| Al-Cu-Ni-Fe四元体系中的准晶探讨 |
| 姜楠;王清;董闯 |
| 大连理工大学三束国家重点实验室 |
|
| Quasicrystals in Al-Cu-Ni-Fe Quaternary System |
| ;; |
| 大连理工大学三束国家重点实验室 |
引用本文:
姜楠; 王清; 董闯 . Al-Cu-Ni-Fe四元体系中的准晶探讨[J]. 金属学报, 2007, 43(4): 374-378 .
[1]Shechtman D,Blech I,Gratias D,Cahn J W.Phys Lett, 1984;53:1951 [2]Dong C.Quasicrystalline Materials.Beijing:National Defence Industry Press,1998:29 (董闯.准晶材料.北京:国防工业出版社,1998:29) [3]Wang R H.Physics in Quasicrystals.Beijing:Science ??Press,2004:4,12 (王仁卉.准晶物理学.北京:科学出版社,2004:4,12) [4]Qiang J B,Wang D H,Bao C M,Wang Y M,Xu W P, Song M L,Dong C.J Mater Res,2001;16:2653 [5]Dong C,Qiang J B,Wang Y M.Philos Mag,2006;86: 263 [6]Mayou D,Cyroy-Lackmann F,de Trambley G,Klein T. J Non-Cryst Solids,1993;153-154:412 [7]Gratias D,Calvayrac Y,Devaud-Rzepski J,Faudot F, Harmelin M,Quivy A,Bancet P A.Non-Cryst Solids, 1993;153-154:482 [8]Dong C,Perrot A,Dubois J M,Belin E.Mater Sci Forum, 1994;150-151:403 [9]Dong C.Chin J Mater Res,1995;9:89 [10]Pearson W B.The Crystal Chemistry and Physics of Met- als and Alloys.New York:Wiley-Interscience,1972:155 [11]Qiang J B,Wang D H,Bao C M.J Mater Res,2001;16: 2653 [12]Tsuda K,Terauchi M,Fujiwara A,Tsai A P.Inoue A, Masumoto T.J Non-Cryst Solids,1993:153:98 [13]Niessen A K,de Boer F R,Boom R,de Chatel P F,Mat- tens W C M,Miedema A R.CALPHAD,1983;7:51 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|