| 液相原位反应法制备Cu-Y2O3复合材料 |
| 卓海鸥,唐建成,叶楠 |
| 南昌大学材料科学与工程学院, 南昌 330031 |
|
| Cu–Y2O3 COMPOSITES PREPARED BY LIQUID PHASE IN SITU REACTION |
| ZHUO Haiou, TANG Jiancheng, YE Nan |
| Institute of Materials Science and Engineering, Nanchang University, Nanchang 330031 |
引用本文:
卓海鸥 唐建成 叶楠. 液相原位反应法制备Cu-Y2O3复合材料[J]. 金属学报, 2012, 48(12): 1474-1478.
ZHUO Haiou TANG Jiancheng YE Nan.
Cu–Y2O3 COMPOSITES PREPARED BY LIQUID PHASE IN SITU REACTION[J]. Acta Metall Sin, 2012, 48(12): 1474-1478.
| [1] Zhang S L, Yin Z M. Mater Rev, 2003; 17: 26(张生龙, 尹志民. 材料导报, 2003; 17: 26)[2] Li Z Y, Shen J, Cao F Y, Li Q C. J Mater Process Technol, 2003; 35: 60[3] Liu P, Kang B X, Cao X G, Hang J L, Gu H C. Acta Metall Sin, 1999; 35: 561(刘平, 康布熙, 曹兴国, 黄金亮, 顾海澄. 金属学报, 1999; 35: 561)[4] Li Q, Ma B, Li L, Hang G J, Chen C L, Xie S S. Rare Met Mater Eng, 2011; 40(suppl): 132(李 强, 马彪, 李雷, 黄国杰, 陈春玲, 谢水生. 稀有金属材料与工程, 2011; 40(增刊): 132)[5] Yan P, Lin C G, Cui S, Lu Y J, Zhou Z L, Li Z D. J Wuhan Univ Technol, 2011; 26: 902[6] Shen Y T, Cui C X, Meng F B, Wu R J. Acta Metall Sin, 1999; 35: 888(申玉田, 崔春翔, 孟凡斌, 吴人洁. 金属学报, 1999; 35: 888)[7] Tian B H, Liu P, Song K X, Li Y, Liu Y, Ren F Z, Su J H. Mater Sci Eng, 2006; A435–436: 750[8] Nagorka M S, Levi C G, Lucas G E, Ridder S D. Mater Sci Eng, 1991; A142: 277[9] Chakrabarti D J, Laughlin D E. In: Massalski T B ed., Binary Alloy Phase Diagrams. Ohio: American Society for Metals, 1986: 977[10] Engels J M, Gasgnier M, Blaise G. J Alloys Compd, 1998; 267: 294[11] Hu H Q. Metal Solidification Principle. Beijing: China Machine Press, 1981: 110(胡汉起 著. 金属凝固原理. 北京: 机械工业出版社, 1981: 110)[12] Ribis J, Carlan Y. Acta Mater, 2012; 60: 238[13] Ribis J, Lozano–Perez S. Mater Lett, 2012; 74: 143[14] Hirsch P, Howie A, Nicholson R B, Pashley D W. Translated by Liu A S, Li Y H. Electron Microscopy of Thin Crystals. Beijing: Science Press, 1983: 355 (Hirsch P, Howie A, Nicholson R B, Pashley D W著, 刘安生, 李永洪 \ 译. 薄晶体电子显微学. 北京: 科学出版社, 1983: 355)[15] Wang Y, Sun F, Dong X P, Zhang L T, Shan A D. Acta Metall Sin, 2010; 46: 334(王衣, 孙锋, 董显平, 张澜庭, 单爱党. 金属学报, 2010; 46: 334)[16] Stobrawa J P, Rdzawski Z M. Arch Mater Sci Eng, 2008; 30: 17[17] Toualbi L, Ratti M, Andr´e G, Onimus F, Carlan Y. J Nucl Mater, 2011; 417: 225[18] Cheng J Y, Yu F X, Ao X W. Adv Mater, 2011; 189–193: 70[19] Nagorka M S, Lucas G E, Levi C G. Metall Mater Trans, 1995; 26A: 873[20] Lee J, Jung J Y, Lee E, Park W J, Ahn S, Kim N J. Mater Sci Eng, 2000; A277: 274[21] Zhu A W, Chen J, Starke JR E A. Acta Mater, 2000; 48: 2239[22] Guo S H, Zhang M, Peng G Y, Tang J C. Adv Mater, 2011; 194–196: 1301[23] Gerold V, Haberkorn H. Phys Status Solidi, 1966; 16B: 675[24] Holzwarth U, Stamm H. J Nucl Mater, 2000; 279: 31[25] Ardell A J. Metall Mater Trans, 1985; 16A: 2131[26] Yong M, Ardell A J. Acta Mater, 2007; 55: 4419[27] Datta A, Soffa W A. Acta Mater, 1976; 24: 987 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|