| 外场作用下BaTiO3单晶裂纹扩展和畴变 |
| 姜冰1), 郭志猛1), 邢献然2) |
1) 北京科技大学冶金与生态工程学院, 北京 100083
2) 北京科技大学新材料技术研究院, 北京 100083 |
|
| CRACK PROPAGATION AND DOMAIN SWITCHING IN BaTiO3 SINGLE CRYSTALS UNDER EXTERNAL FIELD |
| JIANG Bing1), XING Xianran1), GUO Zhimeng2) |
1) School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083
2) Advanced Material and Technology Institute, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
姜冰 郭志猛 邢献然. 外场作用下BaTiO3单晶裂纹扩展和畴变[J]. 金属学报, 2011, 47(5): 605-610.
,
,
.
CRACK PROPAGATION AND DOMAIN SWITCHING IN BaTiO3 SINGLE CRYSTALS UNDER EXTERNAL FIELD[J]. Acta Metall Sin, 2011, 47(5): 605-610.
| [1] Yang W. Mechatronic Reliability. Beijing: Tsinghua University Press, 2001: 1(杨卫. 力电失效学. 北京: 清华大学出版社, 2001: 1)[2] Lynch C S. Acta Mater, 1996, 44: 4137[3] Lu W, Fang D N, Hwang K C. Acta Mater, 1999; 47: 2913[4] Li F X, Rajapakse R K N D. Acta Mater, 2007; 55: 6472[5] Shaikh M G, Phanish S. Sivakumar S M. Comput Mater Sci, 2006; 37: 178[6] Tang L P, Xie S H, Zheng X J, Zhou Y C, Li J Y. Mech Mater, 2008; 40: 362[7] Tan X, Shang J K. J Appl Phys, 2004, 96: 2805[8] Zhang Z K, Fang D N, Soh A K. Mech Mater, 2006; 38: 25[9] Roelofs A, Bottger U, Waser R. Appl Phys Lett, 2000; 77: 3444[10] Shin S, Baek J, Hong J W, Khim Z G. J Appl Phys, 2004; 96: 4372[11] Jiang B, Bai Y, Chu W Y, Shi S Q, Qiao L J. Su Y J. Appl Phys Lett, 2008; 93: 152905[12] Zhang Z H, Qi X Y, Duan X F. Appl Phys Lett, 2006; 89: 242905[13] Park J H, Park J, Lee K B. Appl Phys Lett, 2007; 91: 012906[14] Fang F, Yang W, Zhang F C, Luo H S. J Am Ceram Soc, 2005; 88: 2491[15] Huang H Y, Chu W Y, Su Y J, Qiao L J, Gao K W. Mater Sci Eng, 2005; B122: 1[16] Wang F, Su Y J, He J Y, Qiao L J, Chu W Y. Scr Mater, 2006; 54: 201[17] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. Appl Phys Lett, 2003; 82: 1583[18] Kounga Njiwa A B, Lupascu D C, Rodel J. Acta Mater, 2004; 52: 4919[19] Hwang S C, Lynch C S, McMeeking R M. Acta Metall Mater, 1995; 43: 2073[20] Meschke F, Kollek A, Schneider G A. J Eur Ceram Soc, 1997; 17: 1143[21] Busche M J, Hsia K J. Scr Mater, 2001; 44: 207[22] Beom H G, Kang K J. Acta Mech, 2006; 185: 201[23] Jiang Y J, Fang D N, Li F X. Appl Phys Lett, 2007; 90: 222907[24] Jiang B, Bai Y, Cao J L, Su Y J, Shi S Q, Chu W Y, Qiao L J. J Appl Phys, 2008; 103: 116102[25] Jiang B, Bai Y, Chu W Y, Shi S Q, Qiao L J. Su Y J. Appl Surf Sci, 2008; 254: 5594[26] Huang K Z, Wang Z Q. Macro–Micro–Mechanics and Strengthening and Toughening Design of Materials, Beijing: Tsinghua University Press, 2003: 182(黄克智, 王自强. 材料的宏微观力学与强韧化设计. 北京: 清华大学出版社, 2003: 182)[27] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environment Sensitive Fracture. Beijing: Science Press, 2000: 77(褚武扬, 乔利杰, 陈奇志, 高克玮. 断裂与环境断裂. 北京: 科学出版社, 2000: 77) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|