| Fe81Ga19合金<001>取向单晶生长及磁致伸缩性能 |
| 陈立彪, 朱小溪, 李川, 刘敬华, 蒋成保, 徐惠彬 |
| 北京航空航天大学材料科学与工程学院 空天材料与服役教育部重点实验室, 北京 100191 |
|
| <001> ORIENTED SINGLE CRYSTAL GROWTH AND MAGNETOSTRICTION OF Fe81Ga19 ALLOYS |
| CHEN Libiao, ZHU Xiaoxi, LI Chuan, LIU Jinghua, JIANG Chengbao, XU Huibin |
| Key Laboratory of Aerospace Materials and Performance (Ministry of Education), School of Materials Science and Engineering, Beihang University, Beijing 100191 |
引用本文:
陈立彪 朱小溪 李川 刘敬华 蒋成保 徐惠彬. Fe81Ga19合金<001>取向单晶生长及磁致伸缩性能[J]. 金属学报, 2011, 47(2): 169-172.
,
,
,
,
,
.
<001> ORIENTED SINGLE CRYSTAL GROWTH AND MAGNETOSTRICTION OF Fe81Ga19 ALLOYS[J]. Acta Metall Sin, 2011, 47(2): 169-172.
| [1] Clark A E, Hathaway K B, Wun–Foglea M, Restorff J B, Lograsso T A, Keppens V M, Petculescu G, Taylor R A. J Appl Phys, 2003; 93: 8621[2] Datta S, Atulasimha J, Mudivarthi C, Flatau A B.J Magn Magn Mater, 2010; 322: 2135[3] Kellogg R A, Russell A M, Lograsso T A, Flatau A B, Clark A E, Wun–Fogle M. Acta Mater, 2004; 52: 5043[4] Kellogg R A, Flatau A B, Clark A E, Wun–Fogle M, Lograsso T A. J Appl Phys, 2002; 91: 7821[5] Clark A E, Restorff J B, Wun–Fogle M, Lograsso T A, Schlagel D L. IEEE Trans Magn, 2000; 36: 3238[6] Cullen J, Zhao P, Wuttiga M. J Appl Phys, 2007; 101: 123922[7] Ruffoni M P, Pascarelli S, Gr¨ossinger R, Sato Turtelli R, Bormio–Nunes C, Pettifer R F. Phys Rev Lett, 2008; 101: 147202[8] Mudivarthi C, Laver M, Cullen J, Flatau A B, Wuttig M. J Appl Phys, 2010; 107: 09A957[9] Khachaturyan A G, Viehland D. Metall Mater Trans, 2007; 38A: 2308[10] Khachaturyan A G, Viehland D. Metall Mater Trans, 2007; 38A: 2317[11] Bhattacharyya S, Jinschek J R, Khachaturyan A, Cao H, Li J F, Viehland D. Phys Rev, 2008; 77B: 104107[12] Summers E M, Lograsso T A, Wun–Fogle M. J Mater Sci, 2007; 42: 9582[13] Atulasimha J, Flatau A B. J Intell Mater Syst Struct, 2008; 19: 1371[14] Clark A E, Yoo J H, Cullen J R, Wun–Fogle M, Petculescu G, Flatau A. J Appl Phys, 2009; 105: 07A913[15] Wun–Foglea M, Restorff J B, Clark A E, Dreyer E, Summers E. J Appl Phys, 2005; 97: 10M301[16] Clark A E, Teter J P, McMasters O D. J Appl Phys, 1988; 63: 3910[17] Rafique S, Cullen J R, Wuttig M, Cui J. J Appl Phys, 2004; 95: 6939 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|