| DZ40M钴基高温合金的中温蠕变形变与断裂 |
| 姜文辉 姚向东 |
| 中国科学院金属研究所; 沈阳 110015 |
|
引用本文:
姜文辉; 姚向东 . DZ40M钴基高温合金的中温蠕变形变与断裂[J]. 金属学报, 1999, 35(3): 253-256 .
[1] Leverant C R, Duhl D N. Metall Trans, 1971; 2: 907 [2] Leverant C R, Kear B H. Metall Trans, 1970; 1: 491 [3] EI-Magd E, Nicolini G, Farag M. Metall Mater Trans, 1996;27A: 747 [4] Yao X D, Zhang J H, Zhang Z Y, Li Y G, Zhao N R, GuanH R, Hu Z Q. Acta Metall Sin, 1995; 31: A320(姚向东,张静华,张志亚,李英敖,赵乃仁,管恒荣,胡壮麒.金属学报,1995;31:A320) [5] Mott N F. Philos Mag, 1953; 44: 742 [6] Taira S ed. Guo T W, Li A D, Xu J P trans. High Temperature Strength of Metal Materials: Theory & Design. Beijing:Science Press. 1983: 45(平修二[日]编,郭廷玮,李安定,徐介平译.金属材料的高温强度一理论、设计.北京:科学出版社,1983:45) [7] Sim C T. J Met, 1969; 21: 27 |
|