利用APT对RPV模拟钢中富Cu原子团簇析出的研究 |
徐刚1,蔡琳玲1,冯柳1,周邦新1,2,刘文庆1,2,王均安1,2 |
1. 上海大学材料研究所, 上海 200072
2. 上海大学微结构重点实验室, 上海 200444 |
|
STUDY ON THE PRECIPITATION OF Cu-RICH CLUSTERS IN THE RPV MODEL STEEL BY APT |
XU Gang1, CAI Linling1, FENG Liu1, ZHOU Bangxin1,2,LIU Wenqing1,2, WANG Jun'an1,2
|
1. Institute of Materials, Shanghai University, Shanghai 200072
2. Laboratory for Microstructures, Shanghai University, Shanghai 200444 |
引用本文:
徐刚,蔡琳玲,冯柳,周邦新,刘文庆,王均安. 利用APT对RPV模拟钢中富Cu原子团簇析出的研究[J]. 金属学报, 2012, 48(4): 407-413.
,
,
,
,
,
.
STUDY ON THE PRECIPITATION OF Cu-RICH CLUSTERS IN THE RPV MODEL STEEL BY APT[J]. Acta Metall Sin, 2012, 48(4): 407-413.
[1] Toyama T, Nagai Y, Tang Z, Hasegawa M, Almazouzi A, van Walle E, Gerard R. Acta Mater, 2007; 55: 6852
[2] Auger P, Pareige P, Welzel S, Van Duysen J C. J Nucl Mater,2000; 280: 331
[3] Miller M K, Russell K F, Sokolov M A, Nanstad R K. J Nucl Mater,2007; 361: 248
[4] Miller M K, Russell K F, Sokolov M A, Nanstad R K. J Nucl Mater,2003; 320: 177
[5] Miller M K, Nanstad P K, Sokolov M A, Russell K F. J Nucl Mater,2006; 351: 216
[6] Phythian W J, English C A. J Nucl Mater, 1993; 205: 162
[7] Fukuya K, Ohno K, Nakata H, Dumbill S, Hyde J M. J Nucl Mater, 2003; 312: 163
[8] Carter R G, Soneda N, Dohi K, Hyde J M, English C A, Server W L. J Nucl Mater, 2001; 298: 211
[9] Miller M K, Chernobaeva A A, Shtrombakh Y I, Russell K F,Nanstad R K, Erak D Y, Zabusov O O. J Nucl Mater, 2009; 385: 615
[10] Miller M K, Russell K F. J Nucl Mater, 2007; 371: 145
[11] Hornbogen E, Glenn R C. Trans Metall Soc AIME, 1960; 218: 1064
[12] Speich G R, Oriani R A. Trans Metall Soc AIME, 1965; 233: 623
[13] Goodman S R, Brenners S S, Low J R. Metall Trans, 1973; 4: 2363
[14] Pizzini S, Roberts K J, Phythian W J, English C A, Greaves G N. Philos Mag Lett, 1990; 61: 223
[15] Othen P J, Jenkins M L, Smith G D W, Phythian W J. Philos Mag Lett, 1991; 64: 383
[16] Othen P J, Jenkins M L, Smith G D W. Philos Mag, 1994; 70A: 1
[17] Styman P D, Hyde J M, Wilford K, Morley A, Smith G D W. Prog Nucl Energ, 2011, doi:10.1016/j.pnucene.2011.10.010
[18] Chu D F, Xu G, Wang W, Peng J C, Wang J A, Zhou B X. Acta Metall Sin, 2011; 47: 269
(楚大锋, 徐刚, 王伟, 彭剑超, 王均安, 周邦新. 金属学报,2011; 47: 269)
[19] Xu G, Chu D F, Cai L L, Zhou B X, Wang W, Peng J C. Acta Metall Sin, 2011; 47: 905
(徐刚, 楚大锋, 蔡琳玲, 周邦新, 王伟, 彭剑超.金属学报, 2011; 47: 905)
[20] Miller M K. Atom Probe Tomography: Analysis at the Atomic Level.New York: Kliwer Academic/Plenum Publishers, 2000: 25
[21] Starink M J, Zahra A M. Philos Mag, 1998; 77: 187
[22] Starink M J, Zahra A M. Thermochim Acta, 1997; 292: 159
[23] Miller M K, Russell K F, Pareige P, Starink M J, Thomson R C. Mater Sci Eng, 1998; A250: 49
[24] Zhu J J, Wang W, Lin M D, Liu W Q, Wang J A, Zhou B X. J Shanghai Univ (Nat Sci), 2008; 5: 525
(朱娟娟, 王伟, 林民东, 刘文庆, 王均安, 周邦新.上海大学学报(自然科学版), 2008; 5: 525)
[25] Buswell J T, English C A, Herherington M G, Phythian W J,
Smith G D W, Worral G M. In: Steele L E ed., Proc 14th Int Symp Effects of Radiation on Materials, Vol.2, Andover, Massachusseetts: The American Society for Testing and Materials, 1990: 127 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|