| 钛合金精密铸造用陶瓷模壳研究 |
| 贾 清;崔玉友; 杨 锐 |
| (中国科学院金属研究所; 沈阳 110016) |
|
引用本文:
贾清; 崔玉友; 杨; 锐 . 钛合金精密铸造用陶瓷模壳研究[J]. 金属学报, 2004, 40(11): 1170-1174 .
[1] Jones S, Jolly M R, Lowis K. Br Ceram Trans, 2002; 101(3) : 106 [2] Campbell J. Mater Des, 2000; 21: 373. [3] Yuan C, Jones S, Withey P A, Marquis P M. Br Ceram Tran, 2002; 101(2) : 59. [4] Tong T F, Chen B, Jiang B J. Shell Mould Casting Process. Beijing: China Machine Press, 1991(佟天夫,陈冰,姜不居.熔模铸造工艺.北京:机械工业出版社, 1991) [5] Jia Q, Cui Y Y, Yang R. Inter J Mater Product Technol,2001; SPM 1:793 [6] Wang M R, Bao Y K, Sheng X Y. Spec Cast Non-ferrousAlloys, 1987; 4: 15(王慕荣,包彦堃,盛夏阳.特种铸造及有色合金, 1987;4:15) [7] Tong T F.Spec Cast Non-ferrous Alloys,1983;3:46(佟天夫.特种铸造及有色合金, 1983;3:46)N |
|