| Fe-B共晶合金的净化及超过冷的获得 |
| 杨长林;杨根仓;刘峰;周尧和 |
| 西北工业大学凝固技术国家重点实验室 |
|
| THE PURIFICATION AND HYPERCOOLING OF Fe-B EUTECTIC ALLOY |
| 西北工业大学凝固技术国家重点实验室 |
引用本文:
杨长林; 杨根仓; 刘峰; 周尧和 . Fe-B共晶合金的净化及超过冷的获得[J]. 金属学报, 2008, 44(8): 956-960 .
[1]Herlach D M.Mater Sci Eng,1994;R12:177 [2]Wilde G,Grler G P,Willnecker R.Appl Phys Lett,1996; 69:2995 [3]Yang C L,Yang G C,Lu Y P,Chen J Q,Zhou Y H.Acta Metall Sin,2005;41:1053 (杨长林,杨根仓,卢一平,陈甲琪,周尧和.金属学报,2005;41:1053) [4]Yang C L,Yang G C,Liu F,Chen Y Z,Liu N,Chen D, Zhou Y H.Physics,2006;373B:136 [5]Yang C L,Liu F,Yang G C,Chen Y,Liu N,Zhou Y H. Appl Phys,2007;86A:231 [6]Hu H Q.Principle of Metal Solidification.2nd ed,Beijing: China Machine Press,2000:256 (胡汉起.金属凝固原理.第2版,北京:机械工业出版社,2000:256) [7]Kui H W,Greer A L,Turnbull D.Appl Phys Left,1984; 45:615 [8]Zhou Y H,Hu Z Q,Ji W Q.Solidification Technology. Beijing:China Machine Press,1998:45 (周尧和,胡壮麒,介万奇.凝固技术.北京:机械工业出版社,1998:451 [9]Wei B B.PhD Thesis,Northwestern Polytechnicai Uni- versity,Xi'an,1989 (魏炳波.西北工业大学博士学位论文,西安,1989) [10]Powell G L F.TMS-AIME,1968;242:2133 [11]Kattamis T Z,Flemings M C.Trans TMS-AIME,1966; 236:1523 [12]Zhang Z Z.PhD Thesis,Northwestern Polytechnical Uni- versity,Xi'an,2000 (张振忠.西北工业大学博士学位论文,西安,2000) [13]Perepezko J H.Mater Sci Eng,1997;A226-228:374 [14]Singh R N,Jaju R P,Ali I.Physics,2001;299B:108 [15]Pan S Q.New Glass.Shanghai:Tongji University Press, 1992:30 (潘守芹.新型玻璃.上海:同济大学出版社,1992:30) [16]Battezzati L,Antonione C,Baricco M.J Alloys Compd, 1997;247:16 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|