准晶增强的Mg-Zn-Al-(Y)合金热压缩变形行为 |
童剑1,2,黄华1,2,袁广银1,2,丁文江1,2 |
1. 上海交通大学材料科学与工程学院轻合金精密成型国家工程研究中心, 上海 200240
2. 上海交通大学材料科学与工程学院金属基复合材料国家重点实验室, 上海 200240 |
|
HOT COMPRESSION DEFORMATION BEHAVIOR OF Mg–Zn–Al–(Y) ALLOYS REINFORCED WITH QUASICRYSTAL |
TONG Jian 1,2, HUANG Hua 1,2, YUAN Guangyin 1,2, DING Wenjiang 1,2 |
1. Light Alloy Net Forming National Engineering Research Center, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240
2. The State Key Laboratory of Metal Matrix Composite, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240 |
引用本文:
童剑 黄华 袁广银 丁文江. 准晶增强的Mg-Zn-Al-(Y)合金热压缩变形行为[J]. 金属学报, 2011, 47(12): 1520-1526.
,
,
,
.
HOT COMPRESSION DEFORMATION BEHAVIOR OF Mg–Zn–Al–(Y) ALLOYS REINFORCED WITH QUASICRYSTAL[J]. Acta Metall Sin, 2011, 47(12): 1520-1526.
[1] Decker R F. Adv Mater Processes, 1998; 154(3): 31[2] Liu Q. Acta Metall Sin, 2010; 46: 1458(刘庆. 金属学报, 2010; 46: 1458)[3] Lu Y Z, Wang Q D, Ding W J. Mater Lett, 2000; 44: 265[4] Mukai T, Yamanoi M,Watanabe H, Higashi K. Scr Mater,2001; 45: 89[5] Kim W J, Hong S I, Kim Y S. Acta Mater, 2003; 51: 3293[6] Yang X Y, Zhang L. Acta Metall Sin, 2009; 45: 1303(杨续跃, 张 雷. 金属学报, 2009; 45: 1303)[7] Jin Q L, Shim S Y, Lim S G. Scr Mater, 2006; 55: 843[8] Shechtman D, Blech I, Gratias D, Cahn J W. Phys Rev Lett, 1984; 53: 1951[9] Yuan G Y, Liu Y, DingWJ. Mater Sci Eng, 2008; A474: 348[10] Liu Y, Yuan G Y, Lu C. J Mater Sci, 2008; 43: 5527[11] Somekawa H, Singh A, Mukai T. Adv Eng Mater, 2009; 11: 782[12] Yuan G Y, Amiya K, Kato H, Inoue A. J Mater Res, 2008; 19: 1531[13] Elser V. Phys Rev, 1985; 32B: 4892[14] Bourgeois L, Mendis C L, Muddle B C. Philos Mag Lett, 2001; 81: 709[15] Vogel M, Kraft O, Behm G. Scr Mater, 2001; 45: 517[16] Galiyev A, Kaibyshev R, Gottstein G. Acta Mater, 2001; 49: 1199[17] Agnew S R, Yoo M H, Tome C N. Acta Mater, 2001; 49: 4277[18] Li Z J, Jin Q L, Jiang Y H, Zhou R. Acta Metall Sin, 2009; 45: 924(李再久, 金青林, 蒋业华, 周荣. 金属学报, 2009; 45: 924)[19] Bae D H, Kim S H, Kim D H, Kim W T. Acta Mater, 2002; 50: 2343[20] Singh A, Watanabe M, Kato A, Tsai A P. Sci Technol Adv Mater, 2005; 6: 895[21] Lee J Y, Lim H K, Kim D H, Kim W T, Kim D H. Mater Sci Eng, 2008; A491: 349[22] Hu G X, Cai X. Fundamental of Material Science. Shanghai: Shanghai Jiao Tong University Press, 2004: 193(胡赓祥, 蔡旬.材料科学基础. 上海: 上海交通大学出版社, 2004: 193)[23] Yu K, Shi T, Wang R C, Li W X, Wang X Y, Cai Z Y. J Cent South Univ (Sci Technol), 2008; 39: 216(余琨, 史提, 王日初, 黎文献, 王晓艳, 蔡志勇.中南大学学报(自然科学版), 2008; 39: 216)[24] Poirier J P, translated by Guan D L. The Plastic Deformation of Crystals at High Temperature. Dalian: Dalian University of Science and Technology Press, 1989: 25(Poirier J P著, 关德林译. 晶体的高温塑性变形. 大连: 大连理工大学出版社,1989: 25)[25] Takuda H, Fujimoto H, Hatta N. J Mater Process Technol,1998; 80–81: 513 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|