| Ti-Zr-Ni-Cu非晶系的等电子浓度特征 |
| 羌建兵; 黄火根; 王清; 夏俊海; 董闯 |
| 大连理工大学三束表面改性国家重点实验室及大连理工大学原材料特种制备技术实验室;大连 116024;大连理工大学材料科学与工程学院;大连 116024 |
|
| E/A-CONSTANT PHENOMENA IN TI-ZR-NI-CU GLASS-FORMING SYSTEM |
| QIANG Jianbing; HUANG Huogen; WANG Qing;XIA Junhai; DONG Chuang |
引用本文:
羌建兵; 黄火根; 王清; 夏俊海; 董闯 . Ti-Zr-Ni-Cu非晶系的等电子浓度特征[J]. 金属学报, 2006, 42(6): 561-564 .
,
,
,
,
.
E/A-CONSTANT PHENOMENA IN TI-ZR-NI-CU GLASS-FORMING SYSTEM[J]. Acta Metall Sin, 2006, 42(6): 561-564 .
[1] Inoue A. Acta Mater, 2000; 40: 279 [2] Wang W H, Dong C, Shek C H. Mater Sci Eng, 2004; R44: 45 [3] Loffler J F. Intermetallics, 2003; 11: 529 [4] Wang Y M, Qiang J B, Wong C H, Shek C H, Dong C. J Mater Res, 2003; 18: 642 [5] Chen W W, Wang Y M, Qiang J B, Dong C. Acta Mater, 2003; 51: 1899 [6] Dong C, Wang Y M, Qiang J B, Wang D H, Chen W W, Shek C H. Mater Trans, 2004; 45: 1177 [7] Wang Q, Wang Y M, Qiang J B, Zhang X F, Wang D H, Dong C. Acta Metall Sin, 2004; 40: 1183 (王清,王英敏,羌建兵,张新房,王德和,董闯.金属学 报,2004;40:1183) [8] Zhang X F, Wang Y M, Peng M, Wang Q, Li D J, Dong C. Acta Metall Sin, 2004; 40: 1099 (张新房,王英敏,彭敏,王清,李德俊,董闯.金属学 报,2004;40:1099) [9] Shek C H, Wang Y M, Dong C. Mater Sci Eng, 2000; A291: 78 [10] Qiang J B, Wang Y M, Wang D H, Kramer M J, Dong C. Philos Mag Lett, 2003; 83: 467 [11] Qiang J B, Wang Y M, Wang D H, Kramer M J, Thiel P, Dong C. J Non-Cryst Solids, 2004; 334 & 335: 223 [12] Qiang J B, Huang H G, WangY M, Jiang N, Dong C. Acta Metall Sin, 2004; 40: 677 (羌建兵,黄火根,王英敏,姜楠,董闯.金属学报,2004; 40:677) [13] Cahn J W, Shechtman D, Gratias D. J Mater Res, 1986; 1: 13 [14] Haussler P. Phys Rep, 1992; 222: 65 [15] Hafner J, Krajci M. Phys Rev, 1993; 47B: 11795 [16] Mizutani U, Takeuchi T, Sato H, Mizutani U, Takeuchi T, Sato H. Prog Mater Sci, 2004; 49: 227 [17] Friedel J. Phys Acta, 1988; 61: 538 [18] Sachdev S, Nelson D R. Phys Rev Lett, 1984; 53: 1947 [19] Kelton K F, Lee G W, Gangopadhyay A K, Hyers R W, Rathz T J, Rogers J R, Robinson M B, Robinson D S. Phys Rev Lett, 2003; 90: 195504 [20] Kelton K F. J Non-Cryst Solids, 2004; 334/335: 253 [21] Altounian Z, Tu G H, Strom-Olsen J O, Muir W B. Phys Rev, 1981; 24B: 505 [22] Jiang J Z, Saksl K, Saida J, Inoue A, Franz H, Messel K, Lathe C. Appl Phys Lett, 2002; 80: 781w |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|