| 电沉积制备的两种形貌Sn薄膜锂离子嵌入电极性能的比较 |
| 李昌明;黄启明;张仁元;李伟善;赵灵智;胡社军 |
|
| A comparative study on the performances of thin film and granular tin as Li ion insertion electrodes prepared by electrodeposition |
| Chang-Ming LI;;;; |
引用本文:
李昌明; 黄启明; 张仁元; 李伟善; 赵灵智; 胡社军 . 电沉积制备的两种形貌Sn薄膜锂离子嵌入电极性能的比较[J]. 金属学报, 2007, 43(5): 515-520 .
,
,
,
,
,
.
A comparative study on the performances of thin film and granular tin as Li ion insertion electrodes prepared by electrodeposition[J]. Acta Metall Sin, 2007, 43(5): 515-520 .
[1] Gnanaraj J S, Levi M D, Levi E, Salitra G, Aurbach D, Fischer J E, Claye A. J Elctrochem Soc, 2001; 148: A525 [2] Iodata Y, Kubota T, Matsufuji A, Maekawa Y, Miyasaka T. Science, 1997; 276: 1395 [3] Kim H, Choi J, Sohn H J, Rang T. J Elctrochem Soc, 1999; 146: 4401 [4] Su S F, Cao G S, Zhao X B. Rare Met Mater Eng, 2005; 34: 452 (苏树发,曹高劭,赵新兵.稀有金属材料与工程, 2005;34: 452) [5] Kepler K D, Vaughey J T, Thackeray M M. J Power Sources, 1999; 81-82: 383 [6] Ren J G, He X M, Jiang C Y, Wan C R. Acta Metall Sin, 2006; 42: 727 (任建国,何向明,姜长印,万春荣.金属学报,2006;42:727) [7] Yang J, Winter M, Besenhard J O. Solid State Ionics, 1996; 90: 281 [8] Mukaibo H, Osaka T, Reale P, Panero S, Scrosati B, Wachtler M. J Power Sources, 2004; 132: 225 [9] Beaulieu L Y, Hewitt K C, Turner R L, Bonakdarpour A, Abdo A A, Christensen L, Eberman K W, Krause J L, Dahn J R. J Electrochem Soc, 2003; 150: A149 [10] Kim Y L, Lee H Y, Jang S W, Lee S J, Baik H K, Yoon Y S, Park Y S, Lee S M. Solid State Ionics, 2003; 160: 235 [11] Ehrlich G M, Durand C, Chen X, Hugener T A, Spiess F, Suib S L. J Electrochem Soc, 2000; 147: 886 [12] Wachtler M, Winter M, Besenhard J O. J Power Sources, 2002; 105: 151 [13] Zuo X X, Li W S, Liu J S. Prog Chem, 2003; 15: 441 (左晓希,李伟善,刘建生.化学进展,2003;15:441) [14] Zuo X X, Xu M Q, Li W S, Su D G, Liu J S. Electrochem Solid-State Lett, 2006; 9A: 196 [15] Xu M Q, Zuo X X, Li W S, Zhou H J, Liu J S, Yuan Z Z. Acta Phys-Chim Sin, 2006; 22: 335 (许梦清,左晓希,李伟善,周豪杰,刘建生,袁中直.物理化学学报,2006;22:335) [16] Huggins R A. J Power Sources, 1999; 81-82: 13 [17] Zhu C F, Cheng X Q, Shi P F. Battery Bimon, 2002; 32(1): 10 (朱承飞,程新群,史鹏飞.电池, 2002;32(1):10) [18] Courtney I A , Dahn J R. J Electrochem Soc, 1997; 144: 2045 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|