高铌TiAl合金在疲劳蠕变作用下的裂纹萌生及扩展 |
余龙1, 宋西平1( ), 张敏1, 李宏良1, 焦泽辉2, 于慧臣2 |
1 北京科技大学新金属材料国家重点实验室, 北京100083 2 中航工业北京航空材料研究院先进高温结构材料重点实验室, 北京100095 |
|
CRACK INITIATION AND PROPAGATION OF HIGH Nb-CONTAINING TiAl ALLOY IN FATIGUE-CREEP INTERACTION |
YU Long1, SONG Xiping1( ), ZHANG Min1, LI Hongliang1, JIAO Zehui2, YU Huichen2 |
1 State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083 2 Science and Technology on Advanced High Temperature Structural Materials Laboratory, AVIC Beijing Institute of Aeronautical Materials, Beijing 100095 |
引用本文:
余龙, 宋西平, 张敏, 李宏良, 焦泽辉, 于慧臣. 高铌TiAl合金在疲劳蠕变作用下的裂纹萌生及扩展[J]. 金属学报, 2014, 50(10): 1253-1259.
Long YU,
Xiping SONG,
Min ZHANG,
Hongliang LI,
Zehui JIAO,
Huichen YU.
CRACK INITIATION AND PROPAGATION OF HIGH Nb-CONTAINING TiAl ALLOY IN FATIGUE-CREEP INTERACTION[J]. Acta Metall Sin, 2014, 50(10): 1253-1259.
[1] |
Kim Y W. JOM, 1989; 41(7): 24
|
[2] |
Kim Y W. Acta Metall Mater, 1992; 40: 1121
|
[3] |
Zhang Y G,Han Y F,Chen G L,Guo J T,Wan X J,Feng D. Structural Intermetallics. Beijing: National Defense Industry Press, 2001: 705
|
[3] |
(张永刚,韩雅芳,陈国良,郭建亭,万晓景,冯 涤. 金属间化合物结构材料. 北京: 国防工业出版社, 2001: 705)
|
[4] |
Chen G L,Lin J P.Physical Metallurgy for the structural Ordered Intermetallics. Beijing: Metallurgical Industry Press, 1999: 285
|
[4] |
(陈国良,林均品. 有序金属间化合物结构材料物理金属学基础. 北京: 冶金工业出版社, 1999: 285)
|
[5] |
Chen G L, Wang X T, Ni K Q, Hao S M, Cao J X, Ding J J, Zhang X. Intermetallics, 1996; 4: 13
|
[6] |
Zhang W J, Deevi S C, Chen G L. Intermetallics, 2002; 10: 403
|
[7] |
Tetsui T. Intermetallics, 2002; 10: 239
|
[8] |
Chen G L, Sun Z Q, Zhou X. Mater Sci Eng, 1992; A153: 597
|
[9] |
Chen G L, Sun Z Q, Zhou X. Corrosion, 1992; 48: 939
|
[10] |
Li S J, Liu Z C, Lin J P, Chen G L, Zhang W J. Rare Met Mater Eng, 2002; 31: 31
|
[10] |
(李书江, 刘自成, 林均品, 陈国良, 张卫军. 稀有金属材料与工程, 2002; 31: 31)
|
[11] |
He S F, Lin J P, Xu X J, Gao J F, Wang Y L, Song X P, Chen G L. Rare Met Mater Eng, 2006; 35: 257
|
[11] |
(何素芳, 林均品, 徐向俊, 高建峰, 王艳丽, 宋西平, 陈国良. 稀有金属材料与工程, 2006; 35: 257)
|
[12] |
Chen W R, Triantafillou J, Beddoes J, Zhao L. Acta Metall Sin (Engl Lett), 1996; 9: 565
|
[13] |
Nagai H, Takahashi T, Oikawa H. J Mater Sci, 1990; 25: 629
|
[14] |
Kimm D I, Wolfenstine J. Scr Metall Mater, 1994; 30: 615
|
[15] |
Wang J N, Zhu J, Wu J S, Du X W. Acta Meter, 2002; 50: 1307
|
[16] |
Zhang W J, Chen G L, Appel F, Nieh T G, Deevi S C. Mater Sci Eng, 2001; A315: 250
|
[17] |
Sastry S M L, Lipsitt H A. Metall Trans, 1977; 8A: 299
|
[18] |
Malakondaiah G, Nicholas T. Metall Mater Trans, 1996; 27A: 2239
|
[19] |
Gloanec A L, Jouiad M, Bertheau D, Grange M, Henaff G. Intermetallics, 2007; 15: 520
|
[20] |
Gloanec A L, Milani T, Henaff G. Int J Fatigue, 2010; 32: 1015
|
[21] |
Cao R, Lin Y Z, Hu D, Chen J H. Eng Fract Mech, 2008; 75: 4343
|
[22] |
Kim S W, Kumar K S, Oh M H, Wee D M. Intermetallics, 2007; 15: 976
|
[23] |
Mine Y J, Fujisaki H, Matsuda M, Takeyama M, Takashima K. Scr Mater, 2011; 65: 707
|
[24] |
Li X D, Wang X S, Ren H H, Chen Y L, Mu Z T. Corros Sci, 2012; 55: 26
|
[25] |
Wang X S, Yan C K, Li Y, Xue Y B, Meng X K, Wu B S. Int J Fract, 2008; 151: 269
|
[26] |
Wang X S, Fan J H. Int J Fatigue, 2006; 28: 79
|
[27] |
Polak J, Man J, Petrenec M, Tobias J. Int J Fatigue, 2012; 39: 103
|
[28] |
Christ H J, Wamukwamba C K, Mughrabi H. Mater Sci Eng, 1997; A234-246: 382
|
[29] |
Zhang J S. Deformation and Fracture of Materials at High Temperature. Beijing: Science Press, 2007: 426
|
[29] |
(张俊善. 材料的高温变形与断裂. 北京: 科学出版社, 2007: 426)
|
[30] |
Yu L, Song X P, Zhang M, Lin J P, Jiao Z H, Yu H C. Rare Met Mater Eng, 2014; 43: 881
|
[30] |
(余 龙, 宋西平, 张 敏, 林均品, 焦泽辉, 于慧臣. 稀有金属材料工程, 2014; 43: 881)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|