| 镀Cr层对低碳钢/CFRP激光连接接头剪切强度及界面结合特征的影响 |
| 谭向虎1),单际国1,2),任家烈1) |
1) 清华大学机械工程系,北京 100084
2) 清华大学先进成形制造教育部重点实验室, 北京100084 |
|
| EFFECTS OF Cr PLATING LAYER ON SHEAR STRENGTH AND INTERFACE BONDING CHARACTERISTICS OF MILD STEEL/CFRP JOINT BY LASER HEATING |
| TAN Xianghu1),SHAN Jiguo1,2),REN Jialie1) |
1) Department of Mechanical Engineering, Tsinghua University, Beijing 100084
2) Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, Tsinghua University, Beijing 100084 |
引用本文:
谭向虎,单际国,任家烈. 镀Cr层对低碳钢/CFRP激光连接接头剪切强度及界面结合特征的影响[J]. 金属学报, 2013, 49(6): 751-756.
TAN Xianghu,
SHAN Jiguo,
REN Jialie.
EFFECTS OF Cr PLATING LAYER ON SHEAR STRENGTH AND INTERFACE BONDING CHARACTERISTICS OF MILD STEEL/CFRP JOINT BY LASER HEATING[J]. Acta Metall Sin, 2013, 49(6): 751-756.
| [1]Williams G J,Trask R S, Bond I P. Composites, 2007; 38A: 1525
[2] Soutis C. Mater Sci Eng, 2005; A412: 171
[3] Vaidya U K, Chawla K K. Int Mater Rev, 2008; 53:185
[4] Duflou J R, De Moor J, Verpoest I, Dewulf W.CIRP Ann Manuf Technol, 2009; 58: 9
[5] Jaeschke P, Herzog D, Haferkamp H, Peters C, Herrmann AS. J Reinf Plast Compos, 2010; 29: 3083
[6] Amancio--Filho S T, Santos J F D. Polym Eng Sci,2009; 8: 1461
[7] Ageorges C, Ye L, Hou M. Composites, 2001; 32A:839
[8] Hino M, Mitooka Y, Murakami K, Kanadani T. In: Chandra T,Ionescu M, Mantovani D eds., Materials Science Forum,Quebec: Trans Tech Publications Ltd, 2012: 2956
[9] Katayama S, Jung K W, Kawahito Y. In: David A ed.,ICALEO 2010 Congress Proceedings, Orlando: Laser Instituteof America, 2010: 333
[10] Jung K W, Kawahito Y, Katayama S. Sci Technol Weld Join, 2011; 16: 676
[11] Katayama S, Kawahito Y. Scr Mater, 2008; 59:1247
[12] Wahba M, Kawahito Y, Katayama S. J Mater Process Technol, 2011; 211: 1166
[13] Kawahito Y, Tange A, Kubota S, Katayama S. In: Laser Institute of America ed., ICALEO 2006 Congress Proceedings, Orlando: Laser Institute of America, 2006: 376
[14] Roesner A, Scheik S, Olowinsky A, Gillner A, Poprawe R, Schleser M, Reisgen U. J Laser Appl, 2011; 23:032007-1
[15] Holtkamp J, Roesner A, Gillner A. Int J Adv Manuf Technol, 2010; 47: 923
[16] Lee H Y, Qu J M. J Adhes Sci Technol, 2003; 17:195
[17] Ho P S, Hahn P O, Bartha J W, Rubloff G W, Legoues F K, Silverman B D. J Vac Sci Technol, 1985; 3A: 739
[18] Chou N J, Tang C H. J Vac Sci Technol, 1984; 2A:751
[19] Bebin P, Prud'Homme R E. J Vac Sci Technol, 2002;20A: 1611
[20] Cantrell J H. J Appl Phys, 2004; 96: 3775
[21] McCafferty E. J Adhes Sci Technol, 2002; 16: 239
[22] Fortunato A, Cuccolini G, Ascari A, Orazi L, Campana G, Tani G. Int J Mater Form, 2010; 3(suppl 1): 1131
[23] Goldberg M J, Clabes J G, Kovac C A. J Vac Sci Technol, 1988; 6A: 991
[24] Friedrich J F, Koprinarov I, Giebler R, Lippitz A, Unger W E S. J Adhes, 1999; 71: 297
[25] Tang D Y, Guo Y D, Zhang X H, Liu J. Surf Interface Anal, 2009; 41: 974 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|