Please wait a minute...
金属学报  2013, Vol. 49 Issue (3): 265-270    DOI: 10.3724/SP.J.1037.2012.00616
  论文 本期目录 | 过刊浏览 |
块体超细晶304L不锈钢的腐蚀及钝化性能的研究
韩啸1,陈吉1,孙成2,武占文1,吴新春1,张星航2
1) 辽宁石油化工大学机械工程学院石油化工过程腐蚀与防护技术中心, 抚顺 113001
2) Department of Mechanical Engineering, Texas A &M University, College station, TX 77843-3123, USA
CORROSION AND PASSIVE PROPERTIES OF BULKULTRAFINE-GRAINED 304L STAINLESS STEEL
HAN Xiao1, CHEN Ji1, SUN Cheng2, WU Zhanwen1, WU Xinchun1, ZHANG Xinghang2
1) Center of Corrosion and Protection Technology in Petro-Chemical Industry, Department of Mechanical Engineering,,LiaoningShihua University, Fushun 113001
2) Department of Mechanical Engineering, Texas A&M University, College station, TX 77843-3123, USA
引用本文:

韩啸,陈吉,孙成,武占文,吴新春,张星航. 块体超细晶304L不锈钢的腐蚀及钝化性能的研究[J]. 金属学报, 2013, 49(3): 265-270.
HAN Xiao, CHEN Ji, SUN Cheng, WU Zhanwen, WU Xinchun, ZHANG Xinghang. CORROSION AND PASSIVE PROPERTIES OF BULKULTRAFINE-GRAINED 304L STAINLESS STEEL[J]. Acta Metall Sin, 2013, 49(3): 265-270.

全文: PDF(683 KB)  
摘要: 

利用等通道转角挤压(ECAP)方法, 制备出平均晶粒尺寸为(130±30) nm的块体超细晶304L不锈钢. 在0.05 mol/L H2SO4+0.25 mol/L Na2SO4溶液中测量了其极化曲线和钝化性能的Mott-Schottky曲线.结果表明, 与粗晶合金相比, 超细晶材料的自腐蚀电位更低, 自腐蚀电流密度更大, 更易发生活性溶解且溶解速度更快, 但致钝电位更低, 维钝电流密度更小, 钝化区间更宽. 表面钝化膜均具有n型半导体特征,超细晶粒有助于304L不锈钢表面形成更为稳定的钝化膜, 载流子密度更小, 载流子的扩散系数更低.

关键词 : 304L不锈钢,  超细晶,  耐蚀性能,  钝化,  等通道转角挤压    
Abstract:

 Samples of ultrafine-grained 304L stainless steel with an average grain size of (130±30) nm wereprepared by using equal channel angular pressing (ECAP) technique after 6 passes with route Bc at 500 ℃.The electrochemical behaviors and the passive properties of the material in 0.05 mol/L H2SO4+0.25 mol/L Na2SO4solution were examined by using polarization curves and Mott-Schottky analysis. As compared with the coarse-grained counterpart, the ultrafine-grained 304L stainless steel sample exhibits a lower corrosion potential(-505 mV) and a higher corrosion current density (11.7μA/cm2), indicating the accelerated trend of the activedissolution, and has a broadening of passive region (-341-847 mV) with lower passive potential (-341 mV) andpassivation current density (4.5μA/cm2). Both of the passive films exhibit n-type semi-conductor behaviorsat potentials ranging from 0 to 0.7 V. The ultrafine grains of 304L stainless steel are helpful in forming more stablepassive films with the reduced donor density and the diffusion coefficient of the charge carrier.

Key words: 304L stainless steel    ultrafinegrain    corrosionresistance    passivation    equal channel angularpressing (ECAP)
收稿日期: 2012-10-17     
基金资助:

辽宁省自然科学基金项目201202127和辽宁省高等学校杰出青

作者简介: 韩啸, 男, 1987年生, 硕士生

[1] Valiev R Z, Islamgaliev P K, Alexandrov I V.Prog Mater Sci, 2000; 45: 103


[2] Gleiter H.Acta Mater, 2000; 48: 1

[3] Chen J, Lu L, Lu K.Scr Mater, 2006; 54: 1913

[4] Liu L, Li Y, Wang F H.J Mater SciTechnol, 2010; 26: 1

[5] Peng X, Yan J, Zhou Y,Wang F H.Acta Mater, 2005; 53: 5079

[6] Ye W, Li Y, Wang F H.ElectrochimActa, 2009; 54: 1339

[7] Li N, Li Y, Wang S G, Wang F H.ElectrochimActa, 2006; 52: 760

[8] Liu L, Li Y, Wang F H.ElectrochimActa, 2010; 55: 2430

[9] Ye W, Li Y, Wang F H.ElectrochimActa, 2006; 51: 4426

[10] Zhang Y C, Macdonald D D, Macdonald M U, Engelhardt G R, Dooley R B.CorrosSci, 2006; 48: 3812

[11] Liu L, Li Y, Wang F H.ElectrochimActa, 2008; 54: 768

[12] Meng G Z, Li Y, Wang F H.ElectrochimActa, 2006; 51: 4277

[13] Fattah A A, Saatchi A, Golozar M A, Raeissi K.J ApplElectrochem, 2010; 40: 457

[14] Nicic I, Macdonald D D.J Nucl Mater, 2008; 379: 54

[15] Kiyotaka N, Zenji H, Minoru N, Terence G L.Mater SciEng, 2000; A280: 82

[16] Pan C, Liu L, Li Y, Wang S G, Wang F H.ElectrochimActa, 2011; 56: 7740

[17] Dewald J F.J PhysChem Solids, 1960; 14: 155

[18] Buchler M, Schmuki P, Buhui H.ElectrochimActa, 1997; 43: 635

[19] Sikora J, Sikora E, Macdonald D D.ElectrochimActa, 2000; 45: 1875

[20] Schmuki P, Bohni H.ElectrochimActa, 1995; 40: 775

[21] Chao C Y, Lin L F, MacDonald D D.J ElectrochemSoc, 1981; 128: 1187

[22] Lin L F, Chao C Y, MacDonald D D.J ElectrochemSoc, 1981; 128: 1194

[23] Chao C Y, Lin L F, MacDonald D D.J ElectrochemSoc, 1982; 129: 1874

[24] Sikora E, Sikora J, MacDonald D D.ElectrochimActa, 1996; 41: 783

[25] Guo H X, Lu B T, Luo J L.ElectrochimActa, 2006; 52: 1108
[1] 赵平平, 宋影伟, 董凯辉, 韩恩厚. 不同离子对TC4钛合金电化学腐蚀行为的协同作用机制[J]. 金属学报, 2023, 59(7): 939-946.
[2] 侯娟, 代斌斌, 闵师领, 刘慧, 蒋梦蕾, 杨帆. 尺寸设计对选区激光熔化304L不锈钢显微组织与性能的影响[J]. 金属学报, 2023, 59(5): 623-635.
[3] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.
[4] 许林杰, 刘徽, 任玲, 杨柯. Cu对Ni-Ti合金抗支架内再狭窄与耐蚀性能的影响[J]. 金属学报, 2023, 59(4): 577-584.
[5] 朱云鹏, 覃嘉宇, 王金辉, 马鸿斌, 金培鹏, 李培杰. 机械球磨结合粉末冶金制备AZ61超细晶镁合金的组织与性能[J]. 金属学报, 2023, 59(2): 257-266.
[6] 胡文滨, 张晓雯, 宋龙飞, 廖伯凯, 万闪, 康磊, 郭兴蓬. 共晶高熵合金AlCoCrFeNi2.1 在H2SO4 溶液中的腐蚀行为[J]. 金属学报, 2023, 59(12): 1644-1654.
[7] 孙毅, 郑沁园, 胡宝佳, 王平, 郑成武, 李殿中. 3Mn-0.2C中锰钢形变诱导铁素体动态相变机理[J]. 金属学报, 2022, 58(5): 649-659.
[8] 汤雁冰, 沈新旺, 刘志红, 乔岩欣, 杨兰兰, 卢道华, 邹家生, 许静. 激光选区熔化Inconel 718合金在NaOH溶液中的腐蚀行为[J]. 金属学报, 2022, 58(3): 324-333.
[9] 陈胜虎, 戎利建. 超细晶铁素体-马氏体钢的高温氧化成膜特性及其对Pb-Bi腐蚀行为的影响[J]. 金属学报, 2021, 57(8): 989-999.
[10] 林鹏程, 庞玉华, 孙琦, 王航舵, 刘东, 张喆. 45钢块体超细晶棒材3D-SPD轧制法[J]. 金属学报, 2021, 57(5): 605-612.
[11] 黄一川, 王清, 张爽, 董闯, 吴爱民, 林国强. 用于燃料电池双极板的不锈钢成分优化[J]. 金属学报, 2021, 57(5): 651-664.
[12] 吕晨曦, 孙阳庭, 陈斌, 蒋益明, 李劲. 恒电位脉冲技术对317L不锈钢点蚀行为及耐点蚀性能的影响[J]. 金属学报, 2021, 57(12): 1607-1613.
[13] 王雪梅, 殷正正, 于晓彤, 邹玉红, 曾荣昌. AZ31镁合金表面苯丙氨酸、甲硫氨酸和天冬酰胺诱导Ca-P涂层耐蚀性能比较[J]. 金属学报, 2021, 57(10): 1258-1271.
[14] 彭云,宋亮,赵琳,马成勇,赵海燕,田志凌. 先进钢铁材料焊接性研究进展[J]. 金属学报, 2020, 56(4): 601-618.
[15] 魏琳,王志军,吴庆峰,尚旭亮,李俊杰,王锦程. Mo元素及热处理对Ni2CrFeMox高熵合金在NaCl溶液中耐蚀性能的影响[J]. 金属学报, 2019, 55(7): 840-848.