| Zr52.5Cu17.9Ni14.6Al10Ti5块体非晶退火后的力学性能 |
| 边赞 何国 |
| 北京科技大学新金属材料国家重点实验室; 北京 100083 |
|
引用本文:
边赞; 何国 . Zr52.5Cu17.9Ni14.6Al10Ti5块体非晶退火后的力学性能[J]. 金属学报, 2000, 36(7): 693-696 .
[1] Inoue A, Zhang T, Kim Y H. Mater Trans JIM, 1997; 9:749 [2] Doglione R, Spriano S, Battezzati L. Nanostrvct Mater,1997; 8: 447 [3] He G, Chen G L. Mater Sci Technol, 1998; 6: 105 [4] Spaepen F. Acta Metall, 1977; 25: 407 [5] Saffman P G, Tayer G I. Proc R Soc London, 1958; 245A:312 [6] Sethi K V, Gibala R, Hener A H. Scr Metall, 1978; 12:207 [7] Donovan P E, Stobbs W M. Acta Metall, 1981; 29: 1419 [8] Polk D E, Turnbull D. Acta Metall, 1972; 20: 493 [9] Pampilla C A. Scr Metall, 1972; 6: 915 [10] Li J C M. Metallic Glasses. Metals Park, Ohio: ASM,1978: 224 [11] Kawamura Y, Kato H, Inoue A, Masumoto T. Appl PhysLett, 1995; 67: 2008K |
|