| 0.037%H对铸态Ti-45Al-5Nb-0.8Mo-0.3Y合金高温变形行为的影响 |
| 温道胜,宗影影,徐文臣,杨单媚,单德彬 |
| 哈尔滨工业大学材料科学与工程学院, 哈尔滨 150001 |
|
| EFFECT OF 0.037%H ON HIGH TEMPERATURE DEFORMATION BEHAVIOR OF A CAST Ti-45Al-5Nb-0.8Mo-0.3Y ALLOY |
| WEN Daosheng, ZONG Yingying, XU Wenchen, YANG Danmei, SHAN Debin |
| Department of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001 |
引用本文:
温道胜,宗影影,徐文臣,杨单媚,单德彬. 0.037%H对铸态Ti-45Al-5Nb-0.8Mo-0.3Y合金高温变形行为的影响[J]. 金属学报, 2013, 49(11): 1428-1432.
WEN Daosheng,
ZONG Yingying,
XU Wenchen,
YANG Danmei,
SHAN Debin.
EFFECT OF 0.037%H ON HIGH TEMPERATURE DEFORMATION BEHAVIOR OF A CAST Ti-45Al-5Nb-0.8Mo-0.3Y ALLOY[J]. Acta Metall Sin, 2013, 49(11): 1428-1432.
| [1] Loria E A. Intermetallics, 2001; 9: 997
[2] Li C G, Fu H Z, Yu Q. Materials in Aerospace. Beijing: National Defense Industry Press,2002: 16
(李成功, 傅恒志, 于翘. 航空航天材料. 北京: 国防工业出版社, 2002: 16)
[3] Venkatesware R K T, Kim Y W, Muhlstein C L, Ritchie R O. Mater Sci Eng, 1995; A192-193: 474
[4] Kim Y W. JOM, 1995; 47(7): 39
[5] Wu X H. Intermetallics, 2006; 14: 1114
[6] Chen Y Y, Niu H Z, Kong F T, Xiao S L. Intermetallics, 2011; 19: 1405
[7] Anisimova L I. Met Sci Heat Treat, 1992; 34(2): 143
[8] Li F, Chen Y X, Wan X J, Wang Q J, Liu Y Y. Aata Metall Sin, 2006; 42: 143
(李芳, 陈业新, 万晓景, 王青江, 刘羽寅. 金属学报, 2006; 42: 143)
[9] Shen C C, Yu C Y, Perng T P. Acta Mater, 2009; 57: 868
[10] Zhang Y, Zhang S Q. Scr Mater, 1997; 37: 1315
[11] Zong Y Y. PhD Dissertation, Harbin Institute of Technology, 2007
(宗影影. 哈尔滨工业大学博士学位论文, 2007)
[12] Zhang Y, Zhang S Q, Tao C H. Aata Metall Sin, 1996; 32: 235
(张勇, 张少卿, 陶春虎. 金属学报, 1996; 32: 235)
[13] Liu X W. PhD Dissertation, Harbin Institute of Technology, 2011
(刘鑫旺. 哈尔滨工业大学博士学位论文, 2011)
[14] Lin J P, Cheng G L. Mater China, 2009; 28(1): 31
(林均品, 陈国良. 中国材料进展, 2009; 28(1): 31)
[15] Sakai T. J Mater Process Technol, 1995; 53: 349
[16] Goken M, Kempf M, Nix W D. Acta Mater, 2001; 49: 903
[17] Liu X W, Su Y Q, Luo L S, Liu J P, Guo J J, Fu H Z. Int J Hydrogen Energy, 2010; 35: 13322
[18] Liu X W, Su Y Q, Luo L S, Li K, Dong F Y, Guo J J, Fu H Z. Int J Hydrogen Energy, 2011; 36: 3260
[19] Senkov O N, Froes F H. Int J Hydrogen Energy, 1999; 24: 565
[20] Murzinova M A, Salishchev G A, Afonichev D D. Int J Hydrogen Energy, 2002; 27: 775
[21] Bashkin I O, Ponyatovskiy Y G, Senkov O N, Malyshev V Y. Phys Met Metallogr, 1990; 69(2): 67
[22] Shan D B, Zong Y Y, Lv Y, Guo B. Scr Mater, 2008; 58: 449
[23] Semiatin S L, Seetharaman V, Weiss I. Mater Sci Eng, 1999; A263: 257
[24] Semiatin S L, Bieler T R. Acta Mater, 2001; 49: 3565
[25] Zong Y Y, Shan D B, Lv Y, Guo B. Int J Hydrogen Energy, 2007; 32: 3936
[26] Yuan B G, Li C F, Yu H P, Sun D L. Mater Sci Eng, 2010; A527: 4185 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|