| X70管线钢不同温度下断裂韧性实验研究 |
| 杨政 郭万林 |
| 西安交通大学建筑工程与力学学院 西安710049 |
|
引用本文:
杨政; 郭万林 . X70管线钢不同温度下断裂韧性实验研究[J]. 金属学报, 2003, 39(9): 908-913 .
[1] Li H L. Welded Pipe Tube, 2000; 23: 43(李鹤林.焊管,2000;23:43) [2] Hertzberg R W. Deformation and Fracture Mechanics ofEngineering Materials. 2nd Edition, New York: Wiley,1983: 353 [3] Guo W L, Dong H R, Yang Z, Lu M X, Zhao X W, LuoJ H. Acta Metall Sin, 2001; 37: 386(郭万林,董蕙茹,杨政,路民旭,赵新伟,罗金衡.金属学报,2001;37:386) [4] Guo W L, Dong H R, Lu M X, Zhao X W. Int J PressureVessels Piping, 2002; 79: 403 [5] Kuang Z B, Ma F S. Crack Tip Fields. Xi'an : Xi'anJiaotong University Press, 2002: 71(匡震邦,马法尚.裂纹端部场.西安:西安交通大学出版社,2002:71) [6] Kwon S W, Sun C T. Int J Fract, 2000; 104: 291 [7] Rice J R. J Mech Phys Solids, 1968; 16: 1 [8] Hutchinson J W. 7 Mech Phys Solids, 1968; 16: 13 [9] O'Dowd N P, Shih C F. J Mech Phys Solids, 1991; 39:989 [10] Guo W L. Eng Fract Mech, 1995; 46(1) : 51 [11] Narasimhan R, Rosakis A J. J Appl Mech, 1990; 57, 607 [12] Nakamura T, Parks D M. J Mech Phys Solids, 1990; 38,787 [13] GB 4161-84, Standard Test Method for Plane-Strain Fracture Toughness of Metallic Materials, 1984(GB 4161-84,金属材料平面应变断裂韧性KIc试验方法,1984) [14] ASTM E399-83, Standard Test Method for Plane Strain Fracture Toughness of Metallic Materials, 1983 [15] ASTM E813-81, Metallic Materials-Standard Test Method for JIc, A Measure of Ductile Fracture Toughness, 1981 [16] GB 2038-91, Metallic Materials-Standard Test Method for JIc , a Measure Fracture Toughness, 1991(GB 2038-91,金属材料延性断裂韧度JIc试验方法,1991)j |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|