| Ti-24Al-11Nb合金感应凝壳熔炼(ISM)过程中Al元素的挥发损失行为 |
| 郭景杰 刘源 苏彦庆 丁宏升 贾均 |
| 哈尔滨工业大学材料科学与工程学院;哈尔滨 150001 |
|
引用本文:
郭景杰; 刘源; 苏彦庆; 丁宏升; 贾均 . Ti-24Al-11Nb合金感应凝壳熔炼(ISM)过程中Al元素的挥发损失行为[J]. 金属学报, 1999, 35(4): 416-420 .
[1] Dimiduk D M, Miracle D B. Mater Red Soc Symp Proc,1988; 133: 349 [2] Deng J, Zhang T X. Rear Met Mater Egg, 1991; 1: 10(邓炬,张太贤,稀有金属材料坏蛋工程,1991; 1: 10) [3] Petion A D. Metall Trans, 1986; 17A: 1211 [4] Lupis C H P, Elliott J F. Acta Metall, 1966; 14: 529 [5] Wang Z C, Zhou G Z. Set Chin, 1984; 10A: 959(王之昌,周国治.中国科学,1984; 10A: 959) [6] Su Y Q, Liu Y, Guo J J. J Harbin Inst Technol, in press(苏延庆,刘源,郭景杰.哈尔滨工业大学学报,待发表) [7] Midema A R, Chatel P P. Physica, 1980; 100B(1): 1 [8] Kohler F. Monatsh Chemie, 1960; 91: 738 [9] Kong F Y, Yang K N. Acta Metall Sin, 1991; 27: B361(孔凡亚,杨克努,金属学报,1991; 27: B361) [10] Yang K N, Kong C X. Acta Metall Sin, 1982; 18: 411(杨克努,孔从熙.金属学报,1982; 18: 411) [11] Chen E P, Fu J. Acta Metall Sin, 1984, 20: B1(陈恩普,傅杰.金属学报,1984; 20: B1) [12] Machlin E S. fons TMS AIME, 1960; 218: 314 [13] Zhang D C. fonsjewtng Phenomenon During Foundry Process. Harbin: Harbin institute of Technology Press, 1991:194(张东成.铸造过程传输现象.哈尔滨:哈尔滨工业大学出版社,1991: 194) [14] Kang X D. Vacuum Metallurpy. Shanghai: Shanghai Scienceand Technology Press, 1980: 154(康显登.真空冶金学.上海.上海科学技术出版社, 1980: 154)x |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|