| FH550级海洋平台用钢冲击断裂行为实验研究 |
| 周砚磊, 徐洋, 陈俊, 刘振宇 |
| 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110819 |
|
| EXPERIMENTAL STUDY OF THE IMPACT FRACTURE BEHAVIOR OF FH550 OFFSHORE PLATFORM STEEL |
| ZHOU Yanlei, XU Yang, CHEN Jun, LIU Zhenyu |
| State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819 |
引用本文:
周砚磊 徐洋 陈俊 刘振宇. FH550级海洋平台用钢冲击断裂行为实验研究[J]. 金属学报, 2011, 47(11): 1382-1387.
,
,
,
.
EXPERIMENTAL STUDY OF THE IMPACT FRACTURE BEHAVIOR OF FH550 OFFSHORE PLATFORM STEEL[J]. Acta Metall Sin, 2011, 47(11): 1382-1387.
| [1] Sun X J, Xu H Q, Li W S. Shandong Metall, 2009; 31(3): 11(孙宪进, 徐洪庆, 李旺生. 山东冶金, 2009; 31(3): 11)[2] Di G B, Liu Z Y, Hao L Q, Liu X H. Mater Mech Eng, 2008; 32(8): 1(狄国标, 刘振宇, 郝利强, 刘相华. 机械工程材料, 2008; 32(8): 1)[3] Lu Z X, Wang F C, Zhang Y Y, Guo A M. Res Iron Steel, 2005; 6: 17(陆在学, 汪福成, 张云燕, 郭爱民. 钢铁研究, 2005; 6: 17)[4] Nobuo S, Shinji M, Shigeru E. JFE Tech Rep, 2008; 11: 1[5] Zhang X Z, Knott J F. Acta Mater, 1999; 47: 3483[6] Chai F, Yang C F, Zhang Y Q, Xu Z. J Iron Steel Res, 2005; 17: 42(柴锋, 杨才福, 张永权, 徐洲. 钢铁研究学报, 2005; 17: 42)[7] Guo A M, Zou D H, Yi L X, Dong H X, Li P H, Liu K, Wu K M. Acta Metall Sin, 2009; 45: 390(郭爱民, 邹德辉, 易伦雄, 董汉雄, 李平和, 刘 凯, 吴开明. 金属学报, 2009; 45: 390)[8] Chen Y, Lambert S. Int J Fract, 2003; 124: 179[9] Kunio T, Shimizu M, Yamada K, Suzuki H. Eng Fract Mech, 1975; 7: 411[10] Yong Q L. Secondary Phases in Steels. Beijing: MetallurgicalIndustry Press, 2006: 27(雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 27)[11] Fang H S, Feng C, Zheng Y K, Zheng X H, Zhang C, Bai B Z. Acta Metall Sin, 2007; 43: 583(方鸿生, 冯春, 郑燕康, 郑秀华, 张弛, 白秉哲. 金属学报, 2007; 43: 583)[12] Cui Y X, Wang C L. Fracture Analysis. Harbin: Harbin Institute of Technology Press, 1998: 73(崔约贤, 王常利. 金属断口分析. 哈尔滨: 哈尔滨工业大学出版社, 1998: 73)[13] Wang X S, Liang F, Zeng Y P, Xie X S. Acta Metall Sin, 2005; 41: 1272(王习术, 梁锋, 曾燕屏, 谢锡善. 金属学报, 2005; 41: 1272)[14] Beachem C D. Metall Trans, 1975; 6A: 377[15] Schawlbe K. Eng Fract Mech, 1977; 9: 795[16] David B. Elementary Engineering Fracture Mechanics. Netherlands: Martinus Nijhoff Publishers, 1986: 1[17] Qiao Y, Argon A S. Mech Mater, 2003; 35: 313[18] Qiao Y, Argon A S. Mech Mater, 2003; 35: 129 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|