| La2O3-B4C系反应合成LaB6粉末 |
| 郑树起 闵光辉 邹增大 王效志 韩建德 |
| 山东大学材料科学与工程学院;济南250061 |
|
引用本文:
郑树起; 闵光辉; 邹增大; 王效志; 韩建德 . La2O3-B4C系反应合成LaB6粉末[J]. 金属学报, 2001, 37(4): 419-422 .
[1] Paderno Y, Paderno V, Filippov V. J. Alloys Compd,1995; 219: 116 [2] Yutani A, Kobayashi A, Kinbara A. Appl Surf Sci, 1993;70/71: 737 [3] Paderno V, Paderno Y J. Alloys Compd, 1995; 219: 228 [4] Johnson R W, Daane A H. J Am Ceram Soc, 1970; 65:909 [5] Strull D R, Prophet H. JANAF Thermochemical Tables.2nd ed., Washington: US Government Printing Office,1971 |
|