| ZrO_2/Ni阶梯热障涂层的热冲击行为 |
| 胡望宇;管恒荣;孙晓峰;李诗卓;福本昌宏;岡根功 |
| 中国科学院金属研究所;沈阳;110015;湖南大学应用物理系长沙;410082;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;中国科学院金属研究所;沈阳;110015;丰桥技术科学大学;日本丰桥;丰桥技术科学大学;日本丰桥 |
|
| THERMAL SHOCK BEHAVIOR OF ZrO_2/Ni GRADED THERMAL BARRIER COATINGS |
| HU Wangyu; GUAN Hengrong; SUN Xiaofeng; LI Shizhuo; FUKUMOTO Masahiro;OKANE Isao(Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)(Department of Applied Physics; Hunan University; Changsha 410082)(Toyobashi University of Technology Toyobashi; Japan)Correspondent: SUN Xiaofeng; associate profssor Tel: (024)23843531-55608; Fax: (024)23891320 |
引用本文:
胡望宇;管恒荣;孙晓峰;李诗卓;福本昌宏;岡根功. ZrO_2/Ni阶梯热障涂层的热冲击行为[J]. 金属学报, 1998, 34(10): 1104-1114.
,
,
,
,
,
.
THERMAL SHOCK BEHAVIOR OF ZrO_2/Ni GRADED THERMAL BARRIER COATINGS[J]. Acta Metall Sin, 1998, 34(10): 1104-1114.
1 Leibert C H. Thin Solid Filme, 1979; 64: 329 2 乔海潮,丁传贤,无机材料学报,1991; 6: 103(Qiao H C, Ding C X. J Inoroanic Maten 1991; 6: 103) 3 Wason J W, Levina S R. Thin Solid Filme, 1984; 119: 185 4 McDonald G, Hendricks R C. Thin Solid Filme, 1980; 73: 491 5 福本昌宏.山崎隆典,根功.溶射,1993;30:20(Fukumoto M, Yamasaki T, Okane I. Thermal Spraying, 1993; 30(3): 20) 6 Musil J, Fiala J. Snd Codt Technol,1992; 52: 211 7 Taylor T A, Appleby D L, Weatherill A E, Griffiths J. Surf Coat Technol,1990; 43/44: 470 8 Hu W Y, Guan H R, Sun X F, Li S Z. Surf Coat Technol, in press 9 Hu W Y, Lu S, Li S Z, Sun X F, Guan H R, rubology Int, in press 10 Hu W Y, Guan H R, Sun X F, Li S Z. Mater Lett, 1997; 32: 59 11 Hu W Y, Guan H R, Sun X F, Li S Z. i Am Ceram Soc, in press 12 Araki N, Makino A, Mihara J. Int J Thermophgs, 1992; 13: 331 13 Araki N, Makino A, Ishiguro T, Mihara J. Int J Thermophys, 1992; 13: 515 14 Ishtwro T, Makino A, Araki N, Noda N. Int J Thermophys, 1993; 14: 101 15周本濂.见:师昌绪主编,材料科学进展,北京:科学出版社,1986:186(Zhou B L. In: Shi Changxu ed., Materich Science boss, Beijing: Science Press, 1986: 186) 16 Suresh S, Giannakopoulos A E, Olsson M. J Mech Phys Solids, 1994; 42: 979 17 Shen Y L, Suresh S. J Mater Res, 1995; 10: 1200 18 Wang H, Singh R N. Int Mater Rev, 1994; 39: 228 19 Kingery W D, Bowen H K, Uhlmann D R. Intnduction to Ceromics. 2nd ed., New York: John Wiley &Sons Inc, 1976: 816@ |
|