Please wait a minute...
金属学报  2013, Vol. 49 Issue (3): 277-283    DOI: 10.3724/SP.J.1037.2012.00531
  论文 本期目录 | 过刊浏览 |
Mg-Al合金Mg17Al12连续析出相形貌的相场模拟
韩国民1,韩志强1,Alan A. Luo2,Anil K. Sachdev2,柳百成1, 3
1) 清华大学机械工程系先进成形制造教育部重点实验室, 北京 100084
2)Chemical Sciences and Materials Systems Laboratory, General Motors Global Research and Development Center,Warren, MI 48090-9055, USA
3) 清华大学汽车工程系汽车安全与节能国家重点实验室, 北京 100084
PHASE FIELD SIMULATION ON MORPHOLOGY OF CONTINUOUS PRECIPITATE Mg17Al12IN Mg-Al ALLOY
HAN Guomin1, HAN Zhiqiang1, Alan A. Luo2, Anil K. Sachdev2, LIU Baicheng1, 3
1) Key Laboratory for Advanced Materials Processing Technology (Ministry of Education), Department of Mechanical,Engineering, Tsinghua University, Beijing 100084
2) Chemical Sciences and Materials Systems Laboratory, General Motors Global Research and Development Center,Warren, MI 48090-9055, USA
3) State Key Laboratory of Automotive Safety and Energy, Department of Automotive Engineering, Tsinghua University,Beijing 100084
引用本文:

韩国民,韩志强,Alan A. Luo,Anil K. Sachdev,柳百成. Mg-Al合金Mg17Al12连续析出相形貌的相场模拟[J]. 金属学报, 2013, 49(3): 277-283.
HAN Guomin, HAN Zhiqiang, Alan A. Luo, Anil K. Sachdev, LIU Baicheng. PHASE FIELD SIMULATION ON MORPHOLOGY OF CONTINUOUS PRECIPITATE Mg17Al12IN Mg-Al ALLOY[J]. Acta Metall Sin, 2013, 49(3): 277-283.

全文: PDF(1061 KB)  
摘要: 

基于KKS相场模型模拟了Mg-Al合金Mg17Al12单个连续析出相的形貌演化. 相场模型中, 各相自由能及化学势由Thermo-Calc热力学计算软件计算. 构造各向异性函数时考虑了界面能各向异性的影响, 基于Khachaturyan微观弹性应变能理论考虑了微观弹性应变能的影响. 结果表明: 仅考虑界面能各向异性不考虑微观弹性应变能, 析出相呈板条状形貌; 仅考虑微观弹性应变能不考虑界面能各向异性, 析出相呈菱形; 综合考虑界面能各向异性和微观弹性应变能, 析出相呈板条状形貌, 端部呈平行四边形, 此形貌特征与实验观察结果吻合; 界面能各向异性决定析出相的板条状形貌特征, 微观弹性应变能导致端部产生平行四边形特征.

关键词 : Mg-A合金,  连续析出相,  形貌演化,  热力学计算,  界面能各向异性,  微观弹性应变能,  相场模型    
Abstract:

The morphology evolution of the continuous precipitate Mg17Al12 in aging process was studiedusing KKS phase field model. In the model, the chemical free energy and chemical potential for the precipitatephase and matrix were obtained by using Thermo-Calc software and database. The effects of interfacial energyanisotropy were taken into account by introducing interface anisotropy function, and the effects of micro elasticstrain energy were introduced based on the theory of micro elastic strain energy formulated by Khachaturya. It isdemonstrated that the precipitate phase has a lath shape when only the interfacial energy anisotropy wasconsidered regardless of the micro elastic strain energy.The precipitate phase grows into a diamond shape whenonly the micro elastic strain energy was taken into account regardless of the interfacial energy anisotropy. Whenboth the effects of the interfacial energy anisotropy and the micro elastic strain energy were considered in thesimulation, the precipitate phase has a lath shape with lozenge ends,which is in agreement with experimental observations. The interfacial energy anisotropy affectsthe overall morphology of the precipitate, and combiningthe interfacial energy anisotropy and the micro elastic strain energy results in the lath shape with lozenge ends.

Key words: Mg-Al alloy    continuous precipitate    morphology evolution    thermodynamic calculation    interfacial energyanisotropy    micro elastic strain energy    phase-field model
收稿日期: 2012-09-10     
基金资助:

国家自然科学基金项目51175291, 科技部国际科技合作计划课题2010DFA72760和2011DFA50909及

作者简介: 韩国民, 男, 1983年生, 博士生

[1] Mordike B L, Ebert T.Mater Sci Eng, 2001; A302: 37


[2] Clark J B.Acta Metall, 1968; 16: 141

[3] Celotto S.Acta Mater, 2000; 48: 1775

[4] Duly D, Simon J P, Brechert Y.Acta Metall, 1995; 43: 101

[5] Hutchinson C R, Nie J F, Gorsse S.Metall Mater Trans, 2005; 36A: 2093

[6] Xiao X L, Luo C P, Nie J F, Muddle B C.Acta Metall Sin, 2001; 37: 1

(肖晓玲, 罗承萍, 聂建峰, Muddle B C. 金属学报, 2001; 37: 1)

[7] Luo C P, Xiao X L, Liu J W, Nie J F, Muddle B C.Acta Metall Sin, 2002; 38: 709

(罗承萍, 肖晓玲, 刘江文, 聂建峰, Muddle B C. 金属学报, 2002; 38: 709)

[8] Ke C B, Ma X, Zhang X P.Acta Metall Sin, 2010; 46: 84

(柯常波, 马晓, 张新平. 金属学报, 2010; 46: 84)

[9] Yang M, Wang G, Teng C Y, Xu D S, Zhang J, Yang R, Wang Y Z.Acta Metall Sin, 2012; 48: 148

(杨梅, 王刚, 滕春禹, 徐东生, 张鉴, 杨锐, 王云志. 金属学报, 2012; 48: 148)

[10] Vaithyanathan V, Wolverton C, Chen L Q.Phys Rev Lett, 2002; 88: 125503

[11] Zhu J Z, Wang T, Ardell A J, Zhou S H, Liu Z K, Chen L Q.Acta Mater, 2004; 52: 2837

[12] Gao Y P, Liu H, Shi R, Zhou N, Xu Z, Zhu Y M, Nie J F, Wang Y.Acta Mater, 2012; 60: 4819

[13] Li M, Zhang R J, Allison J. In: Agnew S, Neelameggham N R, Nyberg E A, Sillekens W eds.,

Magnesium Technology 2010. Warrendale: The Minerals, Metals and Materials Society, 2010: 623

[14] Kim S G, Kim W T, Suzuki T.Phys Rev, 1999; 60E: 7186

[15] Hu S Y, Murray J, Weiland H, Liu Z K, Chen L Q.Calphad, 2007; 31: 303

[16] Hu S Y.PhD Dissertation, Pennsylvania State University, 2004

[17] Zhou N, Shen C, Mills M, Wang Y Z.Philos Mag, 2010; 90: 405

[18] Zhou N.PhD Dissertation, Ohio State University, 2008

[19] Khachaturyan A G.Theory of Structural Transformation in Solids.

New York: Wiley-Interscience, 1983: 204, 213

[20] Wang Y Z, Khachaturyan A G.Acta Metall Mater, 1997; 45: 759

[21] Li D Y, Chen L Q.Acta Mater, 1998; 46: 2573

[22] Vaithyanathan V, Wolverton C, Chen L Q.Acta Mater, 2004; 52: 2973

[23] Katarzyna N. Braszczynska M. In: Czerwinski F ed.,

 Magnesium Alloys-Design, Processing and Properties. Rijeka: InTech, 2011: 95
[1] 穆亚航, 张雪, 陈梓名, 孙晓峰, 梁静静, 李金国, 周亦胄. 基于热力学计算与机器学习的增材制造镍基高温合金裂纹敏感性预测模型[J]. 金属学报, 2023, 59(8): 1075-1086.
[2] 陈维, 陈洪灿, 王晨充, 徐伟, 罗群, 李谦, 周国治. Fe-C-Ni体系膨胀应变能对马氏体转变的影响[J]. 金属学报, 2022, 58(2): 175-183.
[3] 孙正阳, 杨超, 柳文波. UO2烧结过程的相场模拟[J]. 金属学报, 2020, 56(9): 1295-1303.
[4] 于家英, 王华, 郑伟森, 何燕霖, 吴玉瑞, 李麟. 热浸镀锌高强汽车板界面组织对其拉伸断裂行为的影响[J]. 金属学报, 2020, 56(6): 863-873.
[5] 赵宝军,赵宇宏,孙远洋,杨文奎,侯华. Mn含量对Fe-Cu-Mn合金纳米富Cu析出相影响的相场法研究[J]. 金属学报, 2019, 55(5): 593-600.
[6] 黄宇, 成国光, 谢有. 稀土Ce对钎具钢中夹杂物的改质机理研究[J]. 金属学报, 2018, 54(9): 1253-1261.
[7] 高英俊, 卢昱江, 孔令一, 邓芊芊, 黄礼琳, 罗志荣. 晶体相场模型及其在材料微结构演化中的应用[J]. 金属学报, 2018, 54(2): 278-292.
[8] 李双明, 王斌强, 刘振鹏, 钟宏, 胡锐, 刘毅, 罗锡明. 高熔点金属Ir和Mo电子束区熔中不同取向晶体的竞争生长[J]. 金属学报, 2018, 54(10): 1435-1441.
[9] 卢艳丽,卢广明,胡婷婷,杨涛,陈铮. 晶体相场法研究Kirkendall效应诱发的相界空洞的形成和演变*[J]. 金属学报, 2015, 51(7): 866-872.
[10] 高英俊, 周文权, 邓芊芊, 罗志荣, 林葵, 黄创高. 晶体相场方法模拟高温应变作用的预熔化晶界的位错运动*[J]. 金属学报, 2014, 50(7): 886-896.
[11] 潘涛, 王小勇, 苏航, 杨才福. 合金元素Al对微B处理特厚钢板淬透性及力学性能的影响*[J]. 金属学报, 2014, 50(4): 431-438.
[12] 高英俊, 卢成健, 黄礼琳, 罗志荣, 黄创高. 晶界位错运动与位错反应过程的晶体相场模拟*[J]. 金属学报, 2014, 50(1): 110-120.
[13] 吴艳,宗亚平,张宪刚. 纳米晶AZ31镁合金显微组织演变的相场法模拟研究[J]. 金属学报, 2013, 49(7): 789-796.
[14] 梁静静,朱明,袁忠华,王君武,金涛,孙晓峰,胡壮麒. Re对NiCoCrAlY涂层合金相组成的影响[J]. 金属学报, 2013, 49(3): 330-340.
[15] 彭东剑,林鑫,张云鹏,郭雄,王猛,黄卫东. 界面追踪法研究界面能各向异性对定向凝固枝晶生长的影响[J]. 金属学报, 2013, 49(3): 365-371.