| 熔剂中添加LaCl3对Mg合金显微组织与性能的影响 |
| 吴国华 高洪涛 朱燕萍 丁文江 |
| 上海交通大学金属基复合材料国家重点实验室; 上海 200030 |
|
| EFFECT OF LaCl3 ADDITION IN FLUX ON THE MICROSTRUCTURE AND PROPERTIES OF MAGNESIUM ALLOYS |
| WU Guohua; GAO Hongtao; ZHU Yanping; DING Wenjiang |
| State Key Laboratory of Metal Matrix Composite; Shanghai Jiaotong University; Shanghai 200030 |
引用本文:
吴国华; 高洪涛; 朱燕萍; 丁文江 . 熔剂中添加LaCl3对Mg合金显微组织与性能的影响[J]. 金属学报, 2004, 40(7): 694-698 .
,
,
,
.
EFFECT OF LaCl3 ADDITION IN FLUX ON THE MICROSTRUCTURE AND PROPERTIES OF MAGNESIUM ALLOYS[J]. Acta Metall Sin, 2004, 40(7): 694-698 .
[1] Wu Z N, Li P J, LIU S X, Zeng D B. Foundry, 2001; 50 (10) : 583(吴振宁,李培杰,刘树勋,曾大本.铸造,2001;50(10) :583) [2] Zhai C Q, Ding W J, Xu X P, Deng Z W. Special Casts Nonferrous Alloy, 1997; (4) : 48(翟春泉,丁文江,徐小平,邓祖威.特种铸造及有色合金,1997;(4) :48) [3] Wu G H, Zhai C Q, Zeng X Q, Ding W J, Zhu Y P. Acta Metall Sin, 2003; 39(7) : 729(吴国华,翟春泉,曾小勤,丁文江,朱燕萍.金属学报,2003;39(7) :729) [4] Lunder O, Videm M, Nisancioglu K. Proc Soc Automotive Eng, Detroit: Society of Automotive Engineers, Inc., 1995: 352 [5] Mercer W E, Hillis J E. Proc Soc Automotive Eng, Detroit: Society of Automotive Engineers, Inc., 1992: 8 [6] Zeng X Q. PhD Dissertation, Shanghai Jiaotong University, Shanghai, 2000(曾小勤.上海交通大学博士学位论文,上海,2000) [7] Lu Y Z, Wang Q D.Zeng X Q, Zhu Y P. Mater Sci EngA, 2000; 278: 66 [8] Yi L, Jones H. Mater Sci Technol, 1996; 12: 651 [9] Wei L Y, Dunlop G L. J Alloy Compd, 1996; 232(1) : 264 [10] Luo Z P, Zhang S Q, Tang Y L, Song D Y. J Chin RareEarth Soc, 1995; 13(2) : 119(罗治平,张少卿,汤亚力,宋德玉.中国稀土学报,1995;13(2) :119) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|