| 非晶态合金磁性能与结构参数的定量关系 |
| 王学业 邱冠周 |
| 湘潭大学化学化工学院; 湘潭江411105 |
|
引用本文:
王学业; 邱冠周 . 非晶态合金磁性能与结构参数的定量关系[J]. 金属学报, 2000, 36(2): 123-125 .
[1] Yang YC, Pan Q. Sci China, 1992; B28(10): 1009(杨应昌,潘 琪.中国科学,1992;B28(10):1009) [2] Liu H L, Chen N Y. J Alloys Comp, 1996; 236: 30 [3] Shi S H, Wang X W, Chen J C. J Beijing Univ AeronautAstronaut, 1992; (4): 15(石双合,王绪威,陈金昌.北京航空航天大学学报,1922(4):15) [4] Li H, Jiang S T, Mei L M, Gao R W. Chin Sci Bull, 1994;39(9): 790(李 华,姜寿亭,梅良模,高汝伟.科学通报,1994;39(9):790) [5] Chen N Y, Xu Z H, Liu H L, Xu H. Computation Chem-istry and its Application. Shanghai: Shanghai Science andTechnology Press, 1987: 37(陈念贻,许志宏,刘洪霖,徐 桦.计算化学及其应用.上海:上海科学技术出版社,1987: 37) [6] Wang X Y, Qiu G Z, Wang D Z, Chen N Y. Trans NonferrousMet Soc China, 1998; 8(1): 142 [7] Wang Y H, Yang Y S. Amorphous Metallic Alloys. Beijing:Metallurgical industry Press, 1989: 202(王一禾,杨膺善.非晶态合金.北京:冶金工业出版社,1989:202) [8] Chen N Y, Li C H, Yao S W, Wang X Y. J Alloys Comp,1996; 234: 125 |
|