| Fe_3Al金属间化合物的电学性能 |
| 余新泉;孙扬善;梅建平;孙国雄 |
| 东南大学材料科学与工程系;南京;210096;东南大学材料科学与工程系;南京;210096;东南大学材料科学与工程系;南京;210096;东南大学材料科学与工程系;南京;210096 |
|
| ELECTRICAL PROPERTIES OF Fe_3Al INTERMETALLICS |
| YU Xinquan;SUN Yangshan;MEI Jianping;SUN Guoxiong (Department of Materials Science and Engineering;Southeast University; Nanjing 210096) |
引用本文:
余新泉;孙扬善;梅建平;孙国雄. Fe_3Al金属间化合物的电学性能[J]. 金属学报, 1998, 34(11): 1126-1130.
,
,
,
.
ELECTRICAL PROPERTIES OF Fe_3Al INTERMETALLICS[J]. Acta Metall Sin, 1998, 34(11): 1126-1130.
1Mckamey C G, Devan J H, Tortoreli P T; Sikka V K. J Mater Res, 1991; 6: 1779 2何开元精密合金材料北京:冶金工业出版社,1991:226(He K Y. Precison Alloy Material.Beijing:Metallurgical Insdustry Press,1991:226) 3顾秉林,王喜坤.固体物理.北京:清华大学出版社。1989:209(Gu B L,Wang X K.Solid State Phys.Beijing:Qinghua Universsity Press,1989:209) 4 Dugdale J S. The Electrical Properties of Metals and Alloys. Edward Arhold(publishers) Ltd, 1977: 114 5 Hyde T A, Sellers C H, Wright J K, Wright R N.Scr Metall, 1993;1: 113 6 Lawlsy A; Vidoz E A、 Cahn R W Acta Metall, 1961; 9: 287 7 Anderson P W.Phys Rev,1958;109:1492 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|