飞,王凤江,乔岩欣. 陶瓷基复合材料辅助脉冲电流液相扩散连接的界面反应及接头强化机制[J]. 金属学报, 2015, 51(9): 1129-1135.
Mingfang WU,
Fei LIU,
Fengjiang WANG,
Yanxin QIAO.
INTERFACIAL REACTION AND STRENGTHENING MECHANISM OF CERAMIC MATRIX COMPOSITE JOINTS USING LIQUID PHASE DIFFUSION BONDING WITH AUXILIARY PULSE CURRENT[J]. Acta Metall Sin, 2015, 51(9): 1129-1135.
| [1] | Zhang D K, Wu A P, Zou G S. Trans China Weld Inst, 2005; 26(10): 59 (张德库, 吴爱萍, 邹贵生. 焊接学报, 2005; 26(10): 59) | | [2] | Wang Q Z, Liu Y, Zhang Y Z, Guan D H, Bi J. Trans China Weld Inst, 2006; 27(8): 43 (王全兆, 刘 越, 张玉政, 关德慧, 毕 敬. 焊接学报, 2006; 27(8): 43) | | [3] | Wu M F, Zhou X L, Ma C, Yang P. Trans China Weld Inst, 2006; 27(12): 1 (吴铭方, 周小丽, 马 骋, 杨 沛. 焊接学报, 2006; 27(12): 1) | | [4] | Wang Y, Cao J, Geng J C. China Welding, 2009; 18(4): 39 | | [5] | Passerone A, Muolo M L. Mater Manuf Process, 2000; 15: 631 | | [6] | Chen Z, Cao M S, Zhao Q Z. Mater Sci Eng, 2004; A380: 394 | | [7] | Li Z R, Cao J, Feng J C. Trans China Weld Inst, 2003; 24(2): 4 (李卓然, 曹 健, 冯吉才. 焊接学报, 2003; 24(2): 4) | | [8] | Osendi M I, De Pablos A, Miranzo P. Mater Sci Eng, 2001; A308: 53 | | [9] | Li S J, Liang X B, Duan H P. Key Eng Mater, 2002; 217: 101 | | [10] | Rabin B H, Moore G A. In: Carin A H, Schwartz D S, Silberglitt R S, Loehman R E eds., Mater Res Soc Symp Proc, 1993; 314: 197 | | [11] | He D H, Fu Z Y, Wang H, Zhang J Y. Trans China Weld Inst, 2002; 23(6): 33 (何代华, 傅正义, 王 皓, 张金咏. 焊接学报, 2002; 23(6): 33) | | [12] | He D H, Fu Z Y, Wang H, Zhang J Y. Trans China Weld Inst, 2002; 23(1): 85 (何代华, 傅正义, 王 皓, 张金咏. 焊接学报, 2002; 23(1): 85) | | [13] | Liu H J, Feng J C, Li G, Wang Y G. Welding Joining, 2000; (9): 7 (刘会杰, 冯吉才, 李 广, 王跃国. 焊接, 2000; (9): 7) | | [14] | Wanger T, Kirchheim R, Rühle M. Acta Metall Mater, 1995; 43: 1053 | | [15] | Zhang G, Zhang J, Pei Y, Li S, Chai D. Mater Sci Eng, 2008; A488: 146 | | [16] | Yang W, Lin T, He P, Wei H, Xing L, Jia D. Ceram Int, 2014; 40: 7253 | | [17] | Wu M F, Yu Z S, Jiang C Y, Qi K, Cheng X N. Rare Met Mater Eng, 2000; 29: 419 (吴铭方, 于治水, 蒋成禹, 祁 凯, 程晓农. 稀有金属材料与工程, 2000; 29: 419) | | [18] | Wu M F, Wang F, Wang F J, Xu G X. Trans China Weld Inst, 2014; 35(6): 31 (吴铭方, 王 斐, 王凤江, 胥国祥. 焊接学报, 2014; 35(6): 31) | | [19] | Loehman R E, Hosking F M, Gauntt B, Kotula P G, Lu P. J Mater Sci, 2005; 40: 2319 | | [20] | Ye D L,Hu J H. Practical Handbook on the Thermodynamic Data of Inorganic Substances. 2nd Ed., Beijing: Metallurgical Industry Press, 2002: 57 (叶大伦,胡建华. 实用无机物热力学数据手册. 第二版, 北京: 冶金工业出版社, 2002: 57) | | [21] | Ihsan B I,translated by Cheng N L,Niu S T,Xu G Y. Thermochemical Data of Pure Substances. Beijing: Science Press, 2003: 17 (Ihsan B I著,程乃良,牛四通,徐桂英译. 纯物质热化学数据手册. 北京: 科学出版社, 2003: 17) | | [22] | Xu R,Jin T F.Thermodynamics and Kinetics of Materials. Harbin: Harbin Institute of Technology Press, 2003: 10 (徐 瑞,荆天辅.材料热力学与动力学. 哈尔滨: 哈尔滨工业大学出版社, 2003: 10) | | [23] | Chen Z, Liu B, Wang Y X, Wei Q L. Rare Met Mater Eng, 2001; 30: 331 (陈 铮, 刘 兵, 王永欣, 魏齐龙. 稀有金属材料与工程, 2001; 30: 331) | | [24] | Chang G W, Xue Q G. J Univ Sci Technol Beijing, 1999; 21: 175 (常国威, 薛庆国. 北京科技大学学报, 1999; 21: 175) | | [25] | He S X, Wang J, Zhou Y H. Acta Metall Sin, 2002; 38: 479 (何树先, 王 俊, 周尧和. 金属学报, 2002; 38: 479) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|