| 板坯连铸结晶器电磁制动和吹氩过程的多相流动现象 |
| 于海岐;朱苗勇 |
| 辽宁省沈阳市东北大学 |
|
| MULTIPHASE FLOW PHENOMENA IN A SLAB CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC BRAKE AND ARGON GAS INJECTION |
| YU Hai-Qi |
| 辽宁省沈阳市东北大学 |
引用本文:
于海岐; 朱苗勇 . 板坯连铸结晶器电磁制动和吹氩过程的多相流动现象[J]. 金属学报, 2008, 44(5): 619-625 .
,
.
MULTIPHASE FLOW PHENOMENA IN A SLAB CONTINUOUS CASTING MOLD WITH ELECTROMAGNETIC BRAKE AND ARGON GAS INJECTION[J]. Acta Metall Sin, 2008, 44(5): 619-625 .
[1]Thomas B G,Dennisov A,Bai H.80th Steelmaking Con- ference,Warrendale,PA:Iron and Steel Society,1997:375 [2]Thomas B G,Huang X.76th Steelmaking Conference, Warrendale,PA:Iron and Steel Society,1993:273 [3]Sussman R C,Burns M T,Huang X,Thomas B G.lOth Process Technology Conference Proceedings,Warrendale, PA:Iron and Steel Society,1992:291 [4]Noriko K,Toshio I,Jun K,Norichika A.ISIJ Int,2002; 42:1251 [5]Li B K,Toshimitsu O,Takateru U.Metall Mater Trans, 2000;31B:1491 [6]Li B K,Fumitaka T.ISIJ Int,2003;43:923 [7]Li B K,He J C,Jia G L,Gao Y Y.Acta Metall Sin,1997; 33:1207 (李宝宽,赫冀成,贾光霖,高允彦.金属学报,1997;33:1207) [8]Lei H,Jin Y L,Zhu M Y,He J C.J Iron Steel Res,2002; 14(3):13 (雷洪,金永丽,朱苗勇,赫冀成.钢铁研究学报,2002;14(3):13) [9]Lei H,Zhu M Y,Wang W Z.Eng Chem Metall,1999;20: 193 (雷洪,朱苗勇,王文忠.化工冶金,1999;20:193) [10]Liu G M,Shi S Q,Deng K,Ren Z M.Iron Steel,2007; 42(7):23 (刘光穆,石绍清,邓康,任忠鸣.钢铁,2007;42(7):23) [11]Wei J,Sun Y H,Cai K K,Zhou Y C,Wei Z K.Iron Steel, 2007;42(8):32 (魏军,孙彦辉,蔡开科,周英超,魏祖康.钢铁,2007;42(8):32) [12]Chen Z H,Wang E G,Zhang X W,He J C.Acta Metall Sin,2007;43:422 (陈芝会,王恩刚,张兴武,赫冀成.金属学报,2007;43:422) [13]Zhang G F,Shen H F,Wang L,Liu B C.Foundry,2005; 54:484 (张桂芳,沈厚发,王镭,柳百成.铸造,2005;54:484) [14]Fluent Inc.Fluent 6.3 Magnetohydrodynamics (MHD) Module Manual,Chapter 1,Lebanon,NH,2006:1 [15]Man Y H,Hyun G,Seung H S.J Mater Process Technol, 2003;133:322 [16]Fluent Inc.Fluent 6.3 User's Guide,Chapter 22, Lebanon,NH,2006:1 [17]Pfeiler C,Wu M,Ludwig A.Mater Sci Eng,2005;A413: 115 [18]Zhang L F,Yang S B,Cai K K,Li J Y,Wan X G,Thomas B G.Metall Mater Trans,2007;38B:63G |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|