| 软接触电磁连铸技术分析 |
| 那贤昭 张兴中 |
| 钢铁研究总院连铸技术国家工程研究中心;北京100081 |
|
引用本文:
那贤昭; 张兴中 . 软接触电磁连铸技术分析[J]. 金属学报, 2002, 38(1): 105-108 .
[1] Cha Pil-Ryung, Hwang Yun-Seong, Nam Ho-Seok,Chung Soon-Hyo, Yoon Jong-Kyu. ISIJ fat, 1999; 38:403 [2] Toh T, Takeuchi E, Hojo M, Kawai H, Matsumura S. ISIJInt, 1997; 37: 1112 [3] Li T, Sassa K, Asai S. ISIJ Int, 1996; 36: 410 [4] Deng A Y, Yu G W, Jia G L, He J C. J Iron Steel Res,2001: 13(3): 10 (邓安元,于光伟,贾光霖,赫冀成 钢铁研究学报,2001;13(3):10) |
|