| 金属成形过程组织演变的Cellular Automaton模拟技术 |
| 李殿中 杜强 胡志勇 李依依 |
| 中国科学院金属研究所; 沈阳 110015 |
|
引用本文:
李殿中; 杜强; 胡志勇; 李依依 . 金属成形过程组织演变的Cellular Automaton模拟技术[J]. 金属学报, 1999, 35(11): 1201-1205 .
[1] Zhu P P, Smith R W. Acta Metall Mater, 1992; 40(12). 3369 [2] Spittle J A, Brown S G R. Acta Metall, 1989; 37(3): 1803 [3] Brown S G R, Spittle J A. In: Rappaz M, Ozgu M R, MahinK W eds, Modeling of Casting, Welding and Advanced Solidification Process-V, TMS, 1991: 395 [4] Rappaz M, Gandin Ch-A. Acta Metall Mater, 1993; 41(2):345 [5] Rappaz M, Gandin Ch-A. MRS Bull, 1994: 20 [6] Marx V, Reher F R, Gottstein G.Acta Mater, 1999, 47(4):1219 [7] Davies C H J. Scr Mater, 1997; 36(1): 35 [8] Numann J V. Theory of Self-Reproducing Automaton.Champaign: Univ. of Illinois Press, 1966: 30 [9] Kurz W, Giovanola B, Trivedi R. Acta Metall, 1986; 34(6):823 [10] Hunt J D. Mater Sci Eng, 1984; 65(2): 75 [11] Jacot A, Rappaz M. Acta Mater, 1999; 47(5): 1645 [12] Kumar M, Sasikumar R, Kesavan Nair P. Acat Mater, 1998;46(17): 6291 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|