| Al-Li-Mg(Ti)合金形成焓的EAM研究 |
| 侯育花 唐 美 徐海龙 方 杰 王建川 欧阳义芳 |
| (广西大学物理科学与工程技术学院; 南宁 530004) |
|
| The formation enthalpies of intermetallic compounds composed of Al, Li and Mg calculate with EAM |
| Yi-Fang OUYANG |
| 广西大学物理科学与工程技术学院 |
引用本文:
侯育花; 唐美; 徐海龙; 方杰; 王建川; 欧阳义芳 . Al-Li-Mg(Ti)合金形成焓的EAM研究[J]. 金属学报, 2008, 44(2): 134-138 .
,
,
,
,
,
.
The formation enthalpies of intermetallic compounds composed of Al, Li and Mg calculate with EAM[J]. Acta Metall Sin, 2008, 44(2): 134-138 .
[1]Ouyang Y F,Chen H M,Zen F J,Du Y,Feng Y P.Proc 13th National Symposium in Phase Diagrams China- Japan Joint Symposium on Phase Diagram.Xiamen:Xi- amen University,2006 [2]Sluiter M,Fontaine D De,Guo X Q,Pldloucky R,Free- man A J.Phys Rev,1994;42B:10460 [3]Das G P,Aryab A,Banerjeeb S.Intermetallics,1996;4: 625 [4]Sluiter M,Wantanabe Y,Fontaine D De,Kawazoe Y. Phys Rev,1996;42B:6137 [5]Daw M S,Baskes M I.Phys Rev Lett,1983;50:1285 [6]Daw M S,Baskes M I.Phys Rev Lett,1984;29:6443 [7]Norskov J K.Phys Rev,1982;26B:2875 [8]Norskov J K,Lang N D.Phys Rev,1980;21B:2131 [9]Stott M J,Zaremba E.Phys Rev,1980;22B:1564 [10]Johnson R A.Phys Rev,1990;41B:9717 [11]Ouyang Y F,Zhang B W,Liao S Z,Jin Z P.Phys Rev, 1996;101B:161 [12]Zhang B W,Ouyang Y F.Phys Rev,1993;48B:3022 [13]Zhang B W,Ouyang Y F.Z Physik,1993;92B:431 [14]Ouyang Y F,Zhang B W.Phys Lett,1994;192A:79 [15]OuyangY F,Zhang B W,Liao S Z,Jin Z P,Chen H M. Trans Nonferrous Met Soc Chin,1998;8:60 [16]Hu W Y,Xu H D,Shu X L.J Phys D:Appl Phys,2000; 33:711 [17]Ouyang Y F,Zhong X P,Tao X M.Mater Sci Forum, 2005;52:57 [18]Li S T.Elements of X-Ray Crystal.Beijing:Metallurgi- cal Industry Press,1990 [19]Kittel C.Introduction to Solid State Physics.7th ed.New York:John Wiley & Sons Inc,1976:2 [20]Boer F R de,Room R,Mattens W C M,Miedema A R, Niessen A K.Cohension in Metals:Transition Metals Al- loys.Amsterdam:Horth-Holland,1988:716 [21]McAlister A J.Bull Alloy Phase Diagram,1982;3:177 [22]Saboungi M A,Husi C C.Calphad,1977;1:237 [23]Jelinek B,Houze J,Kim S H,Horstemeyer M F,Baskes M I.Phys Rev,2007;75B:054106 [24]Hultgren R,Desai P D,Hawkins D T,Gleiser N,Kelly K K.Selected Values of Thermodynamic Properties of Bi- nary Alloys.Metals Park,OH:ASM,1973 [25]Shu X L.PhD Dissertation,Hunan University,Changsha, 1998 (舒小林.湖南大学博士学位论文,长沙,1998) [26]Fu C L,Yoo M H.Intermetallics,1993;1:59 [27]Farkas D.Model Simul Mater Sci Eng,1994;2:975 [28]Wang T M,Wang B Y,Ju X,Gu Q,Wang Y X,Gao F. Chin Phys Lett,2001;18:361 [29]Benedek R,Van de Walle A,Gerstl S S A,Asta M,Seid- man D N.Phys Rev,2005;71B:094201 [30]Zou J,Fu C L,Yoo M H.Intermetallics,1995;3:265 [31]Ghosh G,Vaynman S,Asta M,Fine M E.Intermetallics, 2007;15:44 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|